Recycling glass fiber thermoplastic composites from wind turbine blades

被引:234
|
作者
Cousins, Dylan S. [1 ]
Suzuki, Yasuhito [2 ,4 ]
Murray, Robynne E. [3 ]
Samaniuk, Joseph R. [1 ]
Stebner, Aaron P. [2 ]
机构
[1] Colorado Sch Mines, Chem & Biol Engn, 1500 Illinois St, Golden, CO 80401 USA
[2] Colorado Sch Mines, Mech Engn, 1500 Illinois St, Golden, CO 80401 USA
[3] Natl Renewable Energy Lab, 15013 Denver West Pkwy, Golden, CO 80401 USA
[4] Osaka Prefecture Univ, Dept Appl Chem, Grad Sch Engn, Naka Ku, 1-1 Gakuen Cho, Sakai, Osaka 5998531, Japan
关键词
Thermoplastic; Recycling; Composite; Wind turbine blade; Dissolution; OF-THE-ART; REINFORCED COMPOSITES; ENERGY DEMAND; WASTE; PYROLYSIS; RECOVERY; EPOXY; TECHNOLOGIES; THERMOLYSIS; POLYMERS;
D O I
10.1016/j.jclepro.2018.10.286
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Thermoplastic resin systems have long been discussed for use in large-scale composite parts but have yet to be exploited by the energy industry. The use of these resins versus their thermosetting counterparts can potentially introduce cost savings due to non-heated tooling, shorter manufacturing cycle times, and recovery of raw materials from the retired part. Because composite parts have high embedded energy, recovery of their constituent materials can provide substantial economic benefit. This study determines the feasibility of recycling composite wind turbine blade components that are fabricated with glass fiber reinforced Elium (R) thermoplastic resin. Several experiments are conducted to tabulate important material properties that are relevant to recycling, including thermal degradation, grinding, and dissolution of the polymer matrix to recover the constituent materials. Dissolution, which is a process unique to thermoplastic matrices, allows recovery of both the polymer matrix and full-length glass fibers, which maintain their stiffness (190 N/(mm g)) and strength (160 N/g) through the recovery process. Injection molded regrind material is stiffer (12 GPa compared to 10 GPa) and stronger (150 MPa compared to 84 MPa) than virgin material that had shorter fibers. An economic analysis of the technical data shows that recycling thermoplastic-glass fiber composites via dissolution into their constituent parts is commercially feasible under certain conditions. This analysis concludes that 50% of the glass fiber must be recovered and resold for a price of $0.28/kg. Additionally, 90% of the resin must be recovered and resold at a price of $2.50/kg. (C) 2018 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1252 / 1263
页数:12
相关论文
共 50 条
  • [1] A review on recycling and reuse methods for carbon fiber/glass fiber composites waste from wind turbine blades
    Rani, Manjeet
    Choudhary, Priyanka
    Krishnan, Venkata
    Zafar, Sunny
    COMPOSITES PART B-ENGINEERING, 2021, 215
  • [2] Performance Drivers with Glass Fiber Composites for Wind Turbine Blades
    Serrano, J. C.
    Watson, J. C.
    Vennam, S.
    SAMPE JOURNAL, 2012, 48 (06) : 44 - 52
  • [3] Performance drivers with glass fiber composites for wind turbine blades
    Serrano, J.C., 1600, Soc. for the Advancement of Material and Process Engineering (48):
  • [4] A review of thermoplastic composites on wind turbine blades
    Cheng, Xiangrong
    Du, Bing
    He, Jia
    Long, Wanling
    Su, Guiyang
    Liu, Jingwei
    Fan, Zhenhua
    Chen, Liming
    COMPOSITES PART B-ENGINEERING, 2025, 299
  • [5] Wind turbine blades development using glass/fiber epoxy composites
    Golfman, Yosif
    JOURNAL OF ADVANCED MATERIALS, 2007, : 54 - 57
  • [6] Recycling of shredded composites from wind turbine blades in new thermoset polymer composites
    Beauson, Justine
    Madsen, Bo
    Toncelli, Chiara
    Brondsted, Povl
    Bech, Jakob Ilsted
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2016, 90 : 390 - 399
  • [7] Recovering glass fibers from waste wind turbine blades: Recycling methods, fiber properties, and potential utilization
    Xu, Ming-xin
    Ji, Hai-wen
    Wu, Ya-chang
    Meng, Xiang-xi
    Di, Jin-yi
    Yang, Jie
    Lu, Qiang
    RENEWABLE & SUSTAINABLE ENERGY REVIEWS, 2024, 202
  • [8] Interlaminar/interfiber failure of unidirectional glass fiber reinforced composites used for wind turbine blades
    Leong, Martin
    Overgaard, Lars C. T.
    Daniel, Isaac M.
    Lund, Erik
    Thomsen, Ole T.
    JOURNAL OF COMPOSITE MATERIALS, 2013, 47 (03) : 353 - 368
  • [9] HYDROTHERMAL AGEING OF GLASS/EPOXY COMPOSITES FOR WIND TURBINE BLADES
    Rocha, I. B. C. M.
    Raijmaekers, S.
    Nijssen, R. P. L.
    van der Meer, F. P.
    20TH INTERNATIONAL CONFERENCE ON COMPOSITE MATERIALS, 2015,
  • [10] Hybrid fiber and nanopowder reinforced composites for wind turbine blades
    Chikhradze, Nikoloz M.
    Marquis, Fernand D. S.
    Abashidze, Guram S.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2015, 4 (01): : 60 - 67