Semi-solid behavior of new Al-Si-Mg alloys for thixoforming

被引:77
|
作者
Paes, A [1 ]
Zoqui, EJ [1 ]
机构
[1] Univ Estadual Campinas, UNICAMP, Fac Mech Engn, BR-13083860 Campinas, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
semi-solid material; rheological behavior; aluminum-silicon-magnesium alloys; grain refining; morphological evolution;
D O I
10.1016/j.msea.2005.07.018
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
There is a lack of specific alloys for thixoforming processes. Usually alloys from conventional casting processes were fitted to the thixoforming purpose, e.g. A356, A357. The aim of this study is to produce new Al-Si-Mg alloys specially tailored for thixoforming purpose. The as-rheocast: Al-7 wt%Si-0.5 wt%Mg, Al-4 wt%Si-0.5 wt%Mg, Al-1 wt%Si-0.5 wt%Mg, Al-7 wt%Si-1 wt%Mg, Al-4 wt%Si-1 wt%Mg and Al-1 wt%Si-1 wt%Mg were produced by grain refining. Thus, the effect of Si and Mg content on structure and rheological behavior of these new alloys was analyzed. To simulate the semi-solid behavior at a high temperature, the samples were re-heated to the semi-solid state to produce 45% solid fraction and their structural evolution was analyzed after 0, 90 and 210 s at this solid fraction. At the same temperature and holding time, the samples were submitted to a compression test using a parallel platen viscosimeter. Results showed that the grain/globule size increased as the Si and Mg content increased. Al-7 wt%Si-0.5 wt%Mg, the Al-4 wt%Si-0.5 wt%Mg and the Al-1 wt%Si-0.5 wt%Mg are suitable for thixoforming purposes. Al-Si alloys with 1.0 wt%Mg showed low apparent viscosity values. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:63 / 73
页数:11
相关论文
共 50 条
  • [1] Development and Application of a New Al-Si-Mg Alloy for Semi-Solid Forming
    Pei, Xiao-hu
    Yang, Yi-tao
    [J]. NEW MATERIALS AND PROCESSES, PTS 1-3, 2012, 476-478 : 670 - 675
  • [2] Rheological Properties and Microstructure of Hypereutectic Semi-Solid Al-Si-Mg Alloys Using Rheocasting Route
    Tebib, Mehand
    Ajersch, Frank
    Chen, X-Grant
    [J]. SEMI-SOLID PROCESSING OF ALLOYS AND COMPOSITES XII, 2013, 192-193 : 323 - +
  • [3] Effects of Si Content and Forging Pressure on the Microstructural and Mechanical Characteristics in Semi-solid Forging of Al-Si-Mg Alloys
    Byung Keun Kang
    Il Sohn
    [J]. Metallurgical and Materials Transactions A, 2019, 50 : 3213 - 3222
  • [4] Effects of Si Content and Forging Pressure on the Microstructural and Mechanical Characteristics in Semi-solid Forging of Al-Si-Mg Alloys
    Kang, Byung Keun
    Sohn, Il
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2019, 50A (07): : 3213 - 3222
  • [5] Thixoforming and industrial application of the semi-solid alloy Al-6Si-2Mg
    Xie, Lijun
    Xu, Jun
    Yang, Bicheng
    Zhang, Zhifeng
    Shi, Likai
    [J]. SEMI- SOLID PROCESSING OF ALLOYS AND COMPOSITES, 2006, 116-117 : 72 - 75
  • [6] Semi-solid processing of Al and Mg alloys
    Shehata, MT
    Zoqui, EJ
    Kao, V
    Essadiqi, E
    [J]. Materials in the Automotive Industry, 2001, : 207 - 223
  • [7] Semi-solid characteristics and thixoforming of hypereutectic Al-Si alloy
    Liu, CM
    He, NJ
    Li, HJ
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2000, 10 (03) : 309 - 313
  • [8] Semi-solid characteristics and thixoforming of hypereutectic Al-Si alloy
    LIU Chang ming(刘昌明)
    [J]. Transactions of Nonferrous Metals Society of China, 2000, (03) : 309 - 313
  • [9] Semi-solid characteristics and thixoforming of hypereutectic Al-Si alloy
    [J]. Liu, C.-M., 2000, Allerton Press Inc. (10):
  • [10] Effect of pouring temperature on cooling slope casting of semi-solid Al-Si-Mg alloy
    Prosenjit Das
    Sudip K. Samanta
    Himadri Chattopadhyay
    Pradip Dutta
    [J]. Acta Metallurgica Sinica(English Letters), 2012, 25 (05) : 329 - 339