Challenges in Lift-Off Process Using CAMP Negative Photoresist in III-V IC Fabrication

被引:14
|
作者
Berkoh, Daniel [1 ]
Kulkarni, Sarang [1 ]
机构
[1] Skyworks Solut Inc, Proc Engn, Newbury Pk, CA 91320 USA
关键词
Lift-off; CAMP; negative photoresist; nLOF; loading effect; retrograde profile; bulk effect;
D O I
10.1109/TSM.2019.2944133
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In III-V IC processing, lift-off patterning is universally used. Historically used negative resist has its limitations; hence the image reverse process using positive tone resist has been utilized as the main work horse in lift-off applications. Metal lift-off processes using a specially designed chemically amplified (CAMP) negative tone resist have been evaluated for thin and thick metal layers to have a varying degree of success. Liftoff using CAMP photoresists has made it possible to reduce cycle time (similar to 57% reduction in 1x theoretical cycle time per layer) and reduce cost (due to elimination of steps) as compared to the image reverse process. However, achieving consistent lift-off and critical dimension (CD) control presents challenges, which are discussed in this paper.
引用
收藏
页码:513 / 517
页数:5
相关论文
共 50 条
  • [1] Applications for Epitaxial Lift-Off of III-V Materials
    Stender, C. L.
    Youtsey, C.
    Tuminello, F.
    Osowski, M.
    Adams, J.
    Elarde, V.
    Miyamoto, H.
    Wibowo, A.
    Hillier, G.
    Tatavarti, R.
    Pan, N.
    2014 LESTER EASTMAN CONFERENCE ON HIGH PERFORMANCE DEVICES (LEC), 2014,
  • [2] III-V ON SI - HETEROEPITAXY VERSUS LIFT-OFF TECHNIQUES
    DEBOECK, J
    BORGHS, G
    JOURNAL OF CRYSTAL GROWTH, 1993, 127 (1-4) : 85 - 92
  • [3] A review on epitaxial lift-off for III-V solar cells
    van der Woude, Daan
    Reboucasa, Lara Barros
    Vlieg, Elias
    Smits, Joost
    Schermer, John
    THIN SOLID FILMS, 2024, 808
  • [4] Epitaxial lift-off process for III-V solar cells by using porous germanium for substrate re-use
    Arvinte, Roxana
    Cailleaux, Samuel
    Mbeunmi, Alex Brice Poungoue
    Heintz, Alexandre
    Ares, Richard
    Boucherif, Abderraouf
    2020 47TH IEEE PHOTOVOLTAIC SPECIALISTS CONFERENCE (PVSC), 2020, : 1976 - 1981
  • [5] Modification of photoresist profile in lift-off process for MEMS application
    Nagarajan, R
    Kumar, R
    NANO- AND MICROTECHNOLOGY: MATERIALS, PROCESSES, PACKAGING, AND SYSTEMS, 2002, 4936 : 159 - 167
  • [6] FABRICATION OF AN ALL-REFRACTORY CIRCUIT USING LIFT-OFF WITH IMAGE-REVERSAL PHOTORESIST
    MEIER, DL
    PRZYBYSZ, JX
    KANG, J
    IEEE TRANSACTIONS ON MAGNETICS, 1991, 27 (02) : 3121 - 3124
  • [7] Integration of YAG:Ce Thin FilmWavelength Converter on III-V Blue LED via a Laser Lift-Off Process
    Kundaliya, Darshan
    von Malm, Norwin
    Mishra, K. C.
    ECS JOURNAL OF SOLID STATE SCIENCE AND TECHNOLOGY, 2018, 7 (01) : R3046 - R3051
  • [8] Fine patterning of ceramic thick layer on aerosol deposition by lift-off process using photoresist
    Akedo, Jun
    Park, Jaehyuk
    Tsuda, Hiroki
    JOURNAL OF ELECTROCERAMICS, 2009, 22 (1-3) : 319 - 326
  • [9] Fine patterning of ceramic thick layer on aerosol deposition by lift-off process using photoresist
    Jun Akedo
    Jaehyuk Park
    Hiroki Tsuda
    Journal of Electroceramics, 2009, 22 : 319 - 326
  • [10] High Separation Rate of Epitaxial Lift-Off Using Hydrophilic Solvent for III-V Solar Cell and Reusable Applications
    Horng, Ray-Hua
    Wu, Fan-Lei
    Ou, Sin-Liang
    Kao, Yu-Cheng
    2015 IEEE 42ND PHOTOVOLTAIC SPECIALIST CONFERENCE (PVSC), 2015,