High-temperature corrosion of Fe3Al in chlorine-containing environments

被引:16
|
作者
Kim, I [1 ]
Cho, WD [1 ]
机构
[1] Univ Utah, Dept Met Engn, Salt Lake City, UT 84112 USA
关键词
Fe3Al; high-temperature corrosion; chlorination;
D O I
10.1016/S0921-5093(98)00998-8
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The corrosion of Fe3Al in Cl-2-Ar gas mixtures has been investigated at the temperature range of 600-800 degrees C using thermogravimetric analysis, SEM, XRD, and EDS. Weight gain was observed during the corrosion of Fe(3)A1 at 600 degrees C in 0.25% Cl-2-Ar, which is due to the formation of Fe2O3, while continuous weight loss of the specimen in 5% Cl-2-Ar at 800 degrees C was observed because of the formation of volatile metal chlorides, FeCl2, FeCl3, and AlCl3. Meanwhile, three distinct stages of weight change during the corrosion of Fe3Al at 700 degrees C in 1% Cl-2-Ar were observed, (1) weight gain, (2) linear weight loss, and (3) gradual decrease of weight loss. Initial weight gain is due to the formation of Fe2O3, and the weight loss in the subsequent two stages is in consequence of the formation of volatile metal chlorides, FeCl2, FeCl3 and AlCl3. (C) 1999 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:269 / 278
页数:10
相关论文
共 50 条
  • [1] High-temperature corrosion of Y-doped Fe3Al in environments containing chlorine and oxygen
    Cho, W. D.
    Han, Gilsoo
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2006, 15 (05) : 558 - 563
  • [2] High-temperature corrosion of Y-doped Fe3Al in environments containing chlorine and oxygen
    W. D. Cho
    Gilsoo Han
    Journal of Materials Engineering and Performance, 2006, 15 : 558 - 563
  • [3] Stability of carbides in chlorine-containing high-temperature environments
    Uusitalo, MA
    Backman, R
    Berger, LM
    Vuoristo, PMJ
    Mäntylä, TA
    EURO CERAMICS VIII, PTS 1-3, 2004, 264-268 : 497 - 500
  • [4] High-temperature oxidation of Fe3Al containing yttrium
    Kim, I
    Cho, WD
    Kim, HJ
    JOURNAL OF MATERIALS SCIENCE, 2000, 35 (18) : 4695 - 4703
  • [5] High-temperature oxidation of Fe3Al containing yttrium
    Insoo Kim
    W. D. Cho
    H. J. Kim
    Journal of Materials Science, 2000, 35 : 4695 - 4703
  • [6] High-Temperature Oxidation of Fe3Al and Fe3Al–Zr Intermetallics
    S. Chevalier
    P. Juzon
    G. Borchardt
    A. Galerie
    K. Przybylski
    J. P. Larpin
    Oxidation of Metals, 2010, 73 : 43 - 64
  • [7] High-temperature deformation behaviour of Fe3Al
    Voyzelle, B
    Boyd, JD
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 258 (1-2): : 243 - 248
  • [8] High-Temperature Corrosion of Fe3Al in 1% Cl2/Ar
    Gilsoo Han
    W.D. Cho
    Oxidation of Metals, 2002, 58 : 391 - 413
  • [9] High-temperature corrosion of Fe3Al in 1% Cl2/Ar
    Han, GS
    Cho, WD
    OXIDATION OF METALS, 2002, 58 (3-4): : 391 - 413
  • [10] High-Temperature Corrosion Mechanisms for Selected Iron and Nickel-Based Alloys Exposed to Sulfur and Chlorine-Containing Environments
    Kung, Steven C.
    CORROSION, 2015, 71 (04) : 483 - 501