Effect of NiO content in mesoporous NiO-Al2O3 catalysts for high pressure partial oxidation of methane to syngas

被引:60
|
作者
Kobayashi, Yasukazu [1 ]
Horiguchi, Junpei [1 ]
Kobayashi, Seishiro [1 ]
Yamazaki, Yuichiro [1 ]
Omata, Kohji [1 ]
Nagao, Daisuke [2 ]
Konno, Mikio [2 ]
Yamada, Muneyoshi [3 ]
机构
[1] Tohoku Univ, Grad Sch Engn, Dept Appl Chem, Aoba Ku, Sendai, Miyagi 9808579, Japan
[2] Tohoku Univ, Grad Sch Engn, Dept Chem Engn, Aoba Ku, Sendai, Miyagi 9808579, Japan
[3] Akita Natl Coll Technol, Akita 0118511, Japan
关键词
Partial oxidation; Syngas formation; Oxidative reforming of methane; NiO-Al2O3; catalyst; Short contact time reaction; Mesoporous; REFORMING MODEL CATALYSTS; SYNTHESIS GAS; NI/AL2O3; CATALYSTS; COKE FORMATION; CARBON; ALUMINA; DEACTIVATION; ALKALINE; OXIDES;
D O I
10.1016/j.apcata.2011.01.034
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effect of NiO content in mesoporous NiO-Al2O3 catalysts on stability of the catalytic activity was investigated for partial oxidation of methane to syngas under the reaction conditions at 650 degrees C and 1 MPa over the contact time range from 0.1 to 5 ms. Mesoporous/porous NiO-Al2O3 catalysts with a high BET surface area were prepared with NiO content of 3.7-75 wt%. From XRD patterns and TPR profiles observed in these catalysts before H-2 pretreatment, the presence of strong interactions between NiO and Al2O3 was indicated, which gave relatively small NiO particles in the catalysts. As results of activity tests conducted by changing the contact time from 5 ms to lower until the catalyst lost its oxidation activity, the order of the catalyst tolerance against oxidation of nickel active species on them was: NiO(75)-Al2O3 > NiO(40)-Al2O3 > NiO(90)-Al2O3 > NiO(11)-Al2O3. As results of long runs and TG-DTA analysis, NiO(40)-Al2O3 showed the stable activity without any carbon deposition after 24h reaction. This is because the Ni particle size and dispersion are 5.9-7.1 nm and 10.8%, respectively, which are considered to be suitable to prevent both carbon deposition and oxidation of nickel species during reaction, while NiO(75)-Al2O3 with Ni particle size of 11.7-15.9 nm gave high carbon deposition after a long run. The Ni particle size of 10 nm was a borderline for carbon deposition under reaction conditions at 1 MPa. (c) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:129 / 137
页数:9
相关论文
共 50 条
  • [1] Mesoporous NiO-Al2O3 catalyst for high pressure partial oxidation of methane to syngas
    Horiguchi, Junpei
    Kobayashi, Yasukazu
    Kobayashi, Seishiro
    Yamazaki, Yuichiro
    Omata, Kohji
    Nagao, Daisuke
    Konno, Mikio
    Yamada, Muneyoshi
    [J]. APPLIED CATALYSIS A-GENERAL, 2011, 392 (1-2) : 86 - 92
  • [2] Three-dimensionally ordered macro/mesoporous NiO-Al2O3 nanohybrid catalysts for partial oxidation of methane to syngas
    Liu, Ping
    Zhang, Kan
    Lyu, Zhanjun
    Zhao, Ning
    Xiao, Fukui
    [J]. ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2017, 254
  • [3] One step synthesis of mesoporous NiO-Al2O3 catalyst for partial oxidation of methane to syngas: The role of calcination temperature
    Ding, Chuanmin
    Liu, Weili
    Wang, Junwen
    Liu, Ping
    Zhang, Kan
    Gao, Xiaofeng
    Ding, Guangyue
    Liu, Shibin
    Han, Yulin
    Ma, Xishun
    [J]. FUEL, 2015, 162 : 148 - 154
  • [4] Deactivation studies over NiO/γ-Al2O3 catalysts for partial oxidation of methane to syngas
    Zhang, YH
    Xiong, GX
    Sheng, SS
    Yang, WS
    [J]. CATALYSIS TODAY, 2000, 63 (2-4) : 517 - 522
  • [5] Partial oxidation of methane to syngas using NiO‐supported catalysts
    Russell S. Drago
    Krzysztof Jurczyk
    Nicholas Kob
    Alak Bhattacharyya
    Joseph Masin
    [J]. Catalysis Letters, 1998, 51 : 177 - 181
  • [6] Plasmochemical preparation of NiO-Al2O3 catalysts
    Normatov, IS
    Shermatov, N
    Mirsaidov, U
    [J]. INORGANIC MATERIALS, 2001, 37 (09) : 947 - 949
  • [7] Effect of La2O3 added to NiO/Al2O3 catalyst on partial oxidation of methane to syngas
    Cao, L
    Chen, Y
    Li, W
    [J]. NATURAL GAS CONVERSION IV, 1997, 107 : 467 - 471
  • [8] Partial oxidation of methane to syngas using NiO-supported catalysts
    Drago, RS
    Jurczyk, K
    Kob, N
    Bhattacharyya, A
    Masin, J
    [J]. CATALYSIS LETTERS, 1998, 51 (3-4) : 177 - 181
  • [9] On the reduction kinetics of coprecipitated NiO-Al2O3 and NiO-La2O3-Al2O3 catalysts
    Wang, Xiaoguang
    Wei, Yongde
    Zhang, Jian
    Xu, Hengyong
    Li, Wenzhao
    [J]. REACTION KINETICS AND CATALYSIS LETTERS, 2006, 89 (01): : 97 - 104
  • [10] On the reduction kinetics of coprecipitated NiO-Al2O3 and NiO-La2O3-Al2O3 catalysts
    Xiaoguang Wang
    Yongde Wei
    Jian Zhang
    Hengyong Xu
    Wenzhao Li
    [J]. Reaction Kinetics and Catalysis Letters, 2006, 89 : 97 - 104