Scanning Electrochemical Microscopy for the Investigation of Galvanic Corrosion of Iron with Zinc in 0.1 M NaCl Solution

被引:21
|
作者
Raj, X. Joseph [1 ]
Nishimura, T. [1 ]
机构
[1] Natl Inst Mat Sci, Res Ctr Strateg Mat, Mat Recycling Design Grp, 1-2-1 Sengen, Tsukuba, Ibaraki 3050047, Japan
关键词
corrosion; galvanic couple; iron; SECM; zinc; DEGRADATION PROCESSES; COATED METALS; COATINGS; SECM; VISUALIZATION; ELECTRODE; STEEL; MODE;
D O I
10.1007/s11665-015-1861-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Scanning electrochemical microscopy was used to monitor microscopic aspects of the electrochemical processes at the iron-zinc couple immersed in 0.1 M NaCl aqueous solution. The SECM measured the concentration of chemical species relevant to the corrosion processes. The electrochemical behavior of galvanic Fe/Zn coupling was investigated as a function of time using SECM microelectrode both as Fe/Zn joined together as well as away from each other. SECM amperometric line scan curves were obtained over the Fe/Zn at a constant distance. In the first case, the chemical species participating in the corrosion reactions at the sample are detected at the SECM tip by applying appropriate potential values to the microelectrode. The release of Zn2+ ionic species into the solution phase from local anodic sites, as well as the consumption of dissolved oxygen at the corresponding cathodic locations, was successfully monitored. The results revealed that the galvanic couple where Fe/Zn is close to each other will show higher corrosion rate of zinc than that of galvanic couple away from each other. The Fe/Zn couple away from each other showed a decrease in current values with time. This is due to the formation of oxide layer of Zn over the Fe followed by the protection of the corrosion products with further exposure times.
引用
下载
收藏
页码:474 / 486
页数:13
相关论文
共 50 条
  • [1] Scanning Electrochemical Microscopy for the Investigation of Galvanic Corrosion of Iron with Zinc in 0.1 M NaCl Solution
    X. Joseph Raj
    T. Nishimura
    Journal of Materials Engineering and Performance, 2016, 25 : 474 - 486
  • [2] Studies on galvanic corrosion of iron-magnesium couple by scanning electrochemical microscopy in 0.1 M NaCl solution
    Raj, X. Joseph
    Nishimura, T.
    JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY, 2016, 41 : 141 - 150
  • [3] Galvanic corrosion behaviour of iron coupled to aluminium in NaCl solution by scanning eectrochemical microscopy
    X. Joseph Raj
    T. Nishimura
    Protection of Metals and Physical Chemistry of Surfaces, 2016, 52 : 543 - 554
  • [4] Galvanic corrosion behaviour of iron coupled to aluminium in NaCl solution by scanning eectrochemical microscopy
    Raj, X. Joseph
    Nishimura, T.
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2016, 52 (03) : 543 - 554
  • [5] Electrochemical Investigation of the Galvanic Corrosion of AM60 and AD62 Magnesium Alloy in 0.1 M NaCl Solution
    Ikpi, Magdalene Edet
    Dong, Junhua
    Ke, Wei
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2015, 10 (01): : 552 - 563
  • [6] On the use of mercury-coated tips in scanning electrochemical microscopy to investigate galvanic corrosion processes involving zinc and iron
    Souto, Ricardo M.
    Gonzalez-Garcia, Yaiza
    Battistel, Dario
    Daniele, Salvatore
    CORROSION SCIENCE, 2012, 55 : 401 - 406
  • [7] Measurement of local galvanic surface corrosion using scanning electrochemical microscopy on ductile cast iron
    Tirdad Nickchi
    Paul Rostron
    Imad Barsoum
    Akram Alfantazi
    Journal of Materials Science, 2019, 54 : 9213 - 9221
  • [8] Measurement of local galvanic surface corrosion using scanning electrochemical microscopy on ductile cast iron
    Nickchi, Tirdad
    Rostron, Paul
    Barsoum, Imad
    Alfantazi, Akram
    JOURNAL OF MATERIALS SCIENCE, 2019, 54 (12) : 9213 - 9221
  • [9] Electrochemical corrosion performance of copper and uniformly alloyed bronze and brass in 0.1 M NaCl solution
    Khan, A. Abdullah
    Kaiser, S.
    Kaiser, M. Salim
    REVISTA MEXICANA DE FISICA, 2023, 69 (05)
  • [10] Propolis extract as corrosion inhibitor of iron alloy immersed in an ethylene glycol/water, 0.1 m NaCl solution
    Hachelef H.
    Khelifa A.
    Benmoussat A.
    Defect and Diffusion Forum, 2021, 406 : 265 - 273