Recycling of Sustainable Co-Firing Fly Ashes as an Alkali Activator for GGBS in Blended Cements

被引:14
|
作者
Wu, Yann-Hwang [1 ,2 ]
Huang, Ran [3 ]
Tsai, Chia-Jung [1 ]
Lin, Wei-Ting [4 ]
机构
[1] Natl Taiwan Ocean Univ, Inst Mat Engn, Keelung 20224, Taiwan
[2] Taiwan & Pacific Engineers & Constructors Ltd, Taipei 10669, Taiwan
[3] Natl Taiwan Ocean Univ, Dept Harbor & River Engn, Keelung 20224, Taiwan
[4] Natl Ilan Univ, Dept Civil Engn, Ilan 26047, Taiwan
来源
MATERIALS | 2015年 / 8卷 / 02期
关键词
BLAST-FURNACE SLAG; CONCRETE; PERFORMANCE; DURABILITY; MIXTURE; IRON;
D O I
10.3390/ma8020784
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This study investigates the feasibility of co-firing fly ashes from different boilers, circulating fluidized beds (CFB) or stokers as a sustainable material in alkali activators for ground granulated blast-furnace slag (GGBS). The mixture ratio of GGBS and co-firing fly ashes is 1:1 by weight. The results indicate that only CF fly ash of CFB boilers can effectively stimulate the potential characteristics of GGBS and provide strength as an alkali activator. CF fly ash consists of CaO3 (48.5%), SiO2 (21.1%), Al2O3 (13.8%), SO3 (10.06%), Fe2O3 (2.25%) and others (4.29%). SA fly ash consists of Al2O3 (19.7%), SiO2 (36.3%), Fe2O3 (28.4%) and others (15.6%). SB fly ash consists of Al2O3 (15%), SiO2 (25.4%), Zn (20.6%), SO3 (10.9%), Fe2O3 (8.78%) and others (19.32%). The mixtures of SA fly ash and SB fly ash with GGBS, respectively, were damaged in the compressive strength test during seven days of curing. However, the built up strength of the CF fly ash and GGBS mixture can only be maintained for 7-14 days, and the compressive strength achieves 70% of that of a controlled group (cement in hardening cement paste). The strength of blended CF fly ash and GGBS started to decrease after 28 days, and the phenomenon of ettrigite was investigated due to the high levels of sulfur content. The CaO content in sustainable co-firing fly ashes must be higher than a certain percentage in reacting GGBS to ensure the strength of blended cements.
引用
收藏
页码:784 / 798
页数:15
相关论文
共 50 条
  • [1] Swirling Melting Characteristics of Fly Ashes from Co-firing of MSWI in China
    Wang Xue-tao
    Jiao You-zhou
    Xu Bin
    Jin Bao-sheng
    2009 INTERNATIONAL CONFERENCE ON ENERGY AND ENVIRONMENT TECHNOLOGY, VOL 3, PROCEEDINGS, 2009, : 597 - +
  • [2] Using GGBOS as the alkali activators in GGBS and GGBOS blended cements
    Tsai, Chia-Jung
    Huang, Ran
    Lin, Wei-Ting
    Chiang, Hsiang-Wei
    Construction and Building Materials, 2014, 70 : 501 - 507
  • [3] Using GGBOS as the alkali activators in GGBS and GGBOS blended cements
    Tsai, Chia-Jung
    Huang, Ran
    Lin, Wei-Ting
    Chiang, Hsiang-Wei
    CONSTRUCTION AND BUILDING MATERIALS, 2014, 70 : 501 - 507
  • [4] Melting characteristics of fly ashes from Co-firing of municipal solid waste and coal incinerator
    Wang, Xue-Tao
    Jiao, You-Zhou
    Jin, Bao-Sheng
    Xu, Bin
    Mao, Peng-Jun
    Wu, Jian
    Ranshao Kexue Yu Jishu/Journal of Combustion Science and Technology, 2007, 13 (01): : 35 - 39
  • [5] Improving the performance of ternary blended cements by mixing different types of fly ashes
    Antiohos, S. K.
    Papadakis, V. G.
    Chaniotakis, E.
    Tsimas, S.
    CEMENT AND CONCRETE RESEARCH, 2007, 37 (06) : 877 - 885
  • [6] Effect of Blended Fly Ashes in Mitigating Alkali-Silica Reaction
    Harish, K. V.
    Rangaraju, P. R.
    TRANSPORTATION RESEARCH RECORD, 2011, (2240) : 80 - 88
  • [7] Biomass ashes to produce an alternative alkaline activator for alkali-activated cements
    Soriano, L.
    Font, A.
    Borrachero, M., V
    Monzo, J. M.
    Paya, J.
    Tashima, M. M.
    MATERIALS LETTERS, 2022, 308
  • [8] Effect of Alkali Activator on the Standard Consistency and Setting Times of Fly Ash and GGBS-Based Sustainable Geopolymer Pastes
    Dineshkumar, M.
    Umarani, C.
    ADVANCES IN CIVIL ENGINEERING, 2020, 2020
  • [9] Release of alkali metals during co-firing biomass and coal
    Wu, Dongyin
    Wang, Yuhao
    Wang, Yang
    Li, Sen
    Wei, Xiaolin
    RENEWABLE ENERGY, 2016, 96 : 91 - 97
  • [10] Self-cementitious properties of fly ashes from CFBC boilers co-firing coal and high-sulphur petroleum coke
    Sheng, Guanghong
    Li, Qin
    Zhai, Jianping
    Li, Feihu
    CEMENT AND CONCRETE RESEARCH, 2007, 37 (06) : 871 - 876