Thermodynamic Stability of Low-k Amorphous SiOCH Dielectric Films

被引:28
|
作者
Chen, Jiewei [1 ,2 ]
King, Sean W. [3 ]
Muthuswamy, Elayaraja [1 ,2 ]
Koryttseva, Anastasia [1 ,2 ,4 ]
Wu, Di [1 ,2 ]
Navrotsky, Alexandra [1 ,2 ]
机构
[1] Univ Calif Davis, Peter A Rock Thermochem Lab, Davis, CA 95616 USA
[2] Univ Calif Davis, NEAT ORU, Davis, CA 95616 USA
[3] Intel Corp, Log Technol Dev, Hillsboro, OR 97124 USA
[4] NI Lobachevsky State Univ Nizhny Novgorod, Dept Chem, 23 Gagarin Ave, Nizhnii Novgorod 603950, Russia
关键词
amorphous low-k SiOCH films; formation enthalpy; thermodynamic stability; HIGH-TEMPERATURE CALORIMETRY; CHEMICAL-VAPOR-DEPOSITION; C-O SYSTEM; SILICON-OXYCARBIDE; THIN-FILMS; SPECTROSCOPY CHARACTERIZATION; CONSTANT MATERIALS; CERAMICS; DIRECTIONS; PROGRESS;
D O I
10.1111/jace.14268
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Si-O-C-based amorphous or nanostructured materials are now relatively common and of interest for numerous electronic, optical, thermal, mechanical, nuclear, and biomedical applications. Using plasma-enhanced chemical vapor deposition (PECVD), hydrogen atoms are incorporated into the system to form SiOCH dielectric films with very low dielectric constants (k). While these low-k dielectrics exhibit chemical stability as deposited, they tend to lose hydrogen and carbon (as labile organic groups) and convert to SiO2 during thermal annealing and other fabrication processes. Therefore, knowledge of their thermodynamic properties is essential for understanding the conditions under which they can be stable. High-temperature oxidative drop solution calorimetry measurement in molten sodium molybdate solvent at 800 degrees C showed that these materials possess negative formation enthalpies from their crystalline constituents (SiC, SiO2, C, Si) and H-2. The formation enthalpies at room temperature become less exothermic with increasing carbon content and more exothermic with increasing hydrogen content. Fourier transform infrared spectroscopy (FTIR) spectroscopy examined the structure from a microscopic perspective. Different from polymer-derived ceramics with similar composition, these low-k dielectrics are mainly comprised of Si-O(C)-Si networks, and the primary configuration of carbon is methyl groups. The thermodynamic data, together with the structural analysis suggest that the conversion of sp(2) carbon in the matrix to surface organic functional groups by incorporating hydrogen increases thermodynamic stability. However, the energetic stabilization by hydrogen incorporation is not enough to offset the large entropy gain upon hydrogen release, so hydrogen loss during processing at higher temperatures must be managed by kinetic rather than thermodynamic strategies.
引用
收藏
页码:2752 / 2759
页数:8
相关论文
共 50 条
  • [1] Energetics of porous amorphous low-k SiOCH dielectric films
    Chen, Jiewei
    Calvin, Jason J.
    King, Sean W.
    Woodfield, Brian F.
    Navrotsky, Alexandra
    [J]. JOURNAL OF CHEMICAL THERMODYNAMICS, 2019, 139
  • [2] Dependence of dielectric constant of SiOCH low-k films on porosity and pore size
    Palov, Alexander
    Rakhimova, Tatiana V.
    Krishtab, Mikhail B.
    Baklanov, Mikhail R.
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 2015, 33 (02):
  • [3] Controllable change of porosity of SiOCH low-K dielectric film
    Shamiryan, DG
    Baklanov, MR
    Vanhaelemeersch, S
    Maex, K
    [J]. ADVANCED METALLIZATION CONFERENCE 2000 (AMC 2000), 2001, : 635 - 639
  • [4] Charge Transport Mechanism in a PECVD Deposited Low-k SiOCH Dielectric
    Perevalov, T., V
    Gismatulin, A. A.
    Gritsenko, V. A.
    Xu, H.
    Zhang, J.
    Vorotilov, K. A.
    Baklanov, M. R.
    [J]. JOURNAL OF ELECTRONIC MATERIALS, 2022, 51 (05) : 2521 - 2527
  • [5] Charge Transport Mechanism in a PECVD Deposited Low-k SiOCH Dielectric
    T. V. Perevalov
    A. A. Gismatulin
    V. A. Gritsenko
    H. Xu
    J. Zhang
    K. A. Vorotilov
    M. R. Baklanov
    [J]. Journal of Electronic Materials, 2022, 51 : 2521 - 2527
  • [6] Channel cracking technique for toughness measurement of SiOCH low-k films
    Brillet-Rouxel, Helene
    Dupeux, Michel
    Braccini, Muriel
    Orain, Stephane
    [J]. MATERIALS, TECHNOLOGY AND RELIABILITY OF LOW-K DIELECTRICS AND COPPER INTERCONNECTS, 2006, 914 : 89 - +
  • [7] Towards the Understanding of Intrinsic Degradation and Breakdown Mechanisms of a SiOCH Low-k Dielectric
    Wu, C.
    Li, Y.
    Barbarin, Y.
    Ciofi, I.
    Tang, B.
    Kauerauf, T.
    Croes, K.
    Bommels, J.
    De Wolf, I.
    Tokei, Zs
    [J]. 2014 IEEE INTERNATIONAL RELIABILITY PHYSICS SYMPOSIUM, 2014,
  • [8] Visible room temperature photoluminescence of low-k SiOCH films, prepared by PECVD
    Ligatchev, V
    Wong, TKS
    [J]. COMMAD 2002 PROCEEDINGS, 2002, : 417 - 420
  • [9] Investigation of deposition temperature effect on properties of PECVD SiOCH low-k films
    Wong, TKS
    Liu, B
    Narayanan, B
    Ligatchev, V
    Kumar, R
    [J]. THIN SOLID FILMS, 2004, 462 (SPEC. ISS.) : 156 - 160
  • [10] Study of hydrogen stability in low-k dielectric films by ion beam techniques
    Zhang, Y.
    Saraf, L.
    Shutthanandan, V.
    Hughes, K. D.
    Kuan, R.
    Thevuthasan, S.
    [J]. NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2006, 249 : 335 - 338