Kinetic study on the thermo-oxidative degradation of glyceraldehyde under different oxygen concentrations

被引:6
|
作者
Shen, Dekui [1 ]
Yao, Shuheng [1 ]
Wu, Shiliang [1 ]
Liu, Qian [1 ]
Xiao, Rui [1 ]
机构
[1] Southeast Univ, Minist Educ, Key Lab Energy Thermal Convers & Control, Nanjing 210096, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
Glyceraldehyde; TG-FTIR; Oxidative decomposition; Consecutive kinetic model; Competitive kinetics model; THERMAL-DECOMPOSITION; LIGNOCELLULOSIC BIOMASS; CELLULOSE; PYROLYSIS; PRODUCTS;
D O I
10.1016/j.jaap.2015.04.016
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
The thermo-oxidative decomposition of glyceraldehyde under oxygen-contained atmospheres would be examined by TG-FTIR analysis involving mass loss history, evolution profiles of light gases and kinetic estimation. One mass loss stage around 140 degrees C ascribed to the polymerization of glyceraldehyde to intermediates is slightly influenced by the atmospheres. Another two main mass loss stages termed as the decomposition of produced intermediate and the sequent combustion of char residue was notably enhanced by the increased oxygen concentration. Two multi-step kinetic models considering the complex consecutive and competitive reactions are proposed to describe the decomposition process of glyceraldehyde under oxidative atmospheres. The acceptable fitting performance between experimental and calculated data can be obtained for both two kinetic models. The multi-step consecutive kinetic model is comparatively appropriate for describing the process, finding that the co-existence zone between the decomposition of glyceraldehyde and combustion of char is narrow during the thermo-oxidation process of glyceraldehyde. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:665 / 671
页数:7
相关论文
共 50 条
  • [1] Kinetic study of polypropylene nanocomposite thermo-oxidative degradation
    Lomakin, SM
    Dubnikova, IL
    Berezina, SM
    Zaikov, GE
    [J]. POLYMER INTERNATIONAL, 2005, 54 (07) : 999 - 1006
  • [2] Kinetic study of thermo-oxidative degradation of trans-polyalkenamers
    Giurginca, M
    Zahareucu, T
    [J]. POLYMER DEGRADATION AND STABILITY, 2002, 75 (02) : 267 - 271
  • [3] Study on thermo-oxidative aging characteristics of XLPE cable insulation under different oxygen concentration
    Huan Li
    Yingxin Shi
    Tao Liu
    Zhuobin Xi
    [J]. Journal of Materials Science: Materials in Electronics, 2023, 34
  • [4] Study on thermo-oxidative aging characteristics of XLPE cable insulation under different oxygen concentration
    Li, Huan
    Shi, Yingxin
    Liu, Tao
    Xi, Zhuobin
    [J]. JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2023, 34 (10)
  • [5] SPECTROSCOPIC STUDY OF THE THERMO-OXIDATIVE DEGRADATION OF POLYMETHACRYLONITRILE
    PLATONOVA, NV
    GRACHEV, VI
    KLIMENKO, IB
    GOLTSIN, BE
    SMIRNOV, LV
    [J]. VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA B, 1978, 20 (12): : 914 - 917
  • [6] Influence of environmental concentrations of ozone on thermo-oxidative degradation of PP
    Meijers, G
    Gijsman, P
    [J]. POLYMER DEGRADATION AND STABILITY, 2001, 74 (02) : 387 - 391
  • [7] Thermo-Oxidative Degradation of Hydroxypolychlorobiphenyls
    T. I. Gorbunova
    A. V. Maiorova
    T. V. Kulikova
    M. G. Pervova
    A. P. Safronov
    [J]. Russian Journal of General Chemistry, 2021, 91 : 1540 - 1545
  • [8] Thermo-Oxidative Degradation of Hydroxypolychlorobiphenyls
    Gorbunova, T., I
    Maiorova, A., V
    Kulikova, T., V
    Pervova, M. G.
    Safronov, A. P.
    [J]. RUSSIAN JOURNAL OF GENERAL CHEMISTRY, 2021, 91 (08) : 1540 - 1545
  • [9] A Kinetic Analysis of the Thermo-Oxidative Degradation of PU/POSS nanohybrid Elastomers
    Bartłomiej Janowski
    Krzysztof Pielichowski
    [J]. Silicon, 2016, 8 : 65 - 74
  • [10] Kinetic analysis of thermal and thermo-oxidative degradation of polyethylene (nano) composites
    Sirocic, Anita Pticek
    Krehula, Ljerka Kratofil
    Katancic, Zvonimir
    Hrnjak-Murgic, Zlata
    [J]. COMPOSITE INTERFACES, 2014, 21 (03) : 179 - 189