TiC-NiCr thermal spray coatings as an alternative to WC-CoCr and Cr3C2-NiCr

被引:37
|
作者
Bolelli, Giovanni [1 ,2 ,3 ]
Colella, Alberto [4 ]
Lusvarghi, Luca [1 ,2 ,3 ]
Morelli, Stefania [1 ]
Puddu, Pietro [1 ]
Righetti, Enrico [1 ]
Sassatelli, Paolo [5 ]
Testa, Veronica [1 ]
机构
[1] Univ Modena & Reggio Emilia, Dipartimento Ingn Enzo Ferrari, Via Pietro Vivarelli 10, Modena 41125, MO, Italy
[2] Univ Modena & Reggio Emilia, Interdept Res Ctr Appl Res & Serv Adv Mech & Moto, InterMech MORE, Via Pietro Vivarelli 2, Modena 41125, MO, Italy
[3] Univ Modena & Reggio Emilia, Consorzio Interuniv Nazl Sci & Tecnol Mat INSTM, Local Unit, Via Pietro Vivarelli 10-1, Modena 41125, MO, Italy
[4] MBN Nanomat SpA, Via G Bortolan 42, Vascon Di Carbonera Tv 31050, TV, Italy
[5] Il Sentiero Int Campus Srl, Via Friuli 11, Schio 36015, VI, Italy
关键词
Thermal spray coatings; Cermets; Sliding wear; High temperature; ABRASIVE WEAR BEHAVIOR; TRIBOLOGICAL BEHAVIOR; RESISTANT COATINGS; SLIDING WEAR; HVOF; NANOCRYSTALLINE; POWDERS; MICROSTRUCTURE; MECHANISMS; SYSTEM;
D O I
10.1016/j.wear.2020.203273
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
TiC-based hardmetal coatings containing 25 or 40 vol% Ni-20 wt%Cr matrix (hereafter TiC-25NiCr and TiC-40NiCr) were obtained by High Velocity Oxygen-Fuel (HVOF) and High Velocity Air-Fuel (HVAF) spraying, starting from high-energy ball milled feedstock powders. These coatings are intended as critical raw materials-free solutions against wear and corrosion. HVOF-sprayed coatings contain some more oxide inclusions than do HVAF ones, but, irrespective of the deposition conditions, TiC-40NiCr coatings are usually somewhat harder (800-900 HV0.3) than TiC-25NiCr ones. They also exhibit lower wear rates in ball-on-disc sliding tests against Al(2)O(3 )at room temperature. A hard asperity can indeed penetrate slightly deeper into TiC-25NiCr, as it deforms inelastically through microcracking. Bigger abrasive grooves are thus produced. The wear resistance of TiC-40NiCr coatings compares favourably to that of a Cr3C2-25% (NiCr) reference, and even approaches that of WC-10 wt%Co-4wt.%Cr. TiC-40NiCr coatings are also more corrosion resistant than both reference materials when tested by electrochemical polarization in a 3.5% NaCl solution. At 400 degrees C, to the contrary, TiC-25NiCr coatings exhibit better sliding wear resistance, whilst more severe abrasive grooving and adhesive tearing affect TiC-40NiCr samples. TiC-NiCr coatings are also unaffected by the transverse macro-cracking that was found to compromise the usefulness of WC-CoCr at 400 degrees C.
引用
收藏
页数:23
相关论文
共 50 条
  • [1] Thermal stability of nanostructured Cr3C2-NiCr coatings
    He, JH
    Ice, M
    Schoenung, JM
    Shin, DH
    Lavernia, EJ
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2001, 10 (02) : 293 - 300
  • [2] Thermal stability of nanostructured Cr3C2-NiCr coatings
    He, JH
    Ice, M
    Lavernia, EJ
    METASTABLE, MECHANICALLY ALLOYED AND NANOCRYSTALLINE MATERIALS, PTS 1 AND 2, 2000, 343-3 : 261 - 266
  • [3] Erosion of oxide scales formed on Cr3C2-NiCr thermal spray coatings
    Matthews, S.
    James, B.
    Hyland, M.
    CORROSION SCIENCE, 2008, 50 (11) : 3087 - 3094
  • [4] Thermal stability of nanostructured Cr3C2-NiCr coatings
    Jianhong He
    Michael Ice
    Julie M. Schoenung
    Enrique J. Lavernia
    Dong H. Shin
    Journal of Thermal Spray Technology, 2001, 10 : 293 - 300
  • [5] Effects of thickness coating on the electrochemical behaviour of thermal spray Cr3C2-NiCr coatings
    Guilemany, JM
    Fernández, J
    Delgado, J
    Benedetti, AV
    Climent, F
    SURFACE & COATINGS TECHNOLOGY, 2002, 153 (2-3): : 107 - 113
  • [6] Effect of spray conditions on the properties of HVOF Cr3C2-NiCr coatings
    Li, Chang-Jiu
    Sonoya, K.
    Ji, Gang-Chang
    Wang, Yu-Yue
    1998, Elsevier Sci Ltd, Exeter, United Kingdom (41):
  • [8] Abrasive wear behaviour of WC-CoCr and Cr3C2-20(NiCr) deposited by HVOF and detonation spray processes
    Murthy, JKN
    Venkataraman, B
    SURFACE & COATINGS TECHNOLOGY, 2006, 200 (08): : 2642 - 2652
  • [9] Sliding friction behaviors of TiCN/Cr3C2-NiCr and TiCN/WC-CoCr duplex coatings fabricated by combining HVOF and HT-CVD procedures
    Peng, Dong
    Li, Zhongsheng
    Wu, Hulin
    Cong, Dalong
    Huang, Anwei
    Song, Kaiqiang
    Zhang, Min
    Wang, Xuan
    Wei, Yu
    Jiang, Bin
    Du, Juan
    Bai, Yixin
    Ding, Xingxing
    SURFACE & COATINGS TECHNOLOGY, 2023, 474
  • [10] High temperature erosion of Cr3C2-NiCr thermal spray coatings - The role of phase microstructure
    Matthews, S.
    James, B.
    Hyland, M.
    SURFACE & COATINGS TECHNOLOGY, 2009, 203 (09): : 1144 - 1153