Serrated Flow and Dynamic Strain Aging in Fe-Mn-C TWIP Steel

被引:19
|
作者
Lan, Peng [1 ]
Zhang, Jiaquan [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 10083, Peoples R China
基金
中国国家自然科学基金; 北京市自然科学基金; 中国博士后科学基金;
关键词
INDUCED PLASTICITY STEELS; STACKING-FAULT ENERGY; AUSTENITIC STEEL; MECHANICAL-PROPERTIES; SOLIDIFICATION MICROSTRUCTURE; DEFORMATION MECHANISMS; HOT DUCTILITY; EVOLUTION; BEHAVIOR; TRANSFORMATION;
D O I
10.1007/s11661-017-4421-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The tensile behavior, serrated flow, and dynamic strain aging of Fe-(20 to 24)Mn-(0.4 to 0.6)C twinning-induced plasticity (TWIP) steel have been investigated. A mathematical approach to analyze the DSA and PLC band parameters has been developed. For Fe-(20 to 24)Mn-(0.4 to 0.6)C TWIP steel with a theoretical ordering index (TOI) between 0.1 and 0.3, DSA can occur at the very beginning of plastic deformation and provide serrations during work hardening, while for TOI less than 0.1 the occurrence of DSA is delayed and twinning-dominant work hardening remains relatively smooth. The critical strain for the onset of DSA and PLC bands in Fe-Mn-C TWIP steels decreases as C content increases, while the numbers of serrations and bands increase. As Mn content increases, the critical strain for DSA and PLC band varies irregularly, but the numbers of serrations and bands increase. For Fe-(20 to 24)Mn-(0.4 to 0.6)C TWIP steel with grain size of about 10 to 20 mu m, the twinning-induced work hardening rate is about 2.5 to 3.0 GPa, while the DSA-dominant hardening rate is about 2.0 GPa on average. With increasing engineering strain from 0.01 to 0.55 at an applied strain rate of 0.001s(-1), the cycle time for PLC bands in Fe-Mn-C TWIP steel increases from 6.5 to 162 seconds, while the band velocity decreases from 4.5 to 0.5 mm s(-1), and the band strain increases from 0.005 to 0.08. Increasing applied strain rate leads to a linear increase of band velocity despite composition differences. In addition, the influence of the Mn and C content on the tensile properties of Fe-Mn-C TWIP steel has been also studied. As C content increases, the yield strength and tensile strength of Fe-Mn-C TWIP steel increase, but the total elongation variation against C content is dependent on Mn content. As Mn content increases, the yield strength and tensile strength decrease, while the total elongation increases, despite C content. Taking both tensile properties and serrated flow behavior into consideration, Fe-22Mn-0.4C TWIP steel shows excellent mechanical performance with a high product of tensile strength and total elongation and a slightly serrated stress-strain response. To suppress the negative effect of DSA in Fe-Mn-C TWIP steels on the stability of tensile behavior, a TOI lower than 0.1 is strongly suggested. (C) The Minerals, Metals & Materials Society and ASM International 2017
引用
收藏
页码:147 / 161
页数:15
相关论文
共 50 条
  • [1] Serrated Flow and Dynamic Strain Aging in Fe-Mn-C TWIP Steel
    Peng Lan
    Jiaquan Zhang
    Metallurgical and Materials Transactions A, 2018, 49 : 147 - 161
  • [2] Twinning and dynamic strain aging behavior during tensile deformation of Fe-Mn-C TWIP steel
    Lan, Peng
    Zhang, Jiaquan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 700 : 250 - 258
  • [3] Influence of Dislocation Separation on Dynamic Strain Aging in a Fe-Mn-C Austenitic Steel
    Koyama, Motomichi
    Sawaguchi, Takahiro
    Tsuzaki, Kaneaki
    MATERIALS TRANSACTIONS, 2012, 53 (03) : 546 - 552
  • [4] Microstructure Characteristics of an Fe-Mn-C TWIP Steel After Deformation
    DAI Yong-juan1
    2.School of Materials Science and Engineering
    Journal of Iron and Steel Research(International), 2010, 17 (09) : 53 - 59
  • [5] Microstructure Characteristics of an Fe-Mn-C TWIP Steel After Deformation
    Yong-juan Dai
    Di Tang
    Zhen-li Mi
    Jian-chong LÜ
    Journal of Iron and Steel Research International, 2010, 17 : 53 - 59
  • [6] Microstructure Characteristics of an Fe-Mn-C TWIP Steel After Deformation
    Dai Yong-juan
    Tang Di
    Mi Zhen-li
    Lue Jian-chong
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2010, 17 (09) : 53 - 59
  • [7] SERRATED FLOW IN AUSTENITIC FE-MN-C AND FE-MN-AL-C ALLOYS
    SHUN, TS
    WAN, CM
    BYRNE, JG
    SCRIPTA METALLURGICA ET MATERIALIA, 1991, 25 (08): : 1769 - 1774
  • [8] Mechanical behavior of Fe-Mn-C TWIP steel under high strain rate impact loading
    Gao, Yong-Liang
    Hu, Shi-Lian
    Chen, Wei
    Tian, Yu-Jiang
    Yang, Yang
    Sun, Guo-Jin
    He, Yong
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2015, 36 (09): : 119 - 123
  • [9] Effect of alloying elements on mechanical behavior of Fe-Mn-C TWIP steel
    Wang, Yu-Chang
    Lan, Peng
    Li, Yang
    Zhang, Jia-Quan
    Cailiao Gongcheng/Journal of Materials Engineering, 2015, 43 (09): : 30 - 38
  • [10] Inverse grain size dependence of critical strain for serrated flow in a Fe-Mn-C twinning-induced plasticity steel
    Koyama, Motomichi
    Sawaguchi, Takahiro
    Tsuzaki, Kaneaki
    PHILOSOPHICAL MAGAZINE LETTERS, 2012, 92 (03) : 145 - 152