摘要
Heat treatment is extensively used to accelerate the process of the strength development of concrete for prefabrication purposes. This study was conducted to determine the effect of cement composition on the improvement of the one-day flexural strength of heat-treated mortar prisms. Considering the strength gain at the end of one day of heat treatment application, it call be concluded that a treatment temperature of 80 degrees C seems to be appropriate for CC 32.5 cement while it is 65 degrees C for the other cements tested, It is also concluded that an initial curing of 4 h is suitable in view of the technical success of heat treatment application. However, it may be shorter for blended cements for economic reasons. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:818 / 822
页数:5
相关论文
共 50 条
  • [1] Heat of Hydration, Shrinkage, and Flexural Strength of Portland Limestone Cement Mortar
    Choudhary, Antara
    Ghantous, Rita M.
    Opdahl, Oliver H.
    Isgor, O. Burkan
    Weiss, W. Jason
    ADVANCES IN CIVIL ENGINEERING MATERIALS, 2022, 11 (01): : 500 - 519
  • [2] Influence of wetting-drying cycles on compressive and flexural strength of cement mortar and CFRP-mortar bond strength
    Noor-E-Khuda, Sarkar
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 271
  • [3] Analysis of the Flexural Tensile Strength and Modulus of Elasticity of Mortar Prisms.
    Ohler, A.
    Betonwerk und Fertigteil-Technik/Concrete Precasting Plant and Technology, 1987, 53 (03): : 183 - 189
  • [4] EFFECT OF LOADING RATE ON FLEXURAL STRENGTH OF CEMENT AND MORTAR
    MINDESS, S
    NADEAU, JS
    AMERICAN CERAMIC SOCIETY BULLETIN, 1977, 56 (04): : 429 - 430
  • [5] Influence of cement fineness and water-to-cement ratio on mortar early-age heat of hydration and set times
    Hu, Jiong
    Ge, Zhi
    Wang, Kejin
    CONSTRUCTION AND BUILDING MATERIALS, 2014, 50 : 657 - 663
  • [6] Pozzolanic behaviour and environmental efficiency of heat-treated fines as a partial cement replacement in mortar mixes
    Sharma, Prateek Kumar
    MacLeod, Alastair J.N.
    Aldridge, Laurie P.
    Collins, Frank
    Gates, Will P.
    Journal of Building Engineering, 2025, 99
  • [7] Influences of thermal damage on water transport in heat-treated cement mortar: Experimental and theoretical analyses
    Xue, Shanbin
    Zhang, Peng
    Wang, Junjie
    Bao, Jiuwen
    Han, Songbai
    He, Linfeng
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 288
  • [8] Mechanical Properties of Cement Mortar Containing Heat-Treated Boron Derivative Waste at Elevated Temperatures
    Kaman, Derya Over
    Koroglu, Levent
    Ayas, Erhan
    Tokyay, Mustafa
    Guney, Yucel
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2018, 30 (06)
  • [9] Variation of flexural strength of cement mortar attacked by sulfate ions
    Zhang, Ming-hua
    Jiang, Min-qiang
    Chen, Jian-kang
    ENGINEERING FRACTURE MECHANICS, 2008, 75 (17) : 4948 - 4957
  • [10] Influence of Sulfoaluminate Cement Addition on the Early Age Properties of CA Mortar
    Liu Zhichao
    Wang Fazhou
    Zhang Yunhua
    Hu Shuguang
    PROCEEDINGS OF THE 6TH ASIAN SYMPOSIUM ON POLYMERS IN CONCRETE, 2009, : 523 - 529