On the degradation kinetics of thin oxide layers

被引:1
|
作者
Scarpa, A
Pananakakis, G
Ghibaudo, G
Paccagnella, A
Ghidini, G
机构
[1] Univ Padua, DEI, I-35131 Padua, Italy
[2] ENSERG, Lab Phys Composants Semicond, CNRS, UMR 5531, F-38016 Grenoble, France
[3] SGS Thomson Microelect, I-20041 Agrate Brianza, Italy
关键词
D O I
10.1016/S0038-1101(98)00260-3
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
After Fowler-Nordheim stress, since SiO2 charge trapping occurs up to final dielectric breakdown, oxide layers degrade. The degradation features of very thin gate oxide films have been studied, after constant current stress. Furthermore charge build up in the oxide bulk and in the anodic/cathodic oxide regions has been investigated. For oxides thicker than 5 nm it was possible to provide a physical interpretation of the experimental results, showing a power law of charge trapping kinetics as a function of stress level. For thinner oxides, it has been shown that the degradation mechanisms can be very different and the proposed interpretation is no longer valid. (C) 1998 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:221 / 227
页数:7
相关论文
共 50 条
  • [1] GROWTH KINETICS OF THIN OXIDE LAYERS ON LEAD
    BAKER, JM
    FROMHOLD, AT
    BULLETIN OF THE AMERICAN PHYSICAL SOCIETY, 1976, 21 (03): : 321 - 321
  • [2] Degradation and breakdown in thin oxide layers: mechanisms, models and reliability prediction
    Degraeve, R
    Kaczer, B
    Groeseneken, G
    MICROELECTRONICS RELIABILITY, 1999, 39 (10) : 1445 - 1460
  • [3] Kinetics of electrochemical lithium intercalation into thin tungsten (VI) oxide layers
    A. V. Churikov
    A. V. Ivanishchev
    I. A. Ivanishcheva
    K. V. Zapsis
    I. M. Gamayunova
    V. O. Sycheva
    Russian Journal of Electrochemistry, 2008, 44 : 530 - 542
  • [4] Kinetics of electrochemical lithium intercalation into thin tungsten (VI) oxide layers
    Churikov, A. V.
    Ivanishchev, A. V.
    Ivanishcheva, I. A.
    Zapsis, K. V.
    Gamayunova, I. M.
    Sycheva, V. O.
    RUSSIAN JOURNAL OF ELECTROCHEMISTRY, 2008, 44 (05) : 530 - 542
  • [5] The kinetics of high temperature degradation of thin chromium protective layers on valve steels
    Drozdz, Monika
    Pawlak, Wojciech
    Grzesik, Zbigniew
    OCHRONA PRZED KOROZJA, 2015, 58 (07): : 254 - 257
  • [6] The kinetics of high temperature degradation of thin chromium protective layers on valve steels
    Drozdz, Monika
    Pawlak, Wojciech
    Grzesik, Zbigniew
    OCHRONA PRZED KOROZJA, 2015, 58 (05):
  • [7] Electric stress-induced degradation of thin oxide layers and its impact on device reliability
    Degraeve, R
    Kaczer, B
    Roussel, P
    Groeseneken, G
    SEMICONDUCTOR SILICON 2002, VOLS 1 AND 2, 2002, 2002 (02): : 475 - 488
  • [8] Photocatalytic degradation of methyl green by doped zinc oxide thin layers under solar irradiation
    Azizi, Soulef
    Sellam, Manel
    Mesri, Nadia
    Sehili, Tahar
    Gherraf, Noureddine
    JOURNAL OF PHOTOCHEMISTRY AND PHOTOBIOLOGY A-CHEMISTRY, 2024, 453
  • [9] MOS DIODES WITH THIN OXIDE LAYERS
    IMABUN, Y
    YOSHIDA, K
    OKUDA, M
    ELECTRICAL ENGINEERING IN JAPAN, 1972, 91 (03) : 159 - &
  • [10] THE PREPARATION OF THIN LAYERS OF URANIUM OXIDE
    COOK, GB
    HUDSWELL, F
    JOURNAL OF SCIENTIFIC INSTRUMENTS, 1950, 27 (08): : 230 - 231