Effect of Operating Conditions on the Coke Formation and Nickel Catalyst Performance During Cracking of Tar

被引:24
|
作者
Lu, Peng [1 ]
Huang, Qunxing [1 ]
Bourtsalas, Athanasios C. [2 ]
Chi, Yong [1 ]
Yan, Jianhua [1 ]
机构
[1] Zhejiang Univ, State Key Lab Clean Energy Utilizat, Hangzhou 310027, Zhejiang, Peoples R China
[2] Columbia Univ, Earth Engn Ctr, New York, NY 10027 USA
关键词
Tar; Ni catalyst; Operating conditions; Coke; Activity; CARBON NANOTUBES; MODEL-COMPOUND; BIOMASS TAR; STEAM; GASIFICATION; HYDROGEN; PYROLYSIS; TOLUENE; WASTE; NI;
D O I
10.1007/s12649-017-0044-5
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Catalytic cracking of toluene as a tar model compound was carried out to investigate the effect of operating conditions on the coke formation and performance of nickel catalyst. The deactivation of catalyst depended on the quantity and nature of deposited coke, which were affected by the operating conditions, including temperature, nickel and steam concentration. The highest yield ratio of filamentous coke to the amorphous coke was 1.11 with the Ni/Al2O3 catalyst containing the highest amount of Ni examined, 20%, and heated at 700 degrees C without steam injection. The formation of filamentous coke maintained the catalyst activity at the first 20 min, which had less serious effect on the deactivation than the amorphous coke. Two types of coke deactivation trends were observed. Type I was associated with the deactivation by amorphous coke and type II was due to the corporate effects of amorphous and filamentous coke, which extended the life time of the catalyst.
引用
收藏
页码:155 / 165
页数:11
相关论文
共 50 条
  • [1] Effect of Operating Conditions on the Coke Formation and Nickel Catalyst Performance During Cracking of Tar
    Peng Lu
    Qunxing Huang
    Athanasios C. Bourtsalas
    Yong Chi
    Jianhua Yan
    Waste and Biomass Valorization, 2019, 10 : 155 - 165
  • [2] COKE FORMATION DURING CRACKING OF HYDROCARBONS .1. THE EFFECT OF PRE-SULPHIDING ON COKE FORMATION ON A NICKEL-CHROMIUM-IRON ALLOY UNDER STEAM CRACKING CONDITIONS
    TRIMM, DL
    HOLMEN, A
    LINDVAG, O
    JOURNAL OF CHEMICAL TECHNOLOGY AND BIOTECHNOLOGY, 1981, 31 (06) : 311 - 316
  • [3] Effect of Additives on the Performance of Monolithic Catalyst for Tar Cracking
    Lu, Min
    Xiong, Zuhong
    Lu, Pengmei
    Yuan, Zhenhong
    Fan, Genyu
    Chen, Yong
    ENERGY & FUELS, 2013, 27 (05) : 2599 - 2607
  • [4] COKE FORMATION DURING CRACKING OF HYDROCARBONS - 1. THE EFFECT OF PRE-SULPHIDING ON COKE FORMATION ON A NICKEL-CHROMIUM-IRON ALLOY UNDER STEAM CRACKING CONDITIONS.
    Trimm, David L.
    Holmen, Anders
    Lindvag, Odd
    Journal of chemical technology and biotechnology, 1981, 31 (06): : 311 - 316
  • [5] Pathways of coke formation on an MFI catalyst during the cracking of waste polyolefins
    Castano, Pedro
    Elordi, Gorka
    Ibanez, Maria
    Olazar, Martin
    Bilbao, Javier
    CATALYSIS SCIENCE & TECHNOLOGY, 2012, 2 (03) : 504 - 508
  • [6] RADIOTRACER STUDY OF COKE FORMATION ON CRACKING CATALYST
    MCMAHON, RE
    INDUSTRIAL AND ENGINEERING CHEMISTRY, 1955, 47 (04): : 844 - 845
  • [7] Experimental studies on coke catalyst for cracking of biomass tar model compound
    Mi, Tie
    Tang, Ninglu
    Wu, Zhengshun
    Liu, Xiaoyan
    Sun, Tingting
    Taiyangneng Xuebao/Acta Energiae Solaris Sinica, 2013, 34 (01): : 82 - 85
  • [8] Effect of Phosphine on Coke Formation during Steam Cracking of Propane
    Patil, Manjunath
    Djokic, Marko
    Verbeken, Kim
    Reyniers, Marie-Francoise
    Van Geem, Kevin M.
    MATERIALS, 2021, 14 (17)
  • [9] Study on solid waste pyrolysis coke catalyst for catalytic cracking of coal tar
    Lei, Zhang
    Hao, Shu
    Yang, Jia
    Lei, Zhang
    Dan, Xu
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2020, 45 (38) : 19280 - 19290
  • [10] EFFECT OF RESIDUAL COKE ON BEHAVIOR OF CRACKING CATALYST
    WHITAKER, AC
    KINZER, AD
    INDUSTRIAL AND ENGINEERING CHEMISTRY, 1955, 47 (10): : 2153 - 2157