Development of a new single-bottle multi-purpose primer for bonding to dental porcelain, alumina, zirconia, and dental gold alloy

被引:12
|
作者
Ikemura, Kunio [1 ]
Tanaka, Hisaki [1 ]
Fujii, Toshihide [1 ]
Deguchi, Mikito [1 ]
Endo, Takeshi [2 ]
Kadoma, Yoshinori [3 ]
机构
[1] Shofu Inc, Dept Res & Dev, Higashiyama Ku, Kyoto 6050983, Japan
[2] Kinki Univ, Mol Engn Inst, Fukuoka 8208555, Japan
[3] Tokyo Med & Dent Univ, Dept Appl Funct Mol, Div Biofunct Mol, Inst Biomat & Bioengn,Chiyoda Ku, Tokyo 1010062, Japan
关键词
Dithiooctanoate monomer; Phosphonic acid monomer; Silane coupling agent; Multi-purpose primer; PHOSPHONIC ACID MONOMERS; OF-THE-LITERATURE; LUTING AGENT; RESIN; RESTORATIONS; DURABILITY; ADHESIVES; SURFACES; RAMAN; AU;
D O I
10.4012/dmj.2010-182
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
This study investigated the bonding efficacy of a combined primer application which comprised a silane coupling agent, an acidic adhesive monomer, and a dithiooctanoate monomer, as well as the influence of shelf life on bonding. Five experimental primers (coded as Si-P-SS-1 to Si-P-SS-4, and Si-SS as the control) were prepared using 20.0-40.0 wt% 3-methacryloyloxypropyltriethoxysilane (3-MPTES), 0-7.44 wt% 6-methacryloyloxyhexyl phosphonoacetate (6-MHPA), and 0.50 wt% 10-methacryloyloxydecyl 6,8-dithiooctanoate (10-MDDT). After 24-hour storage at 23 degrees C (Initial) and 2-month storage at 50 degrees C (Aged), tensile bond strengths (TBSs) of a resin cement (ResiCem, Shofu Inc., Kyoto, Japan) to primer-treated porcelain, alumina, zirconia, and Au alloy were measured. With the Initial and Aged primers of Si-P-SS-1 to Si-P-SS-3, there were no statistically significant differences in the mean TBSs (MPa) [porcelain: 21.7-29.2; alumina: 21.4-25.3; zirconia: 20.3-24.5; and Au alloy: 23.4-27.6] among these three primers (p>0.05), but they were significantly higher than that of the control primer (p<0.05). The experimental primers Si-P-SS-1 to Si-P-SS-3 demonstrated good potential as multi-purpose primers: they had good shelf lives as single-bottle primer systems and were thus able to exhibit good bond strength to all the adherends tested after 2-month storage under accelerated aging conditions.
引用
收藏
页码:478 / 484
页数:7
相关论文
共 14 条
  • [1] Effects of a newly designed HEMA-free, multi-purpose, single-bottle, self-etching adhesive on bonding to dental hard tissues, zirconia-based ceramics, and gold alloy
    Department of Research and Development, Shofu Inc, 11 Kamitakamatsu-cho, Fukuine, Higashiyama-ku, Kyoto 605-0983, Japan
    不详
    不详
    Dent. Mater. J., 5 (616-625):
  • [2] Effects of a newly designed HEMA-free, multi-purpose, single-bottle, self-etching adhesive on bonding to dental hard tissues, zirconia-based ceramics, and gold alloy
    Ikemura, Kunio
    Jogetsu, Yoshiyuki
    Shinno, Kazuya
    Nakatsuka, Toshiyuki
    Endo, Takeshi
    Kadoma, Yoshinori
    DENTAL MATERIALS JOURNAL, 2011, 30 (05) : 616 - 625
  • [3] BONDING OF DENTAL PORCELAIN TO METAL .1. GOLD ALLOY/PORCELAIN BOND
    MCLEAN, JW
    SCED, IR
    TRANSACTIONS AND JOURNAL OF THE BRITISH CERAMIC SOCIETY, 1973, 72 (05): : 229 - 233
  • [4] Age-hardening by miscibility limit in a multi-purpose dental gold alloy containing platinum
    Hyo-Joung Seol
    Joo-Hee Park
    Ri-Mo Ku
    Mi-Gyoung Park
    Yong Hoon Kwon
    Hyung-Il Kim
    Gold Bulletin, 2010, 43 : 42 - 48
  • [5] Age-hardening by miscibility limit in a multi-purpose dental gold alloy containing platinum
    Seol, Hyo-Joung
    Park, Joo-Hee
    Ku, Ri-Mo
    Park, Mi-Gyoung
    Kwon, Yong Hoon
    Kim, Hyung-Il
    GOLD BULLETIN, 2010, 43 (01) : 42 - 48
  • [6] Ageing reactions in a high carat gold alloy for dental porcelain bonding
    Hisatsune, K
    Tanaka, Y
    Udoh, K
    Yasuda, K
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 1997, 8 (05) : 277 - 282
  • [7] Ageing reactions in a high carat gold alloy for dental porcelain bonding
    Dept. of Dental Materials Science, Nagasaki University, School of Dentistry, Nagasaki 852, Japan
    J. MATER. SCI. MATER. MED., 5 (277-282):
  • [8] Ageing reactions in a high carat gold alloy for dental porcelain bonding
    K HISATSUNE
    Y TANAKA
    K UDOH
    K YASUDA
    Journal of Materials Science: Materials in Medicine, 1997, 8 : 277 - 282
  • [9] A Pd-free high gold dental alloy for porcelain bonding
    JN Wang
    WB Liu
    Gold Bulletin, 2006, 39 : 114 - 120
  • [10] A Pd-free high gold dental alloy for porcelain bonding
    Wang, J. N.
    Liu, W. B.
    GOLD BULLETIN, 2006, 39 (03) : 114 - 120