The corrosion of pure magnesium in aerated and deaerated sodium sulphate solutions

被引:493
|
作者
Baril, G [1 ]
Pébère, N [1 ]
机构
[1] ENSCT, Ctr Inter Univ Rech & Ingn Mat, Lab Interfaces & Mat, CNRS,UMR 5085, F-31077 Toulouse 4, France
关键词
magnesium; electrochemical impedance spectroscopy; polarization; oxygen reduction;
D O I
10.1016/S0010-938X(00)00095-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion behaviour of pure magnesium in aerated and deaerated Na2SO4 solutions (0.01 and 0.1 M) was investigated by steady-state current-voltage curves and electrochemical impedance measurements with a rotating disc electrode. It was shown that the anodic current densities were lower and the resistance values higher in deaerated media. It was demonstrated that the absence of HCO3- due to the absence of CO2, which is always present ill the natural environment was responsible for the results observed. The magnesium surface was covered with a porous film (MgO, Mg(OH)(2)) which became thicker with time. The protection afforded by the layer was low and the corrosion rate remained constant as the immersion time increased. In addition, experiments carried out at different NaHCO3 concentrations in deaerated media revealed that the corrosion rate of magnesium was accelerated when the NaHCO3 concentration increased due to dissolution of the film (MgO, Mg(OH)(2)). It was concluded that O-2 did not influence magnesium corrosion. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:471 / 484
页数:14
相关论文
共 50 条
  • [1] Investigation of the corrosion of pure magnesium in aerated sodium sulfate solutions
    Baril, G
    Pébère, N
    [J]. ENVIRONMENTAL DEGRADATION OF MATERIALS AND CORROSION CONTROL IN METALS, 1999, : 55 - 68
  • [2] Corrosion Inhibitor Film Forming in Aerated and Deaerated Solutions
    Musa, Ahmed Y.
    Kadhum, Abdul Amir H.
    Muhamad, Abu Baker
    [J]. INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2010, 5 (12): : 1911 - 1921
  • [3] CORROSION OF ZN IN DEAERATED SULPHATE SOLUTIONS AT DIFFERENT PH VALUES
    GMYTRYK, M
    SEDZIMIR, J
    [J]. CORROSION SCIENCE, 1967, 7 (10) : 683 - &
  • [4] A comparative Study on the Corrosion of Monel-400 in Aerated and Deaerated Arabian Gulf Water and 3.5% Sodium Chloride Solutions
    Sherif, El-Sayed M.
    Almajid, A. A.
    Bairamov, A. K.
    Al-Zahrani, Eissa
    [J]. INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2012, 7 (04): : 2796 - 2810
  • [5] Corrosion Behavior of Magnesium in Naturally Aerated Stagnant Seawater and 3.5% Sodium Chloride Solutions
    Sherif, El-Sayed M.
    [J]. INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2012, 7 (05): : 4235 - 4249
  • [6] An impedance investigation of the mechanism of pure magnesium corrosion in sodium sulfate solutions
    Baril, Genevieve
    Galicia, Gonzalo
    Deslouis, Claude
    Pebere, Nadine
    Tribollet, Bernard
    Vivier, Vincent
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2007, 154 (02) : C108 - C113
  • [7] The mechanism of Zn corrosion in both aerated and deaerated aqueous KNO3 solutions
    Roubani-Kalantzopoulou, F
    Patermarakis, G
    Karayianni, H
    [J]. ANTI-CORROSION METHODS AND MATERIALS, 1998, 45 (02) : 84 - +
  • [8] PHOTOREDUCTION OF ACRIDINE IN DEAERATED AND AERATED ETHANOL SOLUTIONS
    KATO, S
    MINAGAWA, S
    KOIZUMI, M
    [J]. BULLETIN OF THE CHEMICAL SOCIETY OF JAPAN, 1961, 34 (07) : 1026 - 1031
  • [9] Galvanic corrosion of nitinol under deaerated and aerated conditions
    Pound, Bruce G.
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2016, 104 (07) : 1322 - 1327
  • [10] Corrosion behavior of Tinplate in Aerated and Deaerated NaCl Solution
    Zhou, Dejing
    Wang, Jihui
    Han, Zhewen
    Liu, Xin
    Mao, Jing
    [J]. INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2017, 12 (01): : 639 - 651