Degradation of MgO refractory in CaO-SiO2-MgO-FeOx and CaO-SiO2-Al2O3-MgO-FeOx slags under forced convection

被引:55
|
作者
Nightingale, SA [1 ]
Brooks, GA
Monaghan, BJ
机构
[1] Univ Wollongong, Fac Engn, Wollongong, NSW 2522, Australia
[2] CSIRO Minerals, Clayton, Vic 3169, Australia
基金
澳大利亚研究理事会;
关键词
D O I
10.1007/s11663-005-0036-x
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Experiments based on exposure of MgO to slags under forced convection flow conditions allowed the identification of different degradation mechanisms and the assessment of the role of Al2O3 in the degradation process. Slag with no alumina present resulted in direct dissolution. Samples immersed in alumina containing slag underwent indirect dissolution, with a spinel forming at the MgO-slag interface. At 1530 degrees C, the spinel was not effective in reducing the corrosion rate, as the scattered spinel grains were easily removed from the MgO surface. At 1500 degrees C, the loss of MgO was reduced due to the formation of a more cohesive spinel layer. Mechanical erosion then appears to play a greater role. Strength of the bond between the spinel and underlying MgO needs to be considered in strategies to reduce degradation of MgO refractories.
引用
收藏
页码:453 / 461
页数:9
相关论文
共 50 条
  • [1] Degradation of MgO refractory in CaO-SiO2-MgO-FeOx and CaO-SiO2-Al2O3-MgO-FeOx slags under forced convection
    S. A. Nightingale
    B. J. Monaghan
    G. A. Brooks
    [J]. Metallurgical and Materials Transactions B, 2005, 36 : 453 - 461
  • [2] REDOX EQUILIBRIA IN AL2O3-CAO-FEOX-SIO2 AND AL2O3-CAO-FEOX-MGO-SIO2 SLAGS
    JAHANSHAHI, S
    WRIGHT, S
    [J]. ISIJ INTERNATIONAL, 1993, 33 (01) : 195 - 203
  • [3] Penetration Behavior of CaO-SiO2-FeOx-MgO-(CaCl2) Slags in MgO Refractory
    Yan, Ziwen
    Deng, Zhiyin
    Zhu, Miaoyong
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2023, 54 (03): : 1582 - 1592
  • [4] Penetration Behavior of CaO–SiO2–FeOx–MgO–(CaCl2) Slags in MgO Refractory
    Ziwen Yan
    Zhiyin Deng
    Miaoyong Zhu
    [J]. Metallurgical and Materials Transactions B, 2023, 54 : 1582 - 1592
  • [5] Study of the Structure of FeOx-CaO-SiO2-MgO and FeOx-CaO-SiO2-MgO-Cu2O-PdO Slags Relevant to Urban Ores Processing through Cu Smelting
    Hasan, Mohammad Mehedi
    Rhamdhani, M. Akbar
    Shuva, M. Al Hossaini
    Brooks, Geoffrey A.
    [J]. METALS, 2020, 10 (01)
  • [6] Distribution of minor elements between MgO saturated FeOx-MgO-SiO2 or FeOx-CaO-MgO-SiO2 slag and nickel alloy
    Pagador, RU
    Hino, M
    Itagaki, K
    [J]. MATERIALS TRANSACTIONS JIM, 1999, 40 (03): : 225 - 232
  • [7] Activity of CaO in CaO-SiO2-Al2O3-MgO Slags
    Wen, Qiulin
    Shen, Fengman
    Zheng, Haiyan
    Yu, Jiyang
    Jiang, Xin
    Gao, Qiangjian
    [J]. ISIJ INTERNATIONAL, 2018, 58 (05) : 792 - 798
  • [8] Density of MgO-Al2O3-SiO2, MgO-CaO-SiO2 and MgO-CaO-Al2O3-SiO2 glasses and the structural role of MgO
    Doweidar, H.
    [J]. PHYSICS AND CHEMISTRY OF GLASSES-EUROPEAN JOURNAL OF GLASS SCIENCE AND TECHNOLOGY PART B, 2020, 61 (01): : 1 - 10
  • [9] LIQUID IMMISCIBILITY IN THE SYSTEM K2O-CAO-FEOX-MGO-AL2O3-SIO2
    COOK, LP
    NEGAS, T
    [J]. AMERICAN CERAMIC SOCIETY BULLETIN, 1979, 58 (03): : 352 - 352
  • [10] Experimental Investigation of the Viscosities in CaO-SiO2-MgO-Al2O3 and CaO-SiO2-MgO-Al2O3-TiO2 Slags
    Amitabh Shankar
    Mårten Görnerup
    A.K. Lahiri
    S. Seetharaman
    [J]. Metallurgical and Materials Transactions B, 2007, 38 : 911 - 915