Synthesis and characterization of polyamide-6/graphite oxide nanocomposites

被引:21
|
作者
Liu, Yan [1 ]
Chen, Zhenming [1 ]
Yang, Guisheng [1 ,2 ]
机构
[1] Zhejiang Univ, Dept Polymer Sci & Engn, Hangzhou 310027, Zhejiang, Peoples R China
[2] Shanghai Genius Adv Mat Co Ltd, Shanghai 201109, Peoples R China
关键词
GRAPHITE OXIDE; MECHANICAL-PROPERTIES; CLAY; FLAMMABILITY; MORPHOLOGY; COMPOSITE; BEHAVIOR; STYRENE; SURFACE;
D O I
10.1007/s10853-010-4829-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Polyamide-6/graphite oxide (PA6/GO) nanocomposites were synthesized using delamination/absorption method. The morphologies of the composites were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). Both XRD and TEM showed that the GO sheets were completely exfoliated and distributed uniformly in PA6 matrix. Differential scanning calorimetry results revealed that the crystallization temperatures of the composites increased compared to that of pristine PA6, which was due to the heterogeneous nucleating effect of GO. However, the half-time of crystallization of the composites were evidently longer than that of pristine PA6, indicating an apparent decrease in the crystallization rate when GO was loaded into the polymer matrix. This was due to the constraining effect of layered GO on PA6 chains. The temperature of maximum decomposition rate was increased by 53 degrees C only by adding 5 wt% GO, and the maximum decomposition rate of the nanocomposites reduced greatly. The storage modulus (G') and loss modulus (G '') curves shifted to higher modulus upon addition of 1-5 wt% of GO. With increasing GO loading, the shear viscosity of the nanocomposites gradually increased compared with pure PA6.
引用
收藏
页码:882 / 888
页数:7
相关论文
共 50 条
  • [1] Synthesis and characterization of polyamide-6/graphite oxide nanocomposites
    Yan Liu
    Zhenming Chen
    Guisheng Yang
    [J]. Journal of Materials Science, 2011, 46 : 882 - 888
  • [2] Expandable graphite/polyamide-6 nanocomposites
    Uhl, FM
    Yao, Q
    Nakajima, H
    Manias, E
    Wilkie, CA
    [J]. POLYMER DEGRADATION AND STABILITY, 2005, 89 (01) : 70 - 84
  • [3] Non-isothermal crystallization kinetics of polyamide-6/graphite oxide nanocomposites
    Liu, Yan
    Yang, Guisheng
    [J]. THERMOCHIMICA ACTA, 2010, 500 (1-2) : 13 - 20
  • [4] Polyamide-6/silica nanocomposites
    García, M
    García-Turiel, J
    Norder, B
    Chavez, F
    Kooi, BJ
    van Zyl, WE
    Verweij, H
    Blank, DHA
    [J]. ADVANCED ENGINEERING MATERIALS, 2004, 6 (09) : 724 - 729
  • [5] Investigation of thermal degradation and flammability of polyamide-6 and polyamide-6 nanocomposites
    Zong, Ruowen
    Hu, Yuan
    Liu, Naian
    Li, Songyang
    Liao, Guangxuan
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2007, 104 (04) : 2297 - 2303
  • [6] Fatigue crack initiation and propagation in polyamide-6 and in polyamide-6 nanocomposites
    Bellemare, SC
    Bureau, MN
    Denault, J
    Dickson, JI
    [J]. POLYMER COMPOSITES, 2004, 25 (04) : 433 - 441
  • [7] Crystalline properties of injection molded polyamide-6 and polyamide-6/montmorillonite nanocomposites
    Yebra-Rodriguez, Africa
    Alvarez-Lloret, Pedro
    Cardell, Carolina
    Rodriguez-Navarro, Alejandro B.
    [J]. APPLIED CLAY SCIENCE, 2009, 43 (01) : 91 - 97
  • [8] Axial fatigue behaviour of polyamide-6 and polyamide-6 nanocomposites at room temperature
    Ramkumar, A.
    Gnanamoorthy, R.
    [J]. COMPOSITES SCIENCE AND TECHNOLOGY, 2008, 68 (15-16) : 3401 - 3405
  • [10] Impact modified polyamide-6/organoclay nanocomposites: Processing and characterization
    Isik, Isil
    Yilmazer, Ulku
    Bayram, Goknur
    [J]. POLYMER COMPOSITES, 2008, 29 (02) : 133 - 141