Effect of process parameters on microstructures and properties of Al-42Si alloy fabricated by selective laser melting

被引:7
|
作者
Cai, Xiaoye [1 ]
Liu, Tong [1 ,2 ]
Yan, Xuan [2 ]
Cheng, Zonghui [1 ]
Pan, Lu [3 ]
Tian, Zongjun [4 ]
Luo, Liangshun [5 ]
Su, Yanqing [5 ]
机构
[1] State Owned Wuhu Machinery Factory, Wuhu 241007, Peoples R China
[2] Anhui Polytech Univ, Anhui Key Lab High Performance Nonferrous Met Mat, Wuhu 241000, Peoples R China
[3] Anhui Tech Coll Mech & Elect Engn, Wuhu 241000, Peoples R China
[4] Nanjing Univ Aeronaut & Astronaut, Coll Mech & Elect Engn, Nanjing 210016, Peoples R China
[5] Anhui HIT3D Addit Technol Co Ltd, Wuhu 241200, Peoples R China
基金
中国国家自然科学基金;
关键词
A1-42Si alloy; Selective laser melting; Process parameters; Microstructures; MECHANICAL-PROPERTIES; HIGH-STRENGTH; PHASE; AL;
D O I
10.1016/j.heliyon.2022.e09680
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
In this paper, high-silicon Al-42Si alloy was prepared by selective laser melting (SLM) with different process parameters. Microstructures evolution and defects formation were studied and process parameters were optimized. The results shown that the density of SLM-fabricated Al-42Si alloy increases as input energy density increases. The highest and lowest density of SLM-fabricated Al-42Si alloy are obtained, when input energy density is 42.9J/mm(3) and 33.8J/mm(3) respectively. The microstructures of Al-42Si alloy fabricated by selective laser melting is mainly composed of primary silicon phase and eutectic silicon phase, which is distinct from casting alloy because of diffient grains size and shapes of the primary silicon. With higher energy density, larger size of the primary silicon observed during process due to higher heat released by powder. The size of primary silicon phase particles is in the range of 2.9-9.4 mu m, and the size of molten pool during SLM process is in the range of 125 +/- 10 mu m-140 +/- 10 mu m in this study. Also the hardness of SLM-fabricated Al-42Si alloy increases as input energy density increases between 40.0J/mm(3) and 42.9J/mm(3). After heat treatment, the residual stress is eliminated, microstructure stability and homogeneous of SLM-fabricated Al-42Si alloy are improved. The silicon distribution is more uniform and sizes increases about 1 similar to 2 mu m, and the hardness decreases after heat treatment. The optimal SLM parameters for Al-42Si alloy are laser power of 320W, scanning speed of 1355 mm/s, layer thickness of 50 mu m and scanning space of 110 mu m.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] Effect of Process Parameters on the Mechanical Properties of Hastelloy X Alloy Fabricated by Selective Laser Melting
    Ni, Xiaoqing
    Kong, Decheng
    Zhang, Liang
    Dong, Chaofang
    Song, Jia
    Wu, Wenheng
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (09) : 5533 - 5540
  • [2] Effect of Process Parameters on the Mechanical Properties of Hastelloy X Alloy Fabricated by Selective Laser Melting
    Xiaoqing Ni
    Decheng Kong
    Liang Zhang
    Chaofang Dong
    Jia Song
    Wenheng Wu
    Journal of Materials Engineering and Performance, 2019, 28 : 5533 - 5540
  • [3] Influence of process parameters and aging treatment on the microstructure and mechanical properties of Al Si8Mg3 alloy fabricated by selective laser melting
    Yaoxiang Geng
    Hao Tang
    Junhua Xu
    Yu Hou
    Yuxin Wang
    Zhen He
    Zhijie Zhang
    Hongbo Ju
    Lihua Yu
    InternationalJournalofMinerals,MetallurgyandMaterials, 2022, (09) : 1770 - 1779
  • [4] Microstructures and mechanical properties of Al-10%Si-0.4%Mg fabricated by selective laser melting
    Kimura, Takahiro
    Nakamoto, Takayuki
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2014, 61 (11): : 531 - 537
  • [5] The effect of hydrogen treatment on microstructures evolution and mechanical properties of titanium alloy fabricated by selective laser melting
    Guo, Yanhua
    Fang, Yuanzhi
    Dai, Guoqing
    Sun, Zhonggang
    Wang, Yaoqi
    Yuan, Qinfeng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 890
  • [6] Microstructures and Mechanical Properties of CoCrW Alloy Fabricated by Simulating Multibeam Selective Laser Melting
    Kuai, Zezhou
    Li, Zhonghua
    Bai, Peikang
    Nie, Yunfei
    Liu, Wenpeng
    Yang, Shuai
    Qi, Kai
    ADVANCED ENGINEERING MATERIALS, 2020, 22 (07)
  • [7] Microstructures and aging characteristics of Al-Mg-Sc alloy fabricated by selective laser melting
    KIMURA T.
    NAKAMOTO T.
    OZAKI T.
    MIKI T.
    HASHIZUME Y.
    MURAKAMI I.
    IMAI H.
    Keikinzoku/Journal of Japan Institute of Light Metals, 2020, 70 (10): : 467 - 474
  • [8] Erratum to: Influence of process parameters and aging treatment on the microstructure and mechanical properties of Al Si8Mg3 alloy fabricated by selective laser melting
    Yaoxiang Geng
    Hao Tang
    Junhua Xu
    Yu Hou
    Yuxin Wang
    Zhen He
    Zhijie Zhang
    Hongbo Ju
    Lihua Yu
    International Journal of Minerals,Metallurgy and Materials, 2022, (11) : 2086 - 2086
  • [9] The Effect of Recrystallization on Creep Properties of Alloy IN939 Fabricated by Selective Laser Melting Process
    Banoth, Santhosh
    Li, Chen-Wei
    Hiratsuka, Yo
    Kakehi, Koji
    METALS, 2020, 10 (08) : 1 - 16
  • [10] MICROSTRUCTURES AND TEXTURE OF INCONEL 718 ALLOY FABRICATED BY SELECTIVE LASER MELTING
    Li Shuai
    Wet Qingsong
    Zhang Dq
    Chua Chee Kai
    PROCEEDINGS OF THE 1ST INTERNATIONAL CONFERENCE ON PROGRESS IN ADDITIVE MANUFACTURING, 2014, : 139 - +