Effect of sintering parameters on physical and mechanical properties of powder injection moulded stainless steel-hydroxyapatite composite

被引:17
|
作者
Ramli, Mohd Ikram [1 ]
Sulong, Abu Bakar [1 ]
Muhamad, Norhamidi [1 ]
Muchtar, Andanastuti [1 ]
Arifin, Amir [2 ]
Foudzi, Farhana Mohd [1 ]
Al-Furjan, Mohannad Saleh Hammadi [3 ]
机构
[1] Univ Kebangsaan Malaysia, Dept Mech & Mat Engn, Bangi, Selangor, Malaysia
[2] Sriwijaya Univ, Dept Mech Engn, Indralaya, Sumatera Selata, Indonesia
[3] Hangzhou Dianzi Univ, Sch Mech Engn, Hangzhou, Zhejiang, Peoples R China
来源
PLOS ONE | 2018年 / 13卷 / 10期
关键词
YTTRIA-STABILIZED ZIRCONIA; RHEOLOGICAL PROPERTIES; TEMPERATURE; COATINGS; ALLOY; MICROSTRUCTURES; BIOACTIVITY; ATMOSPHERE; CORROSION; BEHAVIOR;
D O I
10.1371/journal.pone.0206247
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
The combination of metallic bio-inert material, stainless-steel 316L (SS316L) and a bio-active material, hydroxyapatite (HA) can produce a composite which has superior properties for orthopaedic applications. The main objective of this study is to investigate the effects of sintering temperature and holding time on the physical and mechanical properties of the sintered part. 50wt.% SS316L and 50wt.% HA were mixed with a binder system of palm stearin (PS) and polyethylene (PE) at 61 vol.% powder loading. Rheological properties show a pseudo-plastic behaviour of the feedstock, where viscosity decreases with increasing shear rate. The feedstock was injection moulded into a tensile bar shape while thermal debinding was carried out at 320 degrees C and 500 degrees C. The brown parts were sintered at 1000, 1100, 1200 and 1300 degrees C, with three different sintering times of 1, 3 and 5 hours in the furnace. It was found that the highest sintered density measured was 95.61% of the theoretical density. In addition, the highest hardness and Young's modulus measured were 150.45 HV and 52.61 GPa respectively, which are higher than those of human bone. The lowest percentage of carbon content was 0.022wt.% given by the sample sintered at 1300 degrees C for 1 hour. Therefore, SS316L/HA composite with good mechanical and physical properties was successfully produced through the PIM process.
引用
收藏
页数:17
相关论文
共 50 条
  • [1] Sintering parameters and mechanical properties of injection moulded aluminium powder
    Acar, L.
    Gulsoy, H. O.
    POWDER METALLURGY, 2011, 54 (03) : 427 - 431
  • [2] Effect of FeB additions on sintering characteristics of injection moulded 17-4PH stainless steel powder
    H. Ö. Gülsoy
    S. Salman
    S. Özbek
    Journal of Materials Science, 2004, 39 : 4835 - 4840
  • [3] Effect of FeB additions on sintering characteristics of injection moulded 17-4PH stainless steel powder
    Gülsoy, HÖ
    Salman, S
    Özbek, S
    JOURNAL OF MATERIALS SCIENCE, 2004, 39 (15) : 4835 - 4840
  • [4] Stainless steel 316L-hydroxyapatite composite via powder injection moulding: rheological and mechanical properties characterisation
    Ramli, M. I.
    Sulong, A. B.
    Muhamad, N.
    Muchtar, A.
    Arifin, A.
    MATERIALS RESEARCH INNOVATIONS, 2014, 18 : 100 - 104
  • [5] Investigation of powder size effects on sintering of powder injection moulded 17-4PH stainless steel
    Park, Dong Yong
    Lee, Gyu M.
    Kwon, Young-Sam
    Oh, Yong Jun
    Lee, Seong
    Jeong, Myeong-Sik
    Park, Seong Jin
    POWDER METALLURGY, 2017, 60 (02) : 139 - 148
  • [6] Effect of sintering temperature on mechanical properties of injection moulded 316L stainless steel using natural waste rubber binder
    Rabilah, Rosniza
    Budin, Salina
    Yusoff, Hamid
    Hashim, Siti Mardini
    Halidi, Siti Nur Amalina Mohd
    PROCEEDINGS OF MECHANICAL ENGINEERING RESEARCH DAY 2018 (MERD), 2018, : 233 - 234
  • [7] Physical and Mechanical Properties of Injection Moulded 316L Stainless Steel Using Waste Rubber Binder
    Rabilah, Rosniza
    Wahab, Nor 'Aini
    Omar, Mohd Afian
    Jaafar, Talib Ria
    Budin, Salina
    Hashim, Siti Mardini
    Sauti, Rosliza
    Razak, Mustaqim Abdul
    ADVANCED MATERIALS FOR SUSTAINABILITY AND GROWTH, 2017, 1901
  • [8] Microstructural and mechanical properties of injection moulded gas and water atomised 17-4 PH stainless steel powder
    Guelsoy, H. O.
    Ozbek, S.
    Baykara, T.
    POWDER METALLURGY, 2007, 50 (02) : 120 - 126
  • [9] Mechanical properties of injection moulded tool steel
    LaSalle, J.
    Metal Powder Report, 2001, 56 (03)
  • [10] Experimental and numerical analysis on sintering behaviours of injection moulded components in 316L stainless steel powder
    Song, J.
    Barriere, T.
    Liu, B.
    Gelin, J. C.
    Michel, G.
    POWDER METALLURGY, 2010, 53 (04) : 295 - 304