摘要
Fabrication procedure for silicon carbide power metal oxide semiconductor field effect transistors can be improved through simultaneous formation of ohmic contacts on both the n-source and p-well regions. We have succeeded in the simultaneous formation of Ni/Al ohmic contacts to n- and p-type SiC after annealing at 1000 degrees C for 5 mins in an ultra-high vacuum. Ohmic contacts to n-type SiC were found when Al-layer thickness was less than about 5 nm while ohmic contacts to p-type SiC were observed for an Al-layer thickness greater than about 5 nm. Only the contacts with Al-layer thicknesses in the range of 5 to 6 nm exhibited ohmic 2 behavior to both n- and p-type SiC, with specific contact resistances of 1.8 x 10(-4) Omega cm(2) and 1.2 x 10(-2) Omega cm(2) for n- and p-type SiC, respectively. An about 100 nm-thick contact layer was uniformly formed on the SiC substrate and polycrystalline delta-Ni2Si(Al) grains were formed at the contact/SiC interface. The distribution in values for the Al/Ni ratio in the delta-Ni2Si(Al) grains which exhibited ohmic behavior to both n- and p-type SiC was the largest. The smallest average delta-Ni2Si(Al) grain size was also observed in these contacts. Thus, the large distribution in the Al/Ni ratios and a fine microstructure were found to be characteristic of the ohmic contacts to both n- and p-type SiC.
引用
收藏
页码:189 / +
页数:2
相关论文
共 50 条
  • [1] Simultaneous Formation of Ni/Al Ohmic Contacts to Both n- and p-Type 4H-SiC
    Kazuhiro Ito
    Toshitake Onishi
    Hidehisa Takeda
    Kazuyuki Kohama
    Susumu Tsukimoto
    Mitsuru Konno
    Yuya Suzuki
    Masanori Murakami
    Journal of Electronic Materials, 2008, 37
  • [2] Simultaneous formation of Ni/Al ohmic contacts to both n- and p-type 4H-SiC
    Ito, Kazuhiro
    Onishi, Toshitake
    Takeda, Hidehisa
    Kohama, Kazuyuki
    Tsukimoto, Susumu
    Konno, Mitsuru
    Suzuki, Yuya
    Murakami, Masanori
    JOURNAL OF ELECTRONIC MATERIALS, 2008, 37 (11) : 1674 - 1680
  • [3] STUDY ON SIMULTANEOUS FORMATION OF OHMIC CONTACTS ON p- AND n- TYPE 4H-SiC USING Ni/Ti/Al TERNARY SYSTEM
    Zhang, Xufang
    Tang, Yidan
    Shen, Huajun
    Bai, Yun
    Huo, Ruibin
    Wang, Wenwu
    Liu, Su
    2014 12TH IEEE INTERNATIONAL CONFERENCE ON SOLID-STATE AND INTEGRATED CIRCUIT TECHNOLOGY (ICSICT), 2014,
  • [4] Ni/W/Ni ohmic contacts for both n- and p-type 4H-SiC
    Dongwoo Bae
    Gilcho Ahn
    Chungbu Jeong
    Kwangsoo Kim
    Electrical Engineering, 2018, 100 : 2431 - 2437
  • [5] Ni/W/Ni ohmic contacts for both n- and p-type 4H-SiC
    Bae, Dongwoo
    Ahn, Gilcho
    Jeong, Chungbu
    Kim, Kwangsoo
    ELECTRICAL ENGINEERING, 2018, 100 (04) : 2431 - 2437
  • [6] Simultaneous formation of p- and n-type ohmic contacts to 4H-SiC using the ternary Ni/Ti/Al system
    Tsukimoto, S
    Sakai, T
    Onishi, T
    Ito, K
    Murakami, M
    JOURNAL OF ELECTRONIC MATERIALS, 2005, 34 (10) : 1310 - 1312
  • [7] Simultaneous Formation of Ni/Ti/Al/Ag Ohmic Contacts to both p- and n- type for 4H-SiC RSD
    Yan, Xiaoxue
    Liang, Lin
    Zhang, Ludan
    2019 IEEE WORKSHOP ON WIDE BANDGAP POWER DEVICES AND APPLICATIONS IN ASIA (WIPDA ASIA 2019), 2019,
  • [8] Simultaneous formation of p- and n-type ohmic contacts to 4H-SiC using the ternary Ni/Ti/Al system
    S. Tsukimoto
    T. Sakai
    T. Onishi
    Kazuhiro Ito
    Masanori Murakami
    Journal of Electronic Materials, 2005, 34 : 1310 - 1312
  • [9] Simultaneous formation of ohmic contacts for both n- and p-type 4H-SiC using NiAl-based contact materials
    Tsukimoto, Susumu
    Onishi, Toshitake
    Ito, Kazuhiro
    Murakami, Masanori
    SILICON CARBIDE 2006 - MATERIALS, PROCESSING AND DEVICES, 2006, 911 : 359 - +
  • [10] Simultaneous Formation of Ohmic Contacts on p +- and n +-4H-SiC Using a Ti/Ni Bilayer
    Joo, Sung-Jae
    Baek, Sangwon
    Kim, Sang-Cheol
    Lee, Jeong-Soo
    JOURNAL OF ELECTRONIC MATERIALS, 2013, 42 (10) : 2897 - 2904