Lateral crushing properties of non-woven kenaf (mat)-reinforced epoxy composite hexagonal tubes

被引:15
|
作者
Alkbir, Munir Faraj Almbrouk [1 ]
Salit, Mohd Sapuan B. [1 ,2 ,3 ]
Aziz, Nuraini Bt. Abdul [1 ]
Ishak, Mohamad Ridzwan [3 ,4 ]
机构
[1] Univ Putra Malaysia, Dept Mech & Mfg Engn, Serdang 43400, Selangor, Malaysia
[2] Univ Putra Malaysia, Lab Bio Composite Technol, Inst Trop Forestry & Res Prod INTROP, Serdang 43400, Selangor, Malaysia
[3] Univ Putra Malaysia, AMRC, Serdang 43400, Selangor, Malaysia
[4] Univ Putra Malaysia, Dept Aerosp Engn, Serdang 43400, Selangor, Malaysia
关键词
Supporting plate; Specific energy absorption; Kenaf fiber; NATURAL FIBER-COMPOSITE; MECHANICAL-PROPERTIES; ENERGY-ABSORPTION; CRASHWORTHINESS CHARACTERISTICS; REINFORCED COMPOSITES; TENSILE PROPERTIES; THERMAL-PROPERTIES; SQUARE TUBES; BEHAVIOR; BANANA;
D O I
10.1007/s12541-016-0118-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The current study investigated the energy absorption capability and load carrying capacity of non-woven natural kenaf fiber (mat)/epoxy-hexagonal composite tubes subjected to a lateral quasi-static crushing test. The hexagonal composite tubes were manufactured by the hand lay-up technique. Natural non-woven kenaf (mat) was chosen as reinforcement due to low cost, low specific weight, easy processing, no need for tooling when dealing with the raw material, and no skin irritation and epoxy resin was used as the matrix to manufacture three configurations of beta=40A degrees, beta=50A degrees and beta=60A degrees of natural non-woven kenaf (mat)/epoxy laminate. The effects of hexagonal angles, supporting plate inside the tubes, and failure modes were studied by a lateral compression test. The crashworthiness of the tubes was evaluated by analysis of the specific energy absorption in quasi-static lateral compression. Specific energy absorption (SEA) was obtained from the load-displacement curve during testing. The failure mode of the tubes was analyzed from high-resolution photographs. Overall, the tube with beta=40A degrees had the best crashworthiness among the tubes. Furthermore, the results showed that the tubes with supporting plates have better specific energy absorption for all tested specimens and exhibited approximately 69% better crashworthiness than the non-supporting ones. The results also demonstrated that all specimens failed by the longitudinal failure mode.
引用
收藏
页码:965 / 972
页数:8
相关论文
共 50 条
  • [1] Lateral crushing properties of non-woven kenaf (mat)-reinforced epoxy composite hexagonal tubes
    Munir Faraj Almbrouk Alkbir
    Mohd Sapuan b. Salit
    Nuraini bt. Abdul Aziz
    Mohamad Ridzwan Ishak
    International Journal of Precision Engineering and Manufacturing, 2016, 17 : 965 - 972
  • [2] Experimental Quasi-Static Axial Crushing of Non-Woven Kenaf Fibre/Epoxy Hexagonal Composite Tubes
    Ikbir, Munir Faraj M. A.
    Sapuan, S. M.
    Nuraini, A. A.
    Ishak, Mohamad Ridzwan
    ADVANCES IN MECHANICAL AND MANUFACTURING ENGINEERING, 2014, 564 : 361 - +
  • [3] The Effect of Woven and Non-Woven Fiber Structure on Mechanical Properties Polyester Composite Reinforced Kenaf
    Ratim, S.
    Bonnia, N. N.
    Surip, S. N.
    2ND ASEAN - APCTP WORKSHOP ON ADVANCED MATERIALS SCIENCE AND NANOTECHNOLOGY (AMSN 2010), 2012, 1455 : 131 - 135
  • [4] Thermomechanical and dynamic mechanical properties of bamboo/woven kenaf mat reinforced epoxy hybrid composites
    Chee, Siew Sand
    Jawaid, Mohammad
    Sultan, M. T. H.
    Alothman, Othman Y.
    Abdullah, Luqman Chuah
    COMPOSITES PART B-ENGINEERING, 2019, 163 : 165 - 174
  • [5] Physical and Mechanical Properties of Woven Kenaf/Bamboo Fiber Mat Reinforced Epoxy Hybrid Composites
    Ismail, Ahmad Safwan
    Jawaid, Mohammad
    Sultan, Mohamed T. H.
    Hassan, Azman
    BIORESOURCES, 2019, 14 (01): : 1390 - 1404
  • [6] Performance of jute non-woven mat reinforced polyester matrix composite in multilayered armor
    de Assis, Foluke Salgado
    Pereira, Artur Camposo
    Garcia Filho, Fabio da Costa
    Lima, Edio Pereira, Jr.
    Monteiro, Sergio Neves
    Weber, Ricardo Ponde
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2018, 7 (04): : 535 - 540
  • [7] Crushing behavior of kenaf fiber/wooden stick reinforced epoxy hybrid "green" composite elliptical tubes
    Alkateb, Mohamed
    Sapuan, S. M.
    Leman, Z.
    Jawaid, M.
    Ishak, M. R.
    POLIMERY, 2018, 63 (06) : 436 - 443
  • [8] Performance of Kenaf Non-woven Mat/PLA Biocomposites under Medium Velocity Impact
    Mufaro Moyo
    Krishnan Kanny
    Raman Velmurugan
    Fibers and Polymers, 2020, 21 : 2642 - 2651
  • [9] Performance of Kenaf Non-woven Mat/PLA Biocomposites under Medium Velocity Impact
    Moyo, Mufaro
    Kanny, Krishnan
    Velmurugan, Raman
    FIBERS AND POLYMERS, 2020, 21 (11) : 2642 - 2651
  • [10] Thermal Properties of Woven Kenaf/Carbon Fibre-Reinforced Epoxy Hybrid Composite Panels
    Aisyah, H. A.
    Paridah, M. T.
    Sapuan, S. M.
    Khalina, A.
    Berkalp, O. B.
    Lee, S. H.
    Lee, C. H.
    Nurazzi, N. M.
    Ramli, N.
    Wahab, M. S.
    Ilyas, R. A.
    INTERNATIONAL JOURNAL OF POLYMER SCIENCE, 2019, 2019