Stellite 21 coatings on AISI 410 martensitic stainless steel by gas tungsten arc welding

被引:8
|
作者
Laridjani, M. S. [1 ]
Amadeh, A. [1 ]
Kashani, H. [1 ]
机构
[1] Univ Tehran, Sch Met & Mat Engn, Univ Coll Engn, Tehran, Iran
关键词
Martensitic stainless steels; Stellite; 21; GTAW; Microstructure; Corrosion; HARDFACING ALLOYS; MECHANICAL-PROPERTIES; WEAR-RESISTANCE; TURBINE-BLADES; PART; MICROSTRUCTURE; CORROSION; MO; TRANSFORMATION; DEGRADATION;
D O I
10.1179/174328409X463234
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Degradation of AISI 410 martensitic stainless steel, a typical alloy for many applications such as steam turbine blade, could impair its efficiency and lifetime. To overcome this problem, critical surfaces could be modified by weld cladding via gas tungsten arc welding technique. In the present research, a comparative study of Stellite 21 weld overlays deposited in three different thicknesses, i.e. dilutions, at various preheat and post-weld heat treatment temperatures on the surface of AISI 410 martensitic stainless steel, has been made. The surface of coatings has been examined to reveal their microstructures, phase characterisation and mechanical properties using XRD, microhardness tester and metallographic techniques. The results showed that the deposition of Stellite 21 coating on AISI 410 martensitic stainless steel improved its corrosion resistance. Moreover, the volumetric dilution had a considerable effect on the hardness, microstructure and electrochemical corrosion behaviour of Stellite 21 weld overlays.
引用
收藏
页码:1184 / 1190
页数:7
相关论文
共 50 条
  • [1] Characterization of friction surfaced martensitic stainless steel (AISI 410) coatings
    Puli, Ramesh
    Kumar, E. Nandha
    Ram, G. D. Janaki
    [J]. TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2011, 64 (1-2) : 41 - 45
  • [2] Characterization of friction surfaced martensitic stainless steel (AISI 410) coatings
    Ramesh Puli
    E. Nandha Kumar
    G. D. Janaki Ram
    [J]. Transactions of the Indian Institute of Metals, 2011, 64
  • [3] Wear and corrosion performance of AISI 410 martensitic stainless steel coatings produced using friction surfacing and manual metal arc welding
    Puli, Ramesh
    Ram, G. D. Janaki
    [J]. SURFACE & COATINGS TECHNOLOGY, 2012, 209 : 1 - 7
  • [4] Keyhole gas tungsten arc welding of AISI 316L stainless steel
    Feng, Yueqiao
    Luo, Zhen
    Liu, Zuming
    Li, Yang
    Luo, Yucan
    Huang, Yongxian
    [J]. MATERIALS & DESIGN, 2015, 85 : 24 - 31
  • [5] Hydrogen Cracking in Gas Tungsten Arc Welding of an AISI Type 321 Stainless Steel
    Rozenak, P.
    Unigovsk, Ya.
    Shneck, R.
    [J]. ENERGY MATERIALS CONFERENCE PROCEEDINGS 2014, 2014, : 711 - 716
  • [6] Investigating the effect of arc offsetting in AISI 304 stainless steel and copper welding using gas tungsten arc welding
    Gurdeep Singh
    Ravindra K. Saxena
    Sunil Pandey
    [J]. Journal of the Brazilian Society of Mechanical Sciences and Engineering, 2021, 43
  • [7] Investigating the effect of arc offsetting in AISI 304 stainless steel and copper welding using gas tungsten arc welding
    Singh, Gurdeep
    Saxena, Ravindra K.
    Pandey, Sunil
    [J]. JOURNAL OF THE BRAZILIAN SOCIETY OF MECHANICAL SCIENCES AND ENGINEERING, 2021, 43 (03)
  • [8] Modeling of Linear Gas Tungsten Arc Welding of Stainless Steel
    P. Maran
    T. Sornakumar
    T. Sundararajan
    [J]. Metallurgical and Materials Transactions B, 2008, 39 : 619 - 628
  • [9] Modeling the Flow Curve of AISI 410 Martensitic Stainless Steel
    A. Momeni
    K. Dehghani
    M. Heidari
    M. Vaseghi
    [J]. Journal of Materials Engineering and Performance, 2012, 21 : 2238 - 2243
  • [10] Modeling of linear gas tungsten arc welding of stainless steel
    Maran, P.
    Sornakumar, T.
    Sundararajan, T.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2008, 39 (04): : 619 - 628