The thermal degradation of nanocomposites that contain an oligomeric ammonium cation on the clay

被引:50
|
作者
Su, SP [1 ]
Wilkie, CA [1 ]
机构
[1] Marquette Univ, Dept Chem, Milwaukee, WI 53201 USA
关键词
nanocomposites; TGA/FTIR; polystyrene;
D O I
10.1016/S0141-3910(03)00279-9
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The thermal degradation of polystyrene, high-impact polystyrene, ABS terpolymer, poly(methyl methacrylate), polypropylene and polyethylene nanocomposites has been studied using thermogravimetric analysis coupled to Fourier transform infrared spectroscopy, TGA/FT-IR. The nanocomposites that have been studied include immiscible, intercalated and exfoliated systems and the evolved gases do not depend upon the type of nanocomposite and are qualitatively similar to those of the virgin polymer. In the case of the styrenics, the presence of clay promotes the production of oligomer, rather than monomer. It is suggested that this change in evolved products may offer an explanation for why some polymers give large reduction in peak heat release rates while others give much smaller reductions. According to this notion, any polymer that undergoes degradation to produce both oligomer and monomer should give a large reduction in peak heat release rate. (C) 2003 Elsevier Ltd. All rights reserved.
引用
下载
收藏
页码:347 / 362
页数:16
相关论文
共 50 条
  • [1] Thermal degradation behaviour of PE/clay nanocomposites
    Zanetti, M
    Bracco, P
    Costa, L
    POLYMER DEGRADATION AND STABILITY, 2004, 85 (01) : 657 - 665
  • [2] Thermal degradation behavior of polyamide 6/clay nanocomposites
    Pramoda, KP
    Liu, TX
    Liu, ZH
    He, CB
    Sue, HJ
    POLYMER DEGRADATION AND STABILITY, 2003, 81 (01) : 47 - 56
  • [3] The effect of clay on the thermal degradation of polyamide 6 in polyamide 6/clay nanocomposites
    Jang, BN
    Wilkie, CA
    POLYMER, 2005, 46 (10) : 3264 - 3274
  • [4] An XPS investigation of thermal degradation and charring on PMMA clay nanocomposites
    Du, JX
    Zhu, J
    Wilkie, CA
    Wang, JQ
    POLYMER DEGRADATION AND STABILITY, 2002, 77 (03) : 377 - 381
  • [5] Effect of clay treatment on the thermal degradation of PHB based nanocomposites
    Ollier, Romina P.
    D'Amico, David A.
    Schroeder, Walter F.
    Cyras, Viviana P.
    Alvarez, Vera A.
    APPLIED CLAY SCIENCE, 2018, 163 : 146 - 152
  • [6] Thermal, structural and mechanical analysis of polymer/clay nanocomposites with controlled degradation
    Alicja Rapacz-Kmita
    Marcin Gajek
    Magdalena Dudek
    Ewa Stodolak-Zych
    Barbara Szaraniec
    Radosław Lach
    Journal of Thermal Analysis and Calorimetry, 2017, 127 : 389 - 398
  • [7] Zero-order kinetics of the thermal degradation of polypropylene/clay nanocomposites
    Qin, HL
    Zhang, SM
    Zhao, CG
    Yang, MS
    JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 2005, 43 (24) : 3713 - 3719
  • [8] A study of thermal degradation behavior of polyamide 6/clay nanocomposites.
    Pramoda, KP
    Liu, TX
    Liu, ZH
    He, CB
    Sue, HJ
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2002, 224 : U379 - U379
  • [9] Thermal, structural and mechanical analysis of polymer/clay nanocomposites with controlled degradation
    Rapacz-Kmita, Alicja
    Gajek, Marcin
    Dudek, Magdalena
    Stodolak-Zych, Ewa
    Szaraniec, Barbara
    Lach, Radoslaw
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2017, 127 (01) : 389 - 398
  • [10] Formation of cation-exchanged clay nanocomposites
    Barber, Grant D.
    Storey, Robson F.
    Moore, Robert B.
    American Chemical Society, Polymer Preprints, Division of Polymer Chemistry, 1999, 40 (02): : 768 - 769