Numerical study on Brazilian splitting of heat-treated sandstone under different contact angles

被引:0
|
作者
Xu Hao-chun [1 ,2 ,3 ]
Jin Ai-bing [1 ,2 ]
Zhao Yi-qing [1 ,2 ]
Chen Zhe [1 ,2 ,3 ]
机构
[1] Univ Sci & Technol Beijing, Key Lab, Minist Educ & Safety Met Mine, Beijing, Peoples R China
[2] Univ Sci & Technol Beijing, Sch Civil & Resources Engn, Beijing 100083, Peoples R China
[3] Univ Sci & Technol Beijing, Sch Adv Engineers, Beijing, Peoples R China
关键词
high temperature; Brazilian splitting; loading contact angle; crack propagation; particle flow code; TENSILE-STRENGTH; MECHANICAL-PROPERTIES; HIGH-TEMPERATURE; MICROSTRUCTURE; PARAMETERS; GRANITE;
D O I
10.16285/j.rsm.2021.1778
中图分类号
P5 [地质学];
学科分类号
0709 ; 081803 ;
摘要
Based on the particle flow code (PFC), the Brazilian splitting of sandstone treated at 25-1000 degrees C under different contact angles (2 alpha = 6 degrees-30 degrees) was carried out to study the stress distribution and fracture mode, and the Brazilian splitting was compared with the direct tensile test. The results show that: 1) The surface contact loading can reduce the end effect in Brazilian splitting. During the loading process, tensile cracks appear in the middle of the disc firstly. With the increase of the load, the tensile cracks converge and connect at the central part of the disc, and then extend to the end of the disc. 2) The tensile strength measured by Brazilian splitting at point contact of flat plate is less than that of direct tensile strength. The correction coefficient k of the tensile strength calculation formula decreases linearly with the increase of temperature 7', satisfying k = -3.303x10(-4)T+1.468. With the increase of the contact angle, the tensile strength of the Brazilian disc increases after heat treatment of different temperatures. 3) When 2 alpha >= 18 degrees, the Brazilian disc can guarantee to have a central crack initiation. When 2 alpha = 18 degrees-24 degrees, the fracture mode of the disk keeps unchanged at different temperatures. The disk will develop an inclined crack at a lower temperature (<= 600 degrees C) when the contact angle is too large (2 alpha = 30 degrees) Combined with the correction coefficient and the fracture mode analysis, the contact angle is recommended to be 18 degrees-24 degrees and the correction coefficient is between 0.802 6 and 0.856 0. It can ensure the center crack initiation and the stability of the fracture mode at different temperatures.
引用
收藏
页码:588 / 597
页数:10
相关论文
共 39 条
  • [1] Failure, crack initiation and the tensile strength of transversely isotropic rock using the Brazilian test
    Aliabadian, Zeinab
    Zhao, Gao-Feng
    Russell, Adrian R.
    [J]. INTERNATIONAL JOURNAL OF ROCK MECHANICS AND MINING SCIENCES, 2019, 122
  • [2] Crack development in transversely isotropic sandstone discs subjected to Brazilian tests observed using digital image correlation
    Aliabadian, Zeinab
    Zhao, Gao-Feng
    Russell, Adrian R.
    [J]. INTERNATIONAL JOURNAL OF ROCK MECHANICS AND MINING SCIENCES, 2019, 119 : 211 - 221
  • [3] Bieniawski Z. T., 1978, International Journal of Rock Mechanics and Mining Sciences & Geomechanics Abstracts, V15, P99, DOI 10.1016/0148-9062(78)90003-7
  • [4] ASTM, 2000, C49686 ASTM
  • [5] DISCRETE NUMERICAL-MODEL FOR GRANULAR ASSEMBLIES
    CUNDALL, PA
    STRACK, ODL
    [J]. GEOTECHNIQUE, 1979, 29 (01): : 47 - 65
  • [6] Influence of stress-induced and thermal cracking on physical properties and microstructure of La Peyratte granite
    David, C
    Menéndez, B
    Darot, M
    [J]. INTERNATIONAL JOURNAL OF ROCK MECHANICS AND MINING SCIENCES, 1999, 36 (04) : 433 - 448
  • [7] Loading Rate Effect of Rock Material with the Direct Tensile and Three Brazilian Disc Tests
    Gong, Fengqiang
    Zhang, Le
    Wang, Shanyong
    [J]. ADVANCES IN CIVIL ENGINEERING, 2019, 2019
  • [8] Effects of thermally-induced cracks on acoustic emission characteristics of granite under tensile conditions
    Guo, Pei
    Wu, Shunchuan
    Zhang, Guang
    Chu, Chaoqun
    [J]. INTERNATIONAL JOURNAL OF ROCK MECHANICS AND MINING SCIENCES, 2021, 144
  • [9] HU Bo, 2019, STUDY RHEOLOGICAL ME
  • [10] Huang YH, 2014, ROCK SOIL MECH, V35, P2269