On the response of thin-walled CFRP composite tubular components subjected to static and dynamic axial compressive loading: experimental

被引:192
|
作者
Mamalis, AG [1 ]
Manolakos, DE [1 ]
Ioannidis, MB [1 ]
Papapostolou, DP [1 ]
机构
[1] Natl Tech Univ Athens, Mfg Technol Div, Athens 15780, Greece
关键词
crashworthiness; composite tubes; square cross-section; CFRP; carbon fabric; axial compression; impact;
D O I
10.1016/j.compstruct.2004.07.021
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
In this work the crushing response and crashworthiness characteristics of thin-wall square FRP (fibre reinforced plastic) tubes that were impact tested at high compressive strain rate are compared to the response of the same tubes in static axial compressive loading. The material combination of the tested specimens was carbon fibres in the form of reinforcing woven fabric in epoxy resin, and the tested tubes were constructed trying three different laminate stacking sequences and fibre volume contents on approximately the same square cross-section. Comparison of the static and dynamic crushing characteristics is made by examining the collapse modes, the shape of the load-displacement curves, the peak and average compressive load and the absorbed amount of crushing energy in both loading cases. In addition, the influence of the tube geometry (axial length, aspect ratio and wall thickness), the laminate material properties-such as the fibre volume content and stacking sequence-and the compressive strain rate on the compressive response, the collapse modes, the size of the peak load and the energy absorbing capability of the thin-wall tubes is extensively analysed. (c) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:407 / 420
页数:14
相关论文
共 50 条