Role of late transition metals on pitting resistance of Zr-Ti-(Cu, Ni, Co)-Al bulk metallic glasses in 0.6 M NaCl aqueous solution

被引:15
|
作者
Li, Yu [1 ,2 ]
Xu, Jian [1 ]
机构
[1] Chinese Acad Sci, Shenyang Natl Lab Mat Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China
[2] Univ Chinese Acad Sci, Grad Sch, Beijing 100049, Peoples R China
基金
中国国家自然科学基金;
关键词
Bulk metallic glass; Pitting corrosion; Electrochemical behavior; Passive film; CORROSION BEHAVIOR; OXIDE LAYERS; CHLORIDE-ION; ALLOYS; ALUMINUM;
D O I
10.1016/j.jmst.2017.04.010
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Four quanternary Zr-based bulk metallic glasses (BMGs) were selected, including the Zr46Ti2Cu45Al7, Zr61Ti2Cu25Al12, Zr55Ti4Ni22Al19 and Zr55Ti2Co28Al15, due to their robust glass-forming ability and containing a single species of late transition metal (LTM) in compositions. Their pitting resistances in 0.6 M NaCl aqueous solution were investigated to examine the role of LTM elements in the alloys, with electrochemical measurements, surface morphology observation and x-ray photoelectron spectrometry analysis. It is shown that in comparision with two Cu-bearing BMGs, Zr55Ti4Ni22Al19 and Zr55Ti2Co28Al15 BMGs exhibited significantly superior resistance to pitting. Zr61Ti2Cu25Al12, Zr55Ti4Ni22Al19 and Zr55Ti2Co28Al15 BMGs manifested distinct passivation behaviour, because of the formation of surface passive film mainly comprising of ZrO2, TiO2 and Al2O3. However, no significant differences in the electrochemical resistive properties and thicknesses of passive films were found between Zr61Ti2Cu25Al12 and Zr55Ti4Ni22Al19 BMGs. Nevertheless, at the passive film/metal interface, copper enrichment took place in Zr61Ti2Cu25Al12, whereas the nickel was slightly deficient at the interface in Zr55Ti4Ni22Al19. During pitting propagation, selective dissolution of the zirconium, titanium and aluminum over the copper took place in Zr61Ti2Cu25Al12, but it was not the case in Zr55Ti4Ni22Al19. For the two Cu-bearing BMGs, reduction of passive base metal elements in composition resulted in local selective dissolution, even absence of the passivation. (C) 2017 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
引用
收藏
页码:1278 / 1288
页数:11
相关论文
共 50 条
  • [1] Role of late transition metals on pitting resistance of Zr-Ti-(Cu, Ni,Co)-Al bulk metallic glasses in 0.6 M NaCl aqueous solution
    Yu Li
    Jian Xu
    JournalofMaterialsScience&Technology, 2017, 33 (11) : 1278 - 1288
  • [2] Differences in pitting growth kinetics between Zr60Ni25Al15 and Zr60Cu25Al15 metallic glasses exposed to a 0.6 M NaCl aqueous solution
    Li, Yu
    Xu, Jian
    CORROSION SCIENCE, 2017, 128 : 73 - 84
  • [3] Improved mechanical properties and corrosion resistance of Zr-Cu-Al-Ni-Ti bulk metallic glasses by Co addition
    Xu, Yang
    Hong, Yuan
    Shi, Hongqi
    Chen, Jiajia
    Tang, Tao
    Li, Maomao
    Zhan, Jianming
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2024, 632
  • [4] Homogeneous deformation of Zr-Ti-Al-Cu-Ni bulk metallic glasses
    Bletry, M
    Guyot, P
    Brechet, Y
    Blandin, JJ
    Soubeyroux, JL
    INTERMETALLICS, 2004, 12 (10-11) : 1051 - 1055
  • [5] Limited quasicrystal formation in Zr-Ti-Cu-Ni-Al bulk metallic glasses
    Kuehn, U.
    Eymann, K.
    Mattern, N.
    Eckert, J.
    Gebert, A.
    Bartusch, B.
    Schultz, L.
    ACTA MATERIALIA, 2006, 54 (18) : 4685 - 4692
  • [6] Corrosion resistance of Cu-Zr-Al-Y and Zr-Cu-Ni-Al-Nb bulk metallic glasses
    Zander, Daniela
    Heisterkamp, Beate
    Gallino, Isabella
    JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 434 (SPEC. ISS.) : 234 - 236
  • [7] Crystallization and corrosion resistance of Zr-Ti-Y-Al-Cu-Ni-Co-Fe complex multi -component bulk metallic glasses
    Chen, Chen
    Zhang, Hang
    Fan, Yanzhou
    Zhang, Weiwei
    Wei, Ran
    Guan, Shaokang
    Wang, Tan
    Kong, Bin
    Zhang, Tao
    Li, Fushan
    INTERMETALLICS, 2020, 118
  • [8] Formation and properties of Zr-(Ti, Nb)-Cu-Ni-Al bulk metallic glasses
    Wang, WH
    Wang, RJ
    Fan, GJ
    Eckert, J
    MATERIALS TRANSACTIONS, 2001, 42 (04) : 587 - 591
  • [9] Corrosion of Zr52.5Cu17.9Ni14.6Al10Ti5 bulk metallic glasses in aqueous solutions
    Chieh, TC
    Chu, J
    Liu, CT
    Wu, JK
    MATERIALS LETTERS, 2003, 57 (20) : 3022 - 3025
  • [10] The Dynamic Behavior of "Strong"-"Superstrong" Transition of Bulk Metallic Glasses Zr-Cu-Ni-Al Alloy
    Wang, Dan
    Sun, Min-hua
    Yin, Long-cheng
    Huang, Hai-liang
    Jiang, Hong-wei
    Peng, Hong-yan
    Zheng, You-jin
    Chen, Yu-qiang
    PROCEEDINGS OF THE 7TH NATIONAL CONFERENCE ON CHINESE FUNCTIONAL MATERIALS AND APPLICATIONS (2010), VOLS 1-3, 2010, : 548 - +