Effects of Salt Composition and Wet/Dry Condition on Corrosion Behavior of Type 304 Stainless Steel Inside and Outside of Crevice

被引:0
|
作者
Kajikawa, Shunji [1 ]
Isobe, Yasuaki [1 ]
Okido, Masazumi [2 ]
机构
[1] Denso Corp, R&D Dept, Mat Engn, Kariya, Aichi 4488661, Japan
[2] Nagoya Univ, Grad Sch Engn, Dept Mat Sci & Engn, Nagoya, Aichi 4648603, Japan
关键词
type304 stainless steel; crevice corrosion; pitting corrosion; chloride; humidity; CHLORIDE; CRACKING;
D O I
10.2320/jinstmet.74.493
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
As the requirement for durability of automobile increase, the application of type 304 stainless steel is expanding because of its high workability and corrosion resistance. On the other hand, one of the main corrosion environments of automobile is chloride condition caused by deicing salt or sea salt particle, and it becomes more severe when added to the wet/dry cyclic condition that is specific to automobile. In this case, the corrosion resistance is not enough even if the stainless steel is applied. In the case of stainless steel, crevice corrosion is mainly concerned in chloride environment. Pitting corrosion, however, can sometimes occur at non-crevice site. The purpose of this study is to clarify how the corrosion factor such as salt composition or wet/dry condition affects to the corrosion behavior of type 304 stainless steel inside and outside of crevice. The corrosion factors described above were evaluated by the corrosion test method developed in our previous work. Furthermore, electrochemical measurements were conducted. As a result, when NaCl is used for chloride addition, there is more severe corrosion at crevice than non-crevice site regardless of wet/dry condition. However, when sea salt particle or CaCl2 that is a major component of deicing salt are used, corrosion sites differ depending on wet/dry condition. That is, corrosion is severe at crevice site under high humidity condition of more than 60%RH, while pitting corrosion is prominent at non-crevice site under low humidity of less than 40%RH. Considering the corrosion behavior under various wet/dry conditions, main corrosion factor of sea salt particle is not NaCl but MgCl2 that is not major component.
引用
收藏
页码:493 / 500
页数:8
相关论文
共 50 条
  • [1] Pitting corrosion of sensitised type 304 stainless steel under wet-dry cycling condition
    Cheng, Cong-Qian
    Klinkenberg, Laura-Isabell
    Ise, Yaoki
    Zhao, Jie
    Tada, Eiji
    Nishikata, Atsushi
    CORROSION SCIENCE, 2017, 118 : 217 - 226
  • [2] A STUDY OF CREVICE CORROSION IN TYPE-304 STAINLESS STEEL
    PETERSON, MH
    LENNOX, TJ
    GROOVER, RE
    MATERIALS PROTECTION AND PERFORMANCE, 1970, 9 (01): : 23 - &
  • [3] Effects of crevice geometry on corrosion behavior of 304 stainless steel during crevice corrosion in high temperature pure water
    Chen, Dongxu
    Han, En-Hou
    Wu, Xinqiang
    CORROSION SCIENCE, 2016, 111 : 518 - 530
  • [4] Crevice Corrosion and Cracking Behavior of Cold Rolled Type 304 Stainless Steel in Chloride Environment
    Kajikawa, Shunji
    Isobe, Yasuaki
    Okido, Masazumi
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2009, 73 (05) : 362 - 367
  • [5] A STATISTICAL EVALUATION OF CREVICE CORROSION ON TYPE-304 STAINLESS-STEEL
    FUJIMOTO, S
    SHIBATA, T
    MINAMIDA, M
    UDAKA, S
    CORROSION SCIENCE, 1994, 36 (09) : 1575 - 1583
  • [6] INFLUENCE OF PH ON THE CREVICE CORROSION AND STRESS-CORROSION CRACKING BEHAVIOR OF 304 STAINLESS-STEEL
    PRUITT, NC
    SUDARSHAN, TS
    LOUTHAN, MR
    JOURNAL OF MATERIALS ENGINEERING, 1988, 10 (02) : 99 - 108
  • [7] Corrosion behavior of type 304 stainless steel produced by MIM process under SSRT condition
    Sunada, Satoshi
    Yamamoto, Takahisa
    Tanaka, Shigeo
    Kada, Norio
    Majima, Kazuhiko
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2007, 54 (05): : 336 - 344
  • [8] Influence of application of ultrasonic wave on corrosion behavior of SUS304 stainless steel with crevice
    Wang, Rongguang
    Kido, Mitsuo
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2007, 71 (06) : 511 - 516
  • [9] Modelling stochastic response of type 304 stainless steel (SS-304) crevice corrosion in chloride environments
    Adeniyi, A. G.
    Ogunleye, O. O.
    Durowoju, M. O.
    Odeyemi, S. O.
    INDIAN CHEMICAL ENGINEER, 2019, 61 (03) : 286 - 295
  • [10] FACTORIAL DESIGN BASED OPTIMISATION OF CREVICE CORROSION FOR TYPE 304 STAINLESS STEEL IN CHLORIDE SOLUTIONS
    Ogunleye, O. O.
    Adeniyi, A. G.
    Durowoju, M. O.
    ADVANCES IN MATERIALS SCIENCE, 2016, 16 (02): : 5 - 20