Physical and chemical properties of concrete using GGBFS-KR slag-gypsum binder

被引:41
|
作者
Cho, Bongsuk [1 ]
Choi, Hyeonggil [2 ]
机构
[1] Res Inst Ind Sci & Technol, Slag Utilizat Res Team, Pohang, South Korea
[2] Muroran Inst Technol, Grad Sch Engn, Muroran, Hokkaido, Japan
关键词
Cement-free binder; GGBFS; KR slag; Gypsum; Iron & steel making process; Ettringite; Shrinkage; Strength; Porosity; BLAST-FURNACE SLAG; FLY-ASH; CEMENT; TEMPERATURE; ACTIVATOR; HYDRATION;
D O I
10.1016/j.conbuildmat.2016.07.023
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The Kambara reactor (KR) slag, which is a byproduct generated in the preliminary treatment process of molten iron by a KR mechanical stirring process, is composed of Ca(OH)(2), CaCO3 and 2CaO center dot SiO2. It was confirmed that the alkali stimulus of Ca(OH)(2) contained in the KR slag could cause a cement-free binder to harden. However, the strength performance of a GGBFS-based cement-free binder mixed with only the KR slag was very low. The gypsum (CaSO4) is additionally used in order to enhance the strength performance of the GGBFS-KR slag binder. The result showed that the 28-day compressive strength of the GGBFS-KR slag-gypsum binder (GKGB) concrete was similar to that of slag cement. On the other hand, compared to those of slag cement, the drying shrinkage was shown to be 121.8-129.0%, and the cumulate porosity was shown to be 190-208%. These results imply that ettringite, which is a main hydrate of GKGB, is thick and provides the structural stability by forming a frame structure. However, the thicker ettringite, the more pores may be created. In other words, high amounts of ettringite form a porous structure, which has many micro pores so that the porosity and absorption become higher, leading to higher drying shrinkage. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:436 / 443
页数:8
相关论文
共 50 条
  • [1] STRENGTH AND DURABILITY OF SLAG-GYPSUM CEMENT CONCRETE
    UOMOTO, T
    KOBAYASHI, K
    JOURNAL OF THE AMERICAN CONCRETE INSTITUTE, 1983, 80 (04): : 350 - 350
  • [2] A study on the durability of porous concrete using slag-gypsum cement
    Mitsuiwa, Y.
    Nakamoto, J.
    Amo, K.
    Yokoi, K.
    INNOVATIONS IN STRUCTURAL ENGINEERING AND CONSTRUCTION, VOLS 1 AND 2, 2008, : 483 - +
  • [3] Effect of GGBFS slag on CSA-based ternary binder hydration, and concrete performance
    Ghosh, Debalina
    Ma, Zhongguo John
    Hun, Diana
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 386
  • [4] The Impact of Fly Ash on the Properties of Cementitious Materials Based on Slag-Steel Slag-Gypsum Solid Waste
    Wang, Fei
    Du, Huihui
    Zheng, Zhong
    Xu, Dong
    Wang, Ying
    Li, Ning
    Ni, Wen
    Ren, Chao
    MATERIALS, 2024, 17 (19)
  • [5] The Effects of CuO Nanoparticles on Properties of Self Compacting Concrete with GGBFS as Binder
    Nazari, Ali
    Rafieipour, Mohammad Hossein
    Riahi, Shadi
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2011, 14 (03): : 307 - 316
  • [6] Gypsum-Free Slag Portland Cement as an Effective Binder for Concrete.
    Royak, S.M.
    Gal'perina, T.Ya.
    Perminova, Yu.N.
    Dorogina, N.G.
    Gusev, A.I.
    Tsement, 1984, (11): : 18 - 19
  • [7] Characteristics of GGBFS-Based Pervious Concrete Considering Rheological Properties of the Binder
    Yanchen Oinam
    Suhawn Ju
    Seongwoo Gwon
    Myoungsu Shin
    Sukhoon Pyo
    International Journal of Concrete Structures and Materials, 2022, 16
  • [8] Characteristics of GGBFS-Based Pervious Concrete Considering Rheological Properties of the Binder
    Oinam, Yanchen
    Ju, Suhawn
    Gwon, Seongwoo
    Shin, Myoungsu
    Pyo, Sukhoon
    INTERNATIONAL JOURNAL OF CONCRETE STRUCTURES AND MATERIALS, 2022, 16 (01)
  • [9] Engineering properties of cementless concrete produced from GGBFS and recycled desulfurization slag
    Kuo, Wen-Ten
    Wang, Her-Yung
    Shu, Chun-Ya
    CONSTRUCTION AND BUILDING MATERIALS, 2014, 63 : 189 - 196
  • [10] Effects of Al2O3 nanoparticles on properties of self compacting concrete with ground granulated blast furnace slag (GGBFS) as binder
    Ali NAZARI
    Shadi RIAHI
    Science China(Technological Sciences), 2011, (09) : 2327 - 2338