Fireside corrosion of superheater materials in chlorine containing flue gas

被引:14
|
作者
Valente, T [1 ]
机构
[1] Univ Roma La Sapienza, Dept Chem & Mat Engn, I-00184 Rome, Italy
关键词
9 Cr1Mo Steel; fireside corrosion; Sanicro; 28; steel; type 310 stainless steel;
D O I
10.1361/105994901770344773
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Corrosion resistance of three types of candidate materials for superheater sections under simulated waste incineration conditions was evaluated. A 9Cr1Mo steel, an AISI MOSS, and the Ni-based alloy Sanicro 28 were tested on a laboratory and on a pilot scale with different flue gas compositions (up to 2500 mg/Nm(3) of HCl and 1500 mg/Nm(3) of fly ash). Laboratory tests were carried out in a furnace up to 200 h. Metal and gas temperature were kept constant at 500 degreesC. Pilot scale tests were carried out by using a 0.3 X 0.3 m cross-sectional combustor, with flue gas velocity of 5 m/s. Air-cooled probes, designed to operate at a metal temperature of 500 degreesC and facing gas temperatures as high as 600 degreesC, were used for 200 h as maximum test time. Qualitative correspondence was found between results obtained by the two sets of experimental tests, but quantitative values were not comparable. Metallographic evaluations, metal loss measurements, and weight loss analysis evidenced as the most suitable alloy Sanicro28. Maximum metal loss observed was 240, 182, and 107 mum, respectively, for 9Cr1Mo, AISI310SS, and Sanicro 28 under the most aggressive conditions. Intergranular corrosion attack was evidenced for AlSI310SS, limiting the choice of materials to 9Cr1Mo and Sanicro 28, depending upon the lifetime expected at the design stage.
引用
收藏
页码:608 / 613
页数:6
相关论文
共 50 条
  • [1] Fireside corrosion of superheater materials in chlorine containing flue gas
    T. Valente
    [J]. Journal of Materials Engineering and Performance, 2001, 10 : 608 - 613
  • [2] Superheater corrosion in environments containing potassium and chlorine
    Salmenoja, K
    Makela, K
    Hupa, M
    Backman, R
    [J]. JOURNAL OF THE INSTITUTE OF ENERGY, 1996, 69 (480): : 155 - 162
  • [3] Effect of coal chlorine on the fireside corrosion of boiler furnace wall and superheater/reheater tubing
    James, PJ
    Pinder, LW
    [J]. MATERIALS AT HIGH TEMPERATURES, 1997, 14 (03) : 187 - 196
  • [4] High temperature erosion-corrosion of superheater materials and coatings in chlorine containing environments
    Uusitalo, M
    Kaipiainen, M
    Vuoristo, P
    Mäntylä, T
    [J]. HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 5, PTS 1 AND 2, 2001, 369-3 : 475 - 482
  • [5] Fireside corrosion of superheater materials under oxy-coal firing conditions
    Abang, Roger
    Lisk, Alexander
    Krautz, Hans Joachim
    [J]. EUROPEAN GEOSCIENCES UNION GENERAL ASSEMBLY 2013, EGUDIVISION ENERGY, RESOURCES & THE ENVIRONMENT, ERE, 2013, 40 : 304 - 311
  • [6] Laboratory corrosion tests for simulating fireside wastage of superheater materials in waste incinerators
    Otsuka, N
    Fukuda, Y
    Kawahara, Y
    Hosoda, T
    [J]. MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2000, 51 (04): : 236 - 241
  • [7] IMPROVED MATERIALS FOR COAL FIRED BOILER SUPERHEATER AND REHEATER TUBES SUBJECTED TO FIRESIDE CORROSION
    REHN, IM
    [J]. JOURNAL OF METALS, 1984, 36 (07): : 21 - 21
  • [8] SUPERHEATER FIRESIDE DEPOSITS AND CORROSION IN KRAFT RECOVERY BOILERS
    REEVE, DW
    TRAN, HN
    BARHAM, D
    [J]. TAPPI, 1981, 64 (05): : 109 - 113
  • [9] THE EFFECT OF FIRESIDE DEPOSITS ON KRAFT RECOVERY BOILER SUPERHEATER CORROSION
    TRAN, HN
    REEVE, DW
    BARHAM, D
    [J]. CIM BULLETIN, 1984, 77 (872): : 96 - 99
  • [10] THE EFFECT OF FIRESIDE DEPOSITS ON KRAFT RECOVERY BOILER SUPERHEATER CORROSION
    TRAN, HN
    REEVE, DW
    BARHAM, D
    [J]. CIM BULLETIN, 1982, 75 (842): : 125 - 125