Analysis of the Reaction Layer Formed during Sapphire-Sapphire Brazing Using a Ag-Cu-Ti Filler Metal for Gas-Pressure Sensors

被引:1
|
作者
Zaharinie, Tuan [1 ,2 ]
Huda, Zainul [3 ]
Ibrahim, Suriani [1 ,2 ]
Yusof, Farazila [1 ,2 ]
Hamdi, Mohd [1 ,2 ]
Rehan, Mohammad [4 ]
Ariga, Tadashi [5 ]
机构
[1] Univ Malaya, Dept Mech Engn, Kuala Lumpur 50603, Malaysia
[2] Univ Malaya, Ctr Adv Mfg & Mat Proc AMMP Ctr, Kuala Lumpur 50603, Malaysia
[3] King Abdulaziz Univ, Dept Mech Engn, Jeddah 21589, Saudi Arabia
[4] King Abdulaziz Univ, Ctr Excellence Environm Studies CEES, Jeddah 21589, Saudi Arabia
[5] Tokai Univ, Sch Engn, Dept Mat Sci, Hiratsuka, Kanagawa 2591292, Japan
关键词
sapphire; characterization; joining; scanning electron microscopy; transmission electron microscopy; DIFFUSION; INTERFACE; ALUMINA; AL2O3;
D O I
10.1021/acsaelm.2c00213
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The present research paper introduces a reliable and economical method for direct brazing using an active Ag-Cu-Ti filler metal that can ensure effective brazing. The sapphire-sapphire brazing process has been conducted at temperatures in the range of 830-900 degrees C for durations in the range of 15-30 min in a high-vacuum (10(-4) Pa) furnace. Material and microstructural characterization involved the use of scanning electron microscope-energy-dispersive system (SEM-EDS) and transmission electron microscope (TEM) for investigating the bonding joint morphologies. Two uniform reaction layers were observed to have formed at the sapphire/brazed area interface. On the sapphire side, the first reaction layer, which was uniform and had a thickness in the range of 0.13-0.17 mu m, was identified as a TiO phase, whereas the second layer was identified as a Cu3Ti3O phase with a thickness in the range of 1.72-2.43 mu m. The uniformity of the Cu3Ti3O phase was found to decrease with increasing brazing temperature and time. Therefore, in this research, a lower brazing temperature and time (830 degrees C/15 min) were chosen so as to avoid bonding degradation.
引用
收藏
页码:2405 / 2412
页数:8
相关论文
共 6 条
  • [1] Sapphire joining using Ag70.5Cu27.5Ti2 brazing filler metal
    Ning, HL
    Huang, FX
    Ma, JS
    Geng, ZT
    Han, ZD
    RARE METAL MATERIALS AND ENGINEERING, 2003, 32 (03) : 236 - 239
  • [2] Vacuum brazing of Zircaloy-4 and stainless steel using Ag-Cu-Ti brazing filler metal
    Qi Kai
    Li Ruifeng
    PROGRESS IN MATERIALS AND PROCESSES, PTS 1-3, 2013, 602-604 : 2069 - 2073
  • [3] Reaction Layer Microstructure of SiC/SiC Joints Brazed by Ag-Cu-Ti Filler Metal
    Liu, Yan
    Huang, Zhengren
    Liu, Xiujian
    HIGH-PERFORMANCE CERAMICS VI, 2010, 434-435 : 202 - 204
  • [4] Joining of sapphire and hot pressed Al2O3 using Ag70.5Cu27.5Ti2 brazing filler metal
    Ning, HL
    Geng, ZT
    Ma, JS
    Huang, FX
    Qian, ZY
    Han, ZD
    CERAMICS INTERNATIONAL, 2003, 29 (06) : 689 - 694
  • [5] Reaction layer growth in AlN to molybdenum joint brazed using Ag-Cu-Ti filler metal - Study on bonding of aluminum nitride to metals (Report 2)
    Nakao, Yoshikuni
    Nishimoto, Kazutoshi
    Saida, Kazuyoshi
    Murabe, Kaoru
    Fukaya, Yasuhiro
    Yosetsu Gakkai Ronbunshu/Quarterly Journal of the Japan Welding Society, 1994, 12 (01): : 122 - 125
  • [6] Brazing continuous carbon fiber reinforced Li2O-Al2O3-SiO2 ceramic matrix composites to Ti-6Al-4V alloy using Ag-Cu-Ti active filler metal
    Liu, D.
    Niu, H. W.
    Zhou, Y. H.
    Song, X. G.
    Tang, D. Y.
    Feng, J. C.
    MATERIALS & DESIGN, 2015, 87 : 42 - 48