摘要
An evaluation by hot dip galvanizing on steel after a 1; 2 and 3-minutes immersion was studied. These samples were carried out for evaluating microhardness and thickness measurements. Electrochemical techniques were used to determined the corrosion rate of steel in acid pickling 5; 10 and 16% HCl; rinsed with water of pH 2.50; 3.50 and 4.50 and hot dip galvanized steel in 3.5% NaCl. Certain operational parameters were analyzed, such as the aging bath (HCl), and elimination of the rinsing stage, to observe their influence in the hot dip galvanizing coating. It was found that an increase of coating thickness of hot dip galvanizing steel decreased the corrosion rate and the microhardness. Surfaces of alloy layer of the coating were examined by scanning electron microscope (SEM). SEM measurements was determined that when obvious the rinsing, the chlorine can be catched between two layers (interface), and soon migrates of the outermost alloy layer of the coating (Delta) towards the innermost one (Gamma).
引用
收藏
页码:188 / 197
页数:10
相关论文
共 50 条
  • [1] Operational factors affecting the hot dip galvanizing steel
    Sánchez, Miguel
    Contreras, Ramón
    Pérez, Orlando
    De Rincón, Oladis
    Campos, William
    Revista Tecnica de la Facultad de Ingenieria Universidad del Zulia, 2007, 30 (SPEC. ISSUE):
  • [2] Hot dip galvanizing of steel products
    Nowicka-Nowak, Marzenia
    OCHRONA PRZED KOROZJA, 2016, 59 (10): : 384 - 384
  • [3] Problems concerning hot dip galvanizing of steel
    Winkler, Rolf
    Zgraggen, Markus
    Rizvic, Naila
    Winkler, Markus
    STAHLBAU, 2010, 79 (05) : 363 - 369
  • [4] HOT DIP GALVANIZING STILL PROTECTING STEEL
    不详
    METALLURGIA, 1979, 46 (02): : 120 - 120
  • [5] Steel loss of hot-dip galvanizing
    Mei, Jianting
    Wu, Yongmin
    Cailiao Baohu/Materials Protection, 1997, 30 (07): : 12 - 13
  • [6] Environmental factors in failure during structural steel hot-dip galvanizing
    Carpio, J.
    Casado, J. A.
    Alvarez, J. A.
    Gutierrez-Solana, F.
    ENGINEERING FAILURE ANALYSIS, 2009, 16 (02) : 585 - 595
  • [7] THE HOT-DIP GALVANIZING OF STRUCTURAL STEEL SECTIONS
    PAINTER, RA
    PROCEEDINGS OF THE INSTITUTION OF ELECTRICAL ENGINEERS-LONDON, 1952, 99 (67): : 39 - 46
  • [8] Hot dip galvanizing
    不详
    ANTI-CORROSION METHODS AND MATERIALS, 1999, 46 (02) : 130 - 131
  • [9] Hot tip on hot dip: The pretreatment of hot dip galvanizing
    Feld, Michael
    Galvanotechnik, 2019, 110 (12): : 2213 - 2218
  • [10] PRINCIPLES AND POSSIBILITIES OF HOT-DIP GALVANIZING STEEL WIRE
    HORSTMANN, D
    STAHL UND EISEN, 1968, 88 (10): : 499 - +