Low-damage damascene patterning using porous inorganic low-dielectric-constant materials

被引:39
|
作者
Yonekura, K [1 ]
Goto, K [1 ]
Matsuura, M [1 ]
Fujiwara, N [1 ]
Tsujimoto, K [1 ]
机构
[1] Renesas Technol Corp, Wafer Proc Engn Dev Div, Itami, Hyogo 6640005, Japan
关键词
porous low-k material; dielectric constant; damascene; plasma damage; plasma etching; ashing;
D O I
10.1143/JJAP.44.2976
中图分类号
O59 [应用物理学];
学科分类号
摘要
The degradation of porous low-dielectric-constant (low-k) materials, such as porous methyl silsesquioxane (MSQ) and porous chemical-vapor-deposited SiOCH films, by damascene etch and ash processes has been investigated. The influence of etch damage becomes relatively stronger as ash damage improves. The etch damage to porous low-k dielectric is found particularly at the sidewall of the isolated lines. By investigating the influence of etch conditions on the damage, it is found that O(2) and Ar addition causes large sidewall damage. O(2)-added etch condition, as well as the O(2) ash process, produces oxygen radicals, which extract CH(3) groups from porous low-k films. On the other hand, Ar plasma does not efficiently extract CH(3) groups differently from O(2) plasma, but it changes the bonding states of CH(3) groups and causes H(2)O adsorption. This change in film characteristics increases dielectric constant. Finally, we successfully achieved low-damage dual damascene patterning using a porous SiOCH material whose dielectric constant is 2.2.
引用
收藏
页码:2976 / 2981
页数:6
相关论文
共 50 条
  • [1] Low-damage damascene patterning of SiOC(H) low-k dielectrics
    Struyf, H
    Hendrickx, D
    Van Olmen, J
    Iacopi, F
    Richard, O
    Travaly, Y
    Van Hove, M
    Boullart, W
    Vanhaelemeersch, S
    PROCEEDINGS OF THE IEEE 2005 INTERNATIONAL INTERCONNECT TECHNOLOGY CONFERENCE, 2005, : 30 - 32
  • [2] Properties and thermal stability of porous organic low-dielectric-constant materials
    Chang, SY
    Jang, SM
    Lin, SH
    Liang, MS
    THIN SOLID FILMS, 2004, 466 (1-2) : 54 - 61
  • [3] Characterization of organic low-dielectric-constant materials using optical spectroscopy
    Postava, K
    Yamaguchi, T
    Nakano, T
    OPTICS EXPRESS, 2001, 9 (03): : 141 - 151
  • [4] Low-Dielectric-Constant Materials for ULSI Interlayer-Dielectric Applications
    Wei William Lee
    Paul S. Ho
    MRS Bulletin, 1997, 22 : 19 - 27
  • [5] Low-dielectric-constant materials for ULSI interlayer-dielectric applications
    Lee, WW
    Ho, PS
    MRS BULLETIN, 1997, 22 (10) : 19 - 24
  • [6] Organic and inorganic spin-on polymers for low-dielectric-constant applications
    Hacker, NP
    MRS BULLETIN, 1997, 22 (10) : 33 - 38
  • [7] Cu-Induced Dielectric Breakdown of Porous Low-Dielectric-Constant Film
    Cheng, Yi-Lung
    Lee, Chih-Yen
    Huang, Yao-Liang
    Sun, Chung-Ren
    Lee, Wen-Hsi
    Chen, Giin-Shan
    Fang, Jau-Shiung
    Phan, Bach Thang
    JOURNAL OF ELECTRONIC MATERIALS, 2017, 46 (06) : 3627 - 3633
  • [8] Modeling to Predict Effective Dielectric Constant of Porous Silicon Low-Dielectric-constant Thin Films
    Rahmoun, K.
    Fakiri, S.
    SPECTROSCOPY LETTERS, 2014, 47 (05) : 348 - 355
  • [9] Direct patterning of photosensitive low-dielectric-constant films using electron-beam lithography
    Kikkawa, T
    Nagahara, T
    Matsuo, H
    APPLIED PHYSICS LETTERS, 2001, 78 (17) : 2557 - 2559
  • [10] Organic and Inorganic Spin-On Polymers for Low-Dielectric-Constant Applications
    Nigel P. Hacker
    MRS Bulletin, 1997, 22 : 33 - 38