Failure analysis on premature fracture of anchor bolts in seawater booster pump of nuclear power plant

被引:22
|
作者
Gong, Yi [1 ]
Ding, Qun [1 ]
Yang, Zhen-Guo [1 ]
机构
[1] Fudan Univ, Dept Mat Sci, Shanghai 200433, Peoples R China
关键词
Nuclear power plant; Anchor bolt; Fracture analysis; Seawater booster pump; Stress corrosion cracking; STRESS-CORROSION CRACKING; TRANSFER TITANIUM TUBES; PITTING CORROSION; HEAT-EXCHANGERS; STEEL; CONDENSERS; LEAKAGE;
D O I
10.1016/j.engfailanal.2018.12.008
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Three of the four TP321 stainless steel anchor bolts used in an indoor seawater booster pump of a nuclear power plant were encountered with premature fracture during service. A comprehensive analysis was performed to investigate the operational conditions, base materials and macro/ micro morphologies of the failed bolts to identify the failure causes. The results showed that a collection of banded inclusions was distributed among the grains by metallographic examination, and typical pitting holes were observed and high levels of chlorides were detected on the surfaces of the failed bolts' fractures by scanning electron microscope (SEM) and energy dispersive spectrometer (EDS). In addition, branched cracks were found on the axial sections of the fractured bolts. Given all that, the premature fracture of the anchor bolts was determined to be mainly caused by stress corrosion cracking (SCC) from chlorides, which was then proved to be induced by splashing of the seawater during routine maintenance of the pump. Besides, the sequence of fracture for these three anchor bolts was ascertained by fractography from three aspects, including shapes of fractures, morphologies of corrosion products and chemical compositions of corrosion products. Finally, countermeasures were put forward as well.
引用
收藏
页码:10 / 19
页数:10
相关论文
共 50 条
  • [1] Failure analysis on premature fracture of boric acid recycle pump shaft in 1000 MW nuclear power plant
    Ni, Tong-Wei
    Ding, Qun
    Yang, Zhen-Guo
    Zheng, Hong-Lian
    Lou, Xiao
    ENGINEERING FAILURE ANALYSIS, 2018, 92 : 317 - 326
  • [2] Cause Analysis of Booster Pump Shaft Cracking in Nuclear Power Plant
    Li, Guodong
    Wang, Tao
    Li, Nan
    Lu, Shaohua
    4TH ANNUAL INTERNATIONAL WORKSHOP ON MATERIALS SCIENCE AND ENGINEERING (IWMSE2018), 2018, 381
  • [3] Fracture Analysis and Fatigue Strength Calculation of Anchor Bolt Used in Circulating Water Pump in Nuclear Power Plant
    Chen, Qiang
    Zu, Shuai
    Che, Yinhui
    Feng, Dongxiong
    Li, Yang
    SCANNING, 2021, 2021
  • [4] MODE ANALYSIS OF COOLANT PUMP IN NUCLEAR POWER PLANT
    Ren, Zhaohui
    Ma, Hui
    Wang, Xuejun
    Wen, Feng
    Wen, Bang Chun
    ICONE 16: PROCEEDING OF THE 16TH INTERNATIONAL CONFERENCE ON NUCLEAR ENGINEERING - 2008, VOL 4, 2008, : 733 - 737
  • [5] Fracture Analysis and Working Stress Calculation of Bearing Cage Used in Charging Pump in a Nuclear Power Plant
    Chen, Qiang
    Jiang, Shengli
    Duan, Deli
    METALS, 2023, 13 (08)
  • [6] Premature Failure Analysis of Servovalve Components for a Thermal Power Plant
    Chang, Sung-Yong
    Chang, Joong-Chel
    Kim, Bum-Soo
    Seo, Min-Woo
    Choi, Chel-Jong
    KOREAN JOURNAL OF METALS AND MATERIALS, 2011, 49 (09): : 708 - 714
  • [7] Hydrogeochemical modelling of corrosive environment contributing to premature failure of anchor bolts in underground coal mines
    Peng, Ya
    Timms, Wendy
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2020, 27 (05) : 1599 - 1610
  • [8] Premature failure of MEA pump impellers in a desalination plant
    Malik, AU
    Prakash, TL
    Ahmad, S
    MATERIALS PERFORMANCE, 2001, 40 (10) : 56 - 59
  • [9] Analysis on Wearing of Bearing for Main Pump in Nuclear Power Plant
    Zhang H.
    Huang Z.
    Jiao S.
    Dai H.
    Xu X.
    Sheng F.
    Hedongli Gongcheng/Nuclear Power Engineering, 2022, 43 (02): : 108 - 111
  • [10] Finite element analysis of failure response behavior of anchor bolts in concrete
    Etse, G
    NUCLEAR ENGINEERING AND DESIGN, 1998, 179 (02) : 245 - 252