Analysis of catalyst deactivation during steam reforming of jet fuel on Ni-(PdRh)/γ-Al2O3 catalyst

被引:39
|
作者
Lakhapatri, Satish L. [1 ]
Abraham, Martin A. [2 ]
机构
[1] Univ Toledo, Dept Chem & Environm Engn, Toledo, OH 43606 USA
[2] Youngstown State Univ, Coll Sci Technol Engn & Math, Youngstown, OH 44555 USA
关键词
Steam reforming; Sulfur poisoning; Carbon deposition; Catalyst deactivation; Ni/Al2O3; STEM; Fuel cells; Transportation fuels; LIQUID HYDROCARBONS; HYDROGEN-PRODUCTION; N-HEXADECANE; SULFUR; TEMPERATURE; PLATINUM; SURFACES; RH; DEHYDROGENATION; REDUCTION;
D O I
10.1016/j.apcata.2011.08.004
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Catalyst deactivation during steam reforming of transportation fuels, primarily due to sulfur poisoning and carbon deposition, is a major hurdle in the commercialization of fuel cell technologies. In an attempt to better understand the phenomena, a previously formulated multi-component (Ni, Pd, Rh) catalyst supported on gamma-Al2O3 was studied under steam reforming of Jet A spiked with thiophene to achieve a total sulfur content of 1000 ppm by weight. Analysis of fresh catalysts showed the presence of two groups of active metal particles, primarily distinguished by their size and composition; small particles (1-5 nm) largely comprised of Rh and large particles (10-20 nm) that were predominantly Ni, with or without the presence of Pd. Analysis of used catalysts showed sintering of crystallites containing Ni but no identifiable growth in Rh crystallites. When complete conversion of sulfur compounds to hydrogen sulfide was observed, catalyst deactivation was minimized. However, when the conversion of sulfur compounds was low, significant catalyst deactivation was noted. In the presence of sulfur, increased amounts of cracking products were observed, suggesting that sulfur primarily affected the active sites responsible for steam reforming. Sulfur was preferentially adsorbed on the surface of Ni crystallites. It has been postulated that sulfur adsorption on Ni sites causes the initial deactivation of the catalyst which suppresses carbon gasification on the active sites, leading to the accumulation of carbon deposits over time. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:149 / 159
页数:11
相关论文
共 50 条
  • [1] A study of the deactivation of low loading Ni/Al2O3 steam reforming catalyst by tetrahydrothiophene
    Garbarino, Gabriella
    Romero Perez, Alvaro
    Finocchio, Elisabetta
    Busca, Guido
    CATALYSIS COMMUNICATIONS, 2013, 38 : 67 - 73
  • [2] Steam Methane Reforming Using an Anodic Alumina Supported Nickel Catalyst (Ni/Al2O3/Alloy): Analysis of Catalyst Deactivation
    Guo, Yu
    Thanh Phong Tran
    Zhou, Lu
    Zhang, Qi
    Kameyama, Hideo
    JOURNAL OF CHEMICAL ENGINEERING OF JAPAN, 2007, 40 (13) : 1221 - 1228
  • [3] Analysis of Ni/La2O3-αAl2O3 Catalyst Deactivation by Coke Deposition in the Ethanol Steam Reforming
    Montero, Carolina
    Valle, Beatriz
    Bilbao, Javier
    Gayubo, Ana G.
    ICONBM: INTERNATIONAL CONFERENCE ON BIOMASS, PTS 1 AND 2, 2014, 37 : 481 - 486
  • [4] Steam reforming of glycerol over Ni/Al2O3 catalyst
    Cheng, Chin Kui
    Foo, Say Yei
    Adesina, Adesoji A.
    CATALYSIS TODAY, 2011, 178 (01) : 25 - 33
  • [5] Bio-ethanol steam reforming on Ni/Al2O3 catalyst
    Comas, J
    Mariño, F
    Laborde, M
    Amadeo, N
    CHEMICAL ENGINEERING JOURNAL, 2004, 98 (1-2) : 61 - 68
  • [6] SIMPLIFIED KINETIC MODEL FOR STEAM REFORMING OF ETHANOL ON A NI/AL2O3 CATALYST
    Wu, Y. -J.
    Santos, J. C.
    Li, Ping
    Yu, J. -G.
    Cunha, A. F.
    Rodrigues, A. E.
    CANADIAN JOURNAL OF CHEMICAL ENGINEERING, 2014, 92 (01): : 116 - 130
  • [7] Methane Steam Reforming Kinetics on a Ni/Mg/K/Al2O3 Catalyst
    Robinson, Allison M.
    Gin, Megan E.
    Yung, Matthew M.
    TOPICS IN CATALYSIS, 2013, 56 (18-20) : 1708 - 1715
  • [8] Hydrogen from oxygenated solvents by steam reforming on Ni/Al2O3 catalyst
    Palmeri, N.
    Chiodo, V.
    Freni, S.
    Frusteri, F.
    Bart, J. C. J.
    Cavallaro, S.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2008, 33 (22) : 6627 - 6634
  • [9] Methane Steam Reforming Kinetics on a Ni/Mg/K/Al2O3 Catalyst
    Allison M. Robinson
    Megan E. Gin
    Matthew M. Yung
    Topics in Catalysis, 2013, 56 : 1708 - 1715
  • [10] Reaction Mechanism Development for Methane Steam Reforming on a Ni/Al2O3 Catalyst
    Richter, Jana
    Rachow, Fabian
    Israel, Johannes
    Roth, Norbert
    Charlafti, Evgenia
    Guenther, Vivien
    Flege, Jan Ingo
    Mauss, Fabian
    CATALYSTS, 2023, 13 (05)