Piezoelectric and dielectric aging of Bi0.5(Na0.82K0.18)0.5TiO3 lead-free ferroelectric thick films

被引:19
|
作者
Zhang, Haibo [1 ,2 ,3 ]
Jiang, Shenglin [2 ]
Xiao, Jianzhong [1 ]
Kajiyoshi, Koji [3 ]
机构
[1] Huazhong Univ Sci & Technol, Sch Mat Sci & Engn, Wuhan 430074, Peoples R China
[2] Huazhong Univ Sci & Technol, Dept Elect Sci & Technol, Wuhan 430074, Peoples R China
[3] Kochi Univ, Res Lab Hydrothermal Chem, Fac Sci, Kochi 7808520, Japan
基金
国家高技术研究发展计划(863计划); 中国博士后科学基金; 中国国家自然科学基金;
关键词
ELECTRICAL-PROPERTIES; CERAMICS; PIEZOCERAMICS; TEMPERATURE; TITANATE; BATIO3;
D O I
10.1063/1.3437637
中图分类号
O59 [应用物理学];
学科分类号
摘要
Ferroelectric Bi-0.5(Na0.82K0.18)(0.5)TiO3 (NKBT) thick films have been prepared using screen printing on Pt electroded alumina substrates. The room-temperature dielectric constant of resulting 60 mu m thick NKBT film reaches as high as 823 at 1 kHz and the depolarization temperature, T-d, locates at 130 degrees C. The effect of amplitude and frequency of the applied ac field and the aging temperature as well as the Bi excess on the dielectric and piezoelectric aging characteristics are systemically studied. The results show that the dielectric and piezoelectric aging are associated with the reorientation of defect dipoles which stabilized the non-180 degrees domain walls. By this reorientation the domain wall motions are clamped by a time dependent force resulting in the observed decrease in the dielectric and piezoelectric properties during the aging procedural. Moreover, the aging in NKBT thick films exhibits strong frequency dependence, which is caused by that the reorientation and alignment of the defect dipoles with the local polar domains provide a pinning field to the micropolar region, where the regions with larger micropolar volume will experience stronger pinning potential. The NKBT thick films added with 0.5 mol % Bi2O3 exhibit relative lower aging rate of the dielectric constant and piezoelectric coefficient, resulting from the compensation of the Bi3+ vacancies by the addition of small amount of excess Bi2O3. (c) 2010 American Institute of Physics. [doi:10.1063/1.3437637]
引用
收藏
页数:6
相关论文
共 50 条
  • [1] Large transverse piezoelectric properties of lead-free Bi0.5(Na0.82K0.18)0.5TiO3 films
    Chae, Song A.
    Won, Sung Sik
    Seog, Hae Jin
    Ullah, Aman
    Ahn, Chang Won
    Kim, Ill Won
    CURRENT APPLIED PHYSICS, 2016, 16 (04) : 429 - 434
  • [2] Enhanced Pyroelectric and Piezoelectric Figure of Merit of Porous Bi0.5(Na0.82K0.18)0.5TiO3 Lead-Free Ferroelectric Thick Films
    Zhang, Haibo
    Jiang, Shenglin
    Kajiyoshi, Koji
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (07) : 1957 - 1964
  • [3] Non-180° domain contributions in Bi0.5(Na0.82K0.18)0.5TiO3 lead-free piezoelectric thick films
    Huang, Jinqiang
    Zhang, Yangyang
    Jiang, Huacheng
    Fan, Pengyuan
    Xiao, Jianzhong
    Zhang, Haibo
    CERAMICS INTERNATIONAL, 2015, 41 (09) : 10506 - 10511
  • [4] Control of Paste Rheology and Piezoelectric Properties of Bi0.5(Na0.82K0.18)0.5TiO3 Lead-Free Piezoelectric Thick Films Deposited by Screen Printing
    Zhang, Haibo
    Jiang, Shenglin
    Kajiyoshi, Koji
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2011, 8 (03) : 658 - 668
  • [5] Dielectric and piezoelectric properties of Bi0.5(Na0.82K0.18)0.5TiO3-LiSbO3 lead-free piezoelectric ceramics
    Zhou Chong-Rong
    Chai Li-Yuan
    BULLETIN OF MATERIALS SCIENCE, 2011, 34 (04) : 933 - 936
  • [6] Effect of repeated composite sol infiltrations on the dielectric and piezoelectric properties of a Bi0.5(Na0.82K0.18)0.5TiO3 lead free thick film
    Zhang, Haibo
    Jiang, Shenglin
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2009, 29 (04) : 717 - 723
  • [7] Piezoelectric and Dielectric Properties of Dy2O3-Doped Bi0.5 (Na0.82K0.18)0.5TiO3 Lead-Free Ceramics
    Chen Zhi-Hui
    Ding Jian-Ning
    Mei Lin
    Yuan Ning-Yi
    Zhang Wei-Wei
    FERROELECTRICS, 2011, 425 : 63 - 71
  • [8] Giant strain in Nb-doped Bi0.5(Na0.82K0.18)0.5TiO3 lead-free electromechanical ceramics
    Pham, Ky-Nam
    Hussain, Ali
    Ahn, Chang Won
    Kim, Ill Won
    Jeong, Soon Jong
    Lee, Jae-Shin
    MATERIALS LETTERS, 2010, 64 (20) : 2219 - 2222
  • [9] Microstructure and electrical properties of Bi-based lead-free piezoelectric ceramics Bi0.5 (Na0.82K0.18)0.5TiO3 - BiCrO3
    Zhou, Chang-Rong
    Liu, Xin-Yu
    Yang, Gui-Hua
    Yuan, Chang-Lai
    Jiang, Min-Hong
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2009, 19 (07): : 1289 - 1293
  • [10] Piezoelectric property in morphotropic phase boundary Bi0.5(Na0.82K0.18)0.5TiO3 lead free thick film deposited by screen printing
    Zhang, Haibo
    Jiang, Shenglin
    Zeng, Yike
    APPLIED PHYSICS LETTERS, 2008, 92 (15)