Fatigue Performance of an Additively Manufactured Zr-Based Bulk Metallic Glass and the Effect of Post-Processing

被引:11
|
作者
Sohrabi, Navid [1 ]
Hamidi-Nasab, Milad [1 ,2 ]
Rouxel, Baptiste [1 ]
Jhabvala, Jamasp [1 ]
Parrilli, Annapaola [3 ]
Vedani, Maurizio [2 ]
Loge, Roland E. [1 ]
机构
[1] Ecole Polytech Fed Lausanne EPFL, PX Grp Chair, Thermomech Met Lab LMTM, CH-2002 Neuchatel, Switzerland
[2] Politecn Milan, Dept Mech Engn, I-20156 Milan, Italy
[3] Swiss Fed Labs Mat Sci & Technol Empa, Ctr Xray Analyt, Uberlandstr 129, CH-8600 Dubendorf, Switzerland
关键词
bulk metallic glass; fatigue; laser powder-bed fusion; laser shock peening; defects; FRACTURE-BEHAVIOR; CRACK PROPAGATION; SHEAR BANDS; FREE-VOLUME; TOUGHNESS; DEFECTS; CRYSTALLIZATION; CRYSTALLINITY; RELAXATION; MECHANISMS;
D O I
10.3390/met11071064
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fatigue is the most common cause of failure of mechanical parts in engineering applications. In the current work, we investigate the fatigue life of a bulk metallic (BMG) glass fabricated via additive manufacturing. Specimens fabricated via laser powder-bed fusion (LPBF) are shown to have a fatigue ratio of 0.20 (fatigue limit of 175 MPa) in a three-point bending fatigue test. Three strategies for improving the fatigue behavior were tested, namely (1) relaxation heat treatment, giving a slight fatigue life improvement at high loading conditions (>= 250 MPa), (2) laser shock peening, and (3) changing the build orientation, the latter two of which yielded no significant effects. It was found that the presence of lack of fusion (LoF) had the preponderant effect on fatigue resistance of the specimens manufactured. LoF was observed to be a source of stress localization and initiation of cracks. The fatigue life in BMGs fabricated by LPBF is thus primarily influenced by powder quality and process-induced defects, which cannot be removed by the post-treatments carried out in this study. It is believed that a slight increase in laser power, either in the near-surface regions or in the core of the specimens, could improve the fatigue behavior despite the associated (detrimental) increase of crystallized fraction.
引用
收藏
页数:19
相关论文
共 50 条
  • [1] Thermoplastic forming of additively manufactured Zr-based bulk metallic glass: A processing route for surface finishing of complex structures
    Frey, Maximilian
    Wegner, Jan
    Neuber, Nico
    Reiplinger, Benedikt
    Bochtler, Benedikt
    Adam, Bastian
    Ruschel, Lucas
    Riegler, Sascha Sebastian
    Jiang, Hao-Ran
    Kleszczynski, Stefan
    Witt, Gerd
    Busch, Ralf
    [J]. MATERIALS & DESIGN, 2021, 198
  • [2] Fracture and fatigue behaviour of a laser additive manufactured Zr-based bulk metallic glass
    Best, James P.
    Ostergaard, Halsey E.
    Li, Bosong
    Stolpe, Moritz
    Yang, Fan
    Nomoto, Keita
    Hasib, M. Tarik
    Muransky, Ondrej
    Busch, Ralf
    Li, Xiaopeng
    Kruzic, Jamie J.
    [J]. ADDITIVE MANUFACTURING, 2020, 36
  • [3] Effect of nanocrystalline dispersion on fatigue in a Zr-based bulk metallic glass
    Fujita, K
    Takayama, T
    Inoue, A
    Zhang, T
    Kimura, H
    [J]. JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2003, 67 (02) : 79 - 84
  • [4] Notched fatigue of Zr-based bulk metallic glass
    Nakai, Yoshikazu
    Sei, Naoki
    Kim, Bok-Key
    [J]. MECHANICAL BEHAVIOR OF MATERIALS X, PTS 1AND 2, 2007, 345-346 : 259 - +
  • [5] Fatigue characteristics of a Zr-based bulk metallic glass
    Wang, G. Y.
    Liaw, P. K.
    Smyth, A.
    Denda, M.
    Peker, A.
    Freels, M.
    Buchanan, R. A.
    Brooks, C. R.
    [J]. REVIEWS ON ADVANCED MATERIALS SCIENCE, 2008, 18 (01) : 18 - 22
  • [6] Fracture and fatigue in a Zr-based bulk metallic glass
    Gilbert, CJ
    Schroeder, V
    Ritchie, RO
    [J]. BULK METALLIC GLASSES, 1999, 554 : 343 - 354
  • [7] Influence of powder characteristics on the structural and the mechanical properties of additively manufactured Zr-based bulk metallic glass
    Wegner, Jan
    Frey, Maximilian
    Piechotta, Markus
    Neuber, Nico
    Adam, Bastian
    Platt, Sebastian
    Ruschel, Lucas
    Schnell, Norman
    Riegler, Sascha Sebastian
    Jiang, Hao-Ran
    Witt, Gerd
    Busch, Ralf
    Kleszczynski, Stefan
    [J]. MATERIALS & DESIGN, 2021, 209
  • [8] The fatigue endurance limit of a Zr-based bulk metallic glass
    Menzel, Brian C.
    Dauskardt, Reinhold H.
    [J]. SCRIPTA MATERIALIA, 2006, 55 (07) : 601 - 604
  • [9] Post-processing of additively manufactured metallic alloys - A review
    Malakizadi, Amir
    Mallipeddi, Dinesh
    Dadbakhsh, Sasan
    M'Saoubi, Rachid
    Krajnik, Peter
    [J]. INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2022, 179
  • [10] Effect of shot peening on the fatigue life of a Zr-based bulk metallic glass
    Raghavan, R.
    Ayer, R.
    Jin, H. W.
    Marzinsky, C. N.
    Ramamurty, U.
    [J]. SCRIPTA MATERIALIA, 2008, 59 (02) : 167 - 170