Study on bending fretting fatigue damage in 17CrNiMo6 steel

被引:2
|
作者
Peng, J. F. [1 ,2 ]
Jin, X. [1 ]
Xu, Z. B. [1 ]
Cai, Z. B. [1 ]
Zhang, X. Y. [1 ]
Zhu, M. H. [1 ]
机构
[1] Southwest Jiaotong Univ, Tribol Res Inst, Tract Power State Key Lab, Chengdu 610031, Sichuan, Peoples R China
[2] Donghua Univ, State Key Lab Modificat Chem Fibers & Polymer Mat, Shanghai 200051, Peoples R China
来源
INTERNATIONAL JOURNAL OF MODERN PHYSICS B | 2017年 / 31卷 / 16-19期
基金
中国国家自然科学基金;
关键词
Bending fretting fatigue; 17CrNiMo6; steel; microcrack; damage mechanism; ALLOY;
D O I
10.1142/S0217979217440209
中图分类号
O59 [应用物理学];
学科分类号
摘要
Bending fretting fatigue behavior of 17CrNiMo6 alloy structural steel at room temperature was investigated under different bending and contact loads; and the S-N curve also was built up. The results showed that the S-N curve had a "C" shape. The bending fretting fatigue life was mainly dependent on the bending fatigue stress and fretting displacement. The limit of the specimens and the fretting fatigue life were dramatically decreased by fretting actions. The bending fretting fatigue damage changed under varied bending fatigue stress levels. When the wear first occurred, there is a lower bending fatigue stress; and with a higher bending fatigue load, microcracks were generated. However, some serious wear and surface delamination were observed under the highest fatigue load.
引用
收藏
页数:5
相关论文
共 50 条
  • [1] Bending Fretting Fatigue Characteristics of 18CrNiMo7-6 Alloy Steel
    Shen, Yan-Tuan
    Peng, Jin-Fang
    Xu, Zhi-Biao
    Liu, Jian-Hua
    Cai, Zhen-Bing
    Zhu, Min-Hao
    Cailiao Gongcheng/Journal of Materials Engineering, 2017, 45 (07): : 103 - 110
  • [2] COLD TOUGHNESS OF THE 17CRNIMO6 CASE HARDENING STEEL
    VONFIRCKS, J
    NEUE HUTTE, 1990, 35 (08): : 286 - 289
  • [3] Morphology and crystallographic analysis of lath martensite in 17CrNiMo6 steel
    Wang, Chun-Fang
    Wang, Mao-Qiu
    Shi, Jie
    Hui, Wei-Jun
    Dong, Han
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2007, 28 (02): : 64 - 68
  • [4] 17CrNiMo6渗碳淬火工艺
    张晓云
    温云龙
    金属加工(热加工), 2013, (07) : 40 - 40
  • [5] The Evolution of Microstructure for Carburizing and Quenching 17CrNiMo6 Steel: Forecasting and Experimentation
    Chu, Yuanzhao
    Gai, Dengyu
    Wang, Ruochen
    Zhuang, Zhu
    Zhang, Tao
    Wang, Shibin
    COATINGS, 2022, 12 (08)
  • [6] Fatigue and fretting fatigue of ion-nitrided 34CrNiMo6 steel
    Costa, JD
    Ferreira, JM
    Ramalho, AL
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2001, 35 (01) : 69 - 79
  • [7] 17CrNiMo6钢锭锻裂分析
    程书海
    赵益洛
    胡寒婷
    大型铸锻件, 2017, (06) : 44 - 46+62
  • [8] 17CrNiMo6钢渗碳淬火工艺优化
    朱科
    史仁贵
    王挺
    金属加工(热加工), 2022, (05) : 32 - 34
  • [9] 17CrNiMo6齿轮深层渗碳工艺研究
    张一坤
    王鹏宇
    刘伟
    机械工程与自动化, 2023, (04) : 123 - 125
  • [10] 17CrNiMo6钢齿轮断裂原因分析
    彭碧草
    沈丁杰
    唐远富
    龙毅
    黄桥生
    矿冶工程, 2013, 33 (06) : 101 - 102+106