Removal of Trace Amounts of Copper from Concentrated Hydrochloric Acid Solutions

被引:2
|
作者
Erdogan, Metehan [1 ]
Karakaya, Esra [2 ,3 ]
Aras, Mustafa Serdal [3 ]
Karagul, Sedef Cift [4 ]
Ersoy, Merve Kolay [4 ]
Ozturk, Abdullah [2 ]
Karakaya, Ishak [2 ]
机构
[1] Ankara Yildirim Beyazit Univ, Dept Met & Mat Engn, 150 Sok & Takdir Cad 5, TR-06010 Ankara, Turkey
[2] Middle East Tech Univ, Dept Met & Mat Engn, Dumlupinar Bulvari 1, TR-06800 Ankara, Turkey
[3] MEGAP Co, ODTU Teknokent Gumus Blok A 15-A, TR-06800 Ankara, Turkey
[4] Borusan Technol Dept & R&D Co, Buyukhanli Plaza Defne Sok 3, TR-34758 Istanbul, Turkey
来源
关键词
Copper electrodeposition; Copper recovery; Pickling solution; Current density; SOLVENT-EXTRACTION; PICKLING SOLUTIONS; EXCHANGE MEMBRANE; SULFATE-SOLUTIONS; RECOVERY; WATER; IONS; PRECIPITATION; INHIBITION; REACTOR;
D O I
10.20964/2018.11.75
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Pickling process is recognized as one of the strongest acid consuming processes in the steel industry. A pickling solution that contains hydrochloric acid (HCl) is used for the metal surface treatment of steel plants. The same acid can be used for a long period of time by means of a regeneration process, in which iron concentration of the acid is decreased to insignificant concentrations. However, regenerated pickling solutions contain copper, especially when scrap is used to produce steel. Furthermore, copper deposits on the metal in the following pickling processes when its concentration exceeds a certain critical value. This study describes an electrochemical treatment process for collecting copper from regenerated pickling solutions of steel plants. Copper concentration, electrolysis time, and current density were selected as the operation variables and pH and conductivity of the acid together with the amount and morphology of the deposition were considered as the response variables for optimization. Graphite was used as the anode due to its high conductivity and stability and copper or stainless steel was used as the cathode in this study. The results showed that electrochemical treatment process decreased copper concentration to about 80 from 127 ppm using stainless steel cathode under the optimum constant current density of 2.0 A/dm(2) and electrolysis time of 4 hours, without any acid loss, which was verified by pH, conductivity and acidity measurements.
引用
收藏
页码:10934 / 10947
页数:14
相关论文
共 50 条
  • [1] Solvent extraction of trace amounts of gold from hydrochloric acid solutions with phosphoryl-containing podands
    Turanov, AN
    Karandashev, VK
    Baulin, VE
    Tsvetkov, EN
    [J]. ZHURNAL NEORGANICHESKOI KHIMII, 1995, 40 (11): : 1926 - 1930
  • [2] Thermodynamics of concentrated aqueous solutions of hydrochloric acid
    Akerlof, G
    Teare, JW
    [J]. JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1937, 59 : 1855 - 1868
  • [3] Structure and Dynamics of Concentrated Hydrochloric Acid Solutions
    Xu, Jianqing
    Izvekov, Sergei
    Voth, Gregory A.
    [J]. JOURNAL OF PHYSICAL CHEMISTRY B, 2010, 114 (29): : 9555 - 9562
  • [4] THE HYDROLYSIS OF PICOLINAMIDE AND ISONICOTINAMIDE IN CONCENTRATED HYDROCHLORIC ACID SOLUTIONS
    JELLINEK, HHG
    URWIN, JR
    [J]. JOURNAL OF PHYSICAL CHEMISTRY, 1954, 57 (09): : 900 - 902
  • [5] Diffraction studies on concentrated aqueous hydrochloric acid solutions
    Kameda, Y
    Usuki, T
    Uemura, O
    [J]. ISRAEL JOURNAL OF CHEMISTRY, 1999, 39 (3-4) : 283 - 289
  • [6] Recovery of Copper from Concentrated Seruwila Copper Magnetite Ore from Chloride Electrolyte in the Presence of Hydrochloric Acid
    Dissanayake, Kithsiri
    [J]. MERCON 2020: 6TH INTERNATIONAL MULTIDISCIPLINARY MORATUWA ENGINEERING RESEARCH CONFERENCE (MERCON), 2020, : 516 - 520
  • [7] HYDROFLUORIC AND HYDROCHLORIC-ACID BEHAVIOR IN CONCENTRATED SALINE SOLUTIONS
    CLEGG, SL
    BRIMBLECOMBE, P
    [J]. JOURNAL OF THE CHEMICAL SOCIETY-DALTON TRANSACTIONS, 1988, (03): : 705 - 710
  • [8] The activity coefficient of hydrochloric acid in concentrated solutions of strong electrolytes
    Harned, HS
    [J]. JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1926, 48 (01) : 326 - 342
  • [9] ELECTRODE PROCESSES AT BISMUTH IN CONCENTRATED HYDROCHLORIC-ACID SOLUTIONS
    VASILEVA, LS
    KRASIKOV, BS
    [J]. JOURNAL OF APPLIED CHEMISTRY OF THE USSR, 1979, 52 (10): : 2136 - 2140
  • [10] MEASUREMENT OF ACTIVITIES OF ELECTROLYTES IN CONCENTRATED HYDROCHLORIC-ACID SOLUTIONS
    MAJIMA, H
    AWAKURA, Y
    SATO, T
    [J]. DENKI KAGAKU, 1980, 48 (11): : 597 - 602