Effect of sintering time on structural, morphological and electrical properties of Sb-doped Bi1.6Pb0.4Sr2Ca2Cu3Oy superconductor

被引:7
|
作者
Romero-Sanchez, M. [1 ]
Sanchez-Mera, T. [1 ]
Santos-Cruz, J. [1 ]
Perez-Garcia, C. E. [1 ]
de la L Olvera, M. [2 ]
Santillan-Rodriguez, C. R. [3 ]
Matutes-Aquino, J. [3 ]
Contreras-Puente, G. [4 ]
de Moure-Flores, F. [1 ]
机构
[1] Univ Autonoma Queretaro, Fac Quim, Mat Energia, Queretaro 76010, Mexico
[2] IPN, CINVESTAV, Dept Ingn Elect, Apdo Postal 14-740, Mexico Cdmx 07360, Mexico
[3] Ctr Invest Mat Avanzados SC, Miguel Cervantes 120, Complejo Ind Chihuahua, Mexico
[4] Inst Politecn Nacl, Escuela Super Fis & Matemat, Cdmx 07738, Mexico
关键词
Solid-state reaction; Sintering time; BSCCO superconductor; ENHANCEMENT; PERFORMANCE;
D O I
10.1016/j.ceramint.2022.02.149
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Bi(1.6)Pb(0.4)Sb(0.0)6Sr(2)Ca(2)Cu(3)O(y) superconductors were processed by the solid-state reaction at 860 degrees C, varying the sintering time from 100 to 160 h. The structural characterization was carried out by X-ray diffraction and Raman spectroscopy, which showed that Bi(1.6)Pb(0.4)Sb(0.0)6Sr(2)Ca(2)Cu(3)O(y) samples have a mixture of interest B-2212 and Bi2223 phases. The sintering time strongly influences structural, morphological and electrical properties; the sample sintered by 130 h presents a volume fraction of 62% for the Bi-2223 phase, large grains (between 5 and 20 mu m) and a critical temperature of 107 K.