The effects of room temperature ECAP and subsequent aging on the structure and properties of the Al-3%Mg aluminium alloy

被引:40
|
作者
Tanski, T. [1 ,2 ]
Snopinski, P. [1 ]
Prusik, K. [3 ,4 ]
Sroka, M. [1 ]
机构
[1] Silesian Tech Univ, Inst Engn Mat & Biomat, Div Mat Proc Technol Management & Comp Tech Mat S, Ul Konarskiego 18A, PL-44100 Gliwice, Poland
[2] Silesian Tech Univ, Ctr Nanotechnol, Konarskiego 18A Str, PL-44100 Gliwice, Poland
[3] Univ Silesia, Inst Mat Sci, 75 Pulku Piechoty IA, PL-44500 Chorzow, Poland
[4] Univ Silesia, Silesian Ctr Educ & Interdisciplinary Res, 75 Pulku Piechoty IA, PL-41500 Chorzow, Poland
关键词
Aluminium; Structure; Heat treatment; EBSD; XRD; TEM; AL-MG ALLOYS; SEVERE PLASTIC-DEFORMATION; MECHANICAL-PROPERTIES; GRAIN-REFINEMENT; MICROSTRUCTURAL EVOLUTION; STRENGTHENING MECHANISMS; PRECIPITATION; BEHAVIOR; RECRYSTALLIZATION; STABILITY;
D O I
10.1016/j.matchar.2017.09.039
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The results of the present investigation are focused on the structure examinations of a commercial Al-3%Mg alloy in different conditions using an optical microscope (OM), scanning electron microscopy (SEM), the EBSD technique, transmission electron microscopy (TEM) and X-ray diffraction (XRD). Measurements of the micro hardness and ultimate tensile strength were carried out to evaluate the influence of ECAP and post-ECAP treatment on the mechanical properties. In this study, we found that 6 ECAP passes via route Be result in a significant grain refinement. The measured average grain size of the as deformed sample was about 0.43 pm. As a result of the performed post-ECAP heat treatment (artificial ageing), a material with a more homogenous microstructure, having an average grain size of similar to 0.68 mu m, was obtained. The results of the mechanical property measurements show a significant increase in mechanical strength to about similar to 384 [MPa] in the T9 condition and to similar to 330 [MPa] after post-ECAP treatment (T8 condition). The high strength of the alloy in the T9 condition is suggested to be related to grain size strengthening, dislocation strengthening and precipitation strengthening. An increase in elongation/ductility from 2.4% to 11.2% was observed in the T8 condition sample, which is a result of the grain growth and the dislocation density decrease.
引用
收藏
页码:185 / 195
页数:11
相关论文
共 50 条
  • [1] The effects of room temperature ECAP and subsequent aging on mechanical properties of 2024 Al alloy
    Goodarzy, M. H.
    Arabi, H.
    Boutorabi, M. A.
    Seyedein, S. H.
    Najafabadi, S. H. Hasani
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 585 : 753 - 759
  • [2] The effects of room temperature ECAP and subsequent aging on mechanical properties of 2024 Al alloy
    Goodarzy, M.H. (mh_goodarzy@iust.ac.ir), 1600, Elsevier Ltd (585):
  • [3] Microstructure, grain refinement and hardness of Al-3%Mg aluminium alloy processed by ECAP with helical die
    Snopinski, Przemyslaw
    Tanski, T.
    Matus, K.
    Rusz, S.
    ARCHIVES OF CIVIL AND MECHANICAL ENGINEERING, 2019, 19 (02) : 287 - 296
  • [4] Effect of Microstructure and Mechanical Properties of Al–Mg Alloy Processed by ECAP at Room Temperature and Cryo Temperature
    Ramesh Kumar S.
    Kondaiah Gudimetla
    Tejaswi B.
    Ravisankar B.
    Transactions of the Indian Institute of Metals, 2017, 70 : 639 - 648
  • [5] Effect of Microstructure and Mechanical Properties of Al-Mg Alloy Processed by ECAP at Room Temperature and Cryo Temperature
    Kumar, Ramesh S.
    Gudimetla, Kondaiah
    Tejaswi, B.
    Ravisankar, B.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2017, 70 (03) : 639 - 648
  • [6] A study on cryogenic temperature ECAP on the and mechanical properties of Al-Mg alloy
    Chatterjee, Arnomitra
    Sharma, Garima
    Sarkar, A.
    Singh, J. B.
    Chakravartty, J. K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 556 : 653 - 657
  • [7] Microstructure and mechanical properties of 7005 aluminum alloy processed by room temperature ECAP and subsequent annealing
    Duan, Yulu
    Tang, Lei
    Xu, Guofu
    Deng, Ying
    Yin, Zhimin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 664 : 518 - 529
  • [8] Mechanical properties and microstructure evolution of ultra-high strength Al-Zn-Mg-Cu alloy processed by room temperature ECAP with post aging
    Wang, Weiyi
    Pan, Qinglin
    Wang, Xiangdong
    Sun, Yuanwei
    Long, Liang
    Huang, Zhiqi
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 731 : 195 - 208
  • [9] Effect of ECAP temperature on microstructure and mechanical properties of Al–Zn–Mg–Cu alloy
    M.H.Shaeri
    M.Shaeri
    M.Ebrahimi
    M.T.Salehi
    S.H Seyyedein
    ProgressinNaturalScience:MaterialsInternational, 2016, 26 (02) : 182 - 191
  • [10] Partial Grain Refinement in Al-3%Cu Alloy during ECAP at Elevated Temperatures
    Mazurina, Inna
    Sakai, Taku
    Miura, Hiromi
    Sitdikov, Oleg
    Kaibyshev, Rustam
    MATERIALS TRANSACTIONS, 2009, 50 (01) : 101 - 110