Polycarbosilane-derived SIC fibers (Nicalon) were oxidized at 1773 K under oxygen partial pressures from 10(2) to 10(5) Pa. The effect of oxygen partial pressure on the oxidation behavior of the Nicalon fibers was investigated by examining mass change, surface composition, crystal phase, morphology, and tensile strength. The Nicalon fibers were passively oxidized under oxygen partial pressures of >2.5 x 10(2) Pa and actively oxidized under an oxygen partial pressure of 10(2) Pa. Under oxygen partial pressures front 2.5 x 10(2) to 10(3) Pa, active oxidation occurred at the earliest stage of oxidation, resulting in the formation of both a silica film and a carbon intermediate layer, Although the unoxidized core retained considerable levels of strength under the passive-oxidation condition, fiber strength was last under the active-oxidation condition.
引用
收藏
页码:3049 / 3056
页数:8
相关论文
共 24 条
  • [1] Oxidation behavior of Si-C-O fibers (Nicalon) in alumina
    Shimoo, T
    Okamura, K
    Yamanaka, T
    JOURNAL OF MATERIALS SCIENCE, 2001, 36 (17) : 4137 - 4143
  • [2] Oxidation behavior of Si-C-O fibers (Nicalon) in alumina
    T. Shimoo
    K. Okamura
    T. Yamanaka
    Journal of Materials Science, 2001, 36 : 4137 - 4143
  • [3] Oxidation behavior and thermal stability of Si-C-O fibers (Nicalon) in carbon dioxide
    Shimoo, T
    Morita, T
    Okamura, K
    JOURNAL OF MATERIALS SCIENCE, 2002, 37 (15) : 3181 - 3188
  • [4] Oxidation behavior and thermal stability of Si-C-O fibers (Nicalon) in carbon dioxide
    T. Shimoo
    T. Morita
    K. Okamura
    Journal of Materials Science, 2002, 37 : 3181 - 3188
  • [5] Pyrolysis of Si-C-O fibers (Nicalon) at temperatures from 1473 K to 1673 K
    Shimoo, Toshio
    Chen, Hemin
    Okamura, Kiyohito
    Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan, 1992, 100 (1157): : 48 - 53
  • [6] Oxidation behavior of Si-M-C-O fibers under wide range of oxygen partial pressures
    T. Shimoo
    Y. Morisada
    K. Okamura
    Journal of Materials Science, 2002, 37 : 4361 - 4368
  • [7] Oxidation behavior of Si-M-C-O fibers under wide range of oxygen partial pressures
    Shimoo, T
    Morisada, Y
    Okamura, K
    JOURNAL OF MATERIALS SCIENCE, 2002, 37 (20) : 4361 - 4368
  • [8] EFFECTS OF MICROSTRUCTURAL INSTABILITY ON THE CREEP-BEHAVIOR OF SI-C-O (NICALON) FIBERS IN ARGON
    JIA, NY
    BODET, R
    TRESSLER, RE
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (12) : 3051 - 3060
  • [9] Microstructural stability and creep behavior of Si-C-O (Nicalon) fibers in carbon monoxide and argon environments
    Bodet, R
    Lamon, J
    Jia, NY
    Tressler, RE
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (10) : 2673 - 2686
  • [10] Effect of oxygen partial pressure on oxidation rate of Si-C-O fiber
    Shimoo, T
    Toyoda, F
    Okamura, K
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1998, 106 (05) : 447 - 451