Organosilane-functionalized hydrothermal-derived coatings on titanium alloys for hydrophobization and corrosion protection

被引:21
|
作者
Rahimipour, S. [1 ]
Rafiei, B. [1 ]
Salahinejad, E. [1 ]
机构
[1] KN Toosi Univ Technol, Fac Mat Sci & Engn, Tehran, Iran
关键词
Titanium-based alloys; Organosilanes; Surface free energy; Potentiodynamic polarization; Electrochemical impedance spectroscopy; SURFACE MODIFICATION; HEAT-TREATMENT; MILD-STEEL; TI METAL; BEHAVIOR; RESISTANCE; ROUGHNESS; COPPER; WETTABILITY; ADSORPTION;
D O I
10.1016/j.porgcoat.2020.105594
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
This work focuses on the structure, wettability and corrosion behaviors of Ti-6Al-4 V alloy after roughening treatments in different concentrations of NaOH aqueous solutions followed by low surface energy hexadecyl-trimethoxysilane (HDTMS) coating. In this regard, scanning electron microscopy, contact angle measurements, potentiodynamic polarization and electrochemical impedance spectroscopy were used to characterize the samples. In contrast to hydrophilicity caused by the hydrothermal alkaline treatments, the subsequent HDTMS coating donated considerable hydrophobicity. Typically, the highest sessile water contact angle (about 147 degrees) was obtained for the sample treated in 3 M NaOH solution followed by the HDTMS coating. In addition, the alkaline treatment reduced the corrosion resistance of the surface in a NaCl aqueous solution; however, the HDTMS hydrophobization process improved it significantly. It is eventually concluded that the coupled use of alkaline treatment and HDTMS functionalization can be further considered for moisture-exposed applications of Ti-based alloys.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] Titanium and Titanium Alloy Coatings for Corrosion Protection
    Zhou, Hong
    Gabbitas, Brian
    Mathews, Steven
    Zhang, Deliang
    TI-2011: PROCEEDINGS OF THE 12TH WORLD CONFERENCE ON TITANIUM, VOL III, 2012, : 1906 - 1910
  • [2] Recent Progress in Functionalized Coatings for Corrosion Protection of Magnesium Alloys-A Review
    Li, Bingzhi
    Zhang, Zhaoqi
    Liu, Tengteng
    Qiu, Zhenghui
    Su, Yan
    Zhang, Jinwei
    Lin, Cunguo
    Wang, Li
    MATERIALS, 2022, 15 (11)
  • [3] Organosilane-functionalized graphene oxide-epoxy nanocomposite coating: corrosion performance and self-healing properties
    Madani, S. M.
    Sangpour, P.
    Vaezi, M. R.
    Ramezanzadeh, B.
    Amani-Tehran, M.
    SURFACE TOPOGRAPHY-METROLOGY AND PROPERTIES, 2022, 10 (03)
  • [4] Technological Coatings for Protection of Titanium Alloys on Heating
    Kazakhskij Khimiko-Tekhnologicheskij, Inst, Alma-Ata, Kazakhstan
    Steklo Keram, 11 (27-29):
  • [5] Superhydrophobic coatings for corrosion protection of magnesium alloys
    Wenhui Yao
    Liang Wu
    Guangsheng Huang
    Bin Jiang
    rej Atrens
    Fusheng Pan
    Journal of Materials Science & Technology, 2020, 52 (17) : 100 - 118
  • [6] Superhydrophobic coatings for corrosion protection of magnesium alloys
    Yao, Wenhui
    Wu, Liang
    Huang, Guangsheng
    Jiang, Bin
    Atrens, Andrej
    Pan, Fusheng
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 52 : 100 - 118
  • [7] Corrosion Protection of Aluminum by Hydrophobization Using Nanoparticle Polymer Coatings Containing Plant Oil
    Samyn, Pieter
    JOURNAL OF THE BRAZILIAN CHEMICAL SOCIETY, 2014, 25 (05) : 947 - 960
  • [8] Trilaminar structure hydrophobic graphene oxide decorated organosilane composite coatings for corrosion protection
    Liang, Jiafeng
    Wu, Xiu-Wen
    Ling, Yunhan
    Yu, Siqi
    Zhang, Zhengjun
    SURFACE & COATINGS TECHNOLOGY, 2018, 339 : 65 - 77
  • [9] Preparation of MgO coatings on magnesium alloys for corrosion protection
    Lei, Ting
    Ouyang, Chun
    Tang, Wei
    Li, Lian-Feng
    Zhou, Le-Shan
    SURFACE & COATINGS TECHNOLOGY, 2010, 204 (23): : 3798 - 3803
  • [10] Functionalized chitosan-based coatings for active corrosion protection
    Carneiro, J.
    Tedim, J.
    Fernandes, S. C. M.
    Freire, C. S. R.
    Gandini, A.
    Ferreira, M. G. S.
    Zheludkevich, M. L.
    SURFACE & COATINGS TECHNOLOGY, 2013, 226 : 51 - 59