A strong static magnetic field (SSMF) of about 10 T was introduced to the aging process of AZ91 magnesium alloy. Comparing with conventional aging, in the first stage of aging with SSMF, discontinuous precipitation of Mg17Al12 at grain boundary was accelerated. The magnetically induced grain boundary migration might be responsible for this acceleration effect. The density of the Mg17Al12 continuous precipitates inside the grains was increased and the precipitation plates became thinner in SSMF pre-aged specimens, which might be ascribed to the retarded volume diffusion resulted from the SSMF.
引用
收藏
页码:849 / 852
页数:4
相关论文
共 50 条
  • [1] Effect of grain boundary misorientation on discontinuous precipitation in an AZ91 alloy
    H. Azzeddine
    S. Abdessameud
    B. Alili
    Z. Boumerzoug
    D. Bradai
    [J]. Bulletin of Materials Science, 2011, 34 : 1471 - 1476
  • [2] Effect of grain boundary misorientation on discontinuous precipitation in an AZ91 alloy
    Azzeddine, H.
    Abdessameud, S.
    Alili, B.
    Boumerzoug, Z.
    Bradai, D.
    [J]. BULLETIN OF MATERIALS SCIENCE, 2011, 34 (07) : 1471 - 1476
  • [3] Precipitation Simulation of AZ91 Alloy
    Zhang, C.
    Cao, W.
    Chen, S. -L.
    Zhu, J.
    Zhang, F.
    Luo, A. A.
    Schmid-Fetzer, R.
    [J]. JOM, 2014, 66 (03) : 389 - 396
  • [4] Precipitation Simulation of AZ91 Alloy
    C. Zhang
    W. Cao
    S.-L. Chen
    J. Zhu
    F. Zhang
    A. A. Luo
    R. Schmid-Fetzer
    [J]. JOM, 2014, 66 : 389 - 396
  • [5] Suppression of discontinuous precipitation in AZ91 by addition of Sn
    I. C. Jung
    Y. K. Kim
    T. H. Cho
    S. H. Oh
    T. E. Kim
    S. W. Shon
    W. T. Kim
    D. H. Kim
    [J]. Metals and Materials International, 2014, 20 : 99 - 103
  • [6] Effect of precipitation on internal friction of AZ91 magnesium alloy
    刘树伟
    姜海昌
    李秀艳
    戎利建
    [J]. Transactions of Nonferrous Metals Society of China, 2010, 20 (S2) : 453 - 457
  • [7] Suppression of discontinuous precipitation in AZ91 by addition of Sn
    Jung, I. C.
    Kim, Y. K.
    Cho, T. H.
    Oh, S. H.
    Kim, T. E.
    Shon, S. W.
    Kim, W. T.
    Kim, D. H.
    [J]. METALS AND MATERIALS INTERNATIONAL, 2014, 20 (01) : 99 - 103
  • [8] Effect of precipitation on internal friction of AZ91 magnesium alloy
    Liu Shu-wei
    Jiang Hai-chang
    Li Xiu-yan
    Rong Li-jian
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 : S453 - S457
  • [9] Effect of Pb Addition on the Discontinuous and Continuous Mg17Al12-β Precipitate During Solidification of AZ91 Magnesium Alloy
    Arun Boby
    U. T. S. Pillai
    B. C. Pai
    [J]. Transactions of the Indian Institute of Metals, 2013, 66 : 105 - 108
  • [10] Effect of Pb Addition on the Discontinuous and Continuous Mg17Al12-β Precipitate During Solidification of AZ91 Magnesium Alloy
    Boby, Arun
    Pillai, U. T. S.
    Pai, B. C.
    [J]. TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2013, 66 (02) : 105 - 108