Photoelectrochemical analysis on the passive film formed on Ni in pH 8.5 buffer solution

被引:70
|
作者
Jang, HJ
Park, CJ
Kwon, HS
机构
[1] Korea Adv Inst Sci & Technol, Dept Mat Sci & Engn, Taejon 305701, South Korea
[2] POSCO, Stainless Steel Res Grp, Tech Res Labs, Pohang 790385, Gyeongsangbuk D, South Korea
关键词
Ni; passive film; photocurrent; Mott-Schottky analysis; semiconducting properties;
D O I
10.1016/j.electacta.2004.12.027
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The structure and composition of passive film formed on Ni in pH 8.5 buffer solution were examined by comparing the photocurrent and Mott-Schottky responses for both the passive film and the thermally grown oxide on Ni in air at 400 degrees C. The photocurrent spectra for the passive film on Ni are resolved into two spectral components, each of which originated from inner NiO and outer Ni(OH)2 layers, respectively. The band gap energy (E-g) for the inner NiO and the outer Ni(OH)(2) were measured to be 4.80 +/- 0.1 and 3.05 +/- 0.1 eV, respectively. E-g (4.80 0.1 eV) of the inner NiO of the passive film on Ni was close to that (4.97 eV) of the thermally grown oxide of Ni within an error range, suggesting that the inner NiO in the passive film is crystalline. The Mott-Schottky plots for both the passive film and the thermal oxide film on Ni demonstrated that the two films exhibited p-type semiconductivity with different values of flat band potential (U-fb); 0.3 V-SCE for the passive film and 0 V-SCE for the thermally grown NiO. An electronic energy band model of P-p heterojunction composed of inner NiO and outer Ni(OH)(2) layers was proposed to explain the photocurrent and Mott-Schottky responses for the passive film on Ni. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:3503 / 3508
页数:6
相关论文
共 50 条
  • [1] Photoelectrochemical analysis on the passive film formed on Ti in pH 8.5 buffer solution
    Kim, DongYung
    Ahn, SeJin
    Kwon, HyukSang
    THIN SOLID FILMS, 2006, 513 (1-2) : 212 - 216
  • [2] Photoelectrochemical analysis on the passive film formed on Fe-20Cr in pH 8.5 buffer solution
    Cho, EA
    Kwon, H
    Macdonald, DD
    ELECTROCHIMICA ACTA, 2002, 47 (10) : 1661 - 1668
  • [3] Photoelectrochemical study of the growth of the passive film formed on Fe-20Cr-15Ni in a pH 8.5 buffer solution
    Jang, HeeJin
    Park, ChanJin
    Kwon, HyukSang
    METALS AND MATERIALS INTERNATIONAL, 2010, 16 (02) : 247 - 252
  • [4] Photoelectrochemical study of the growth of the passive film formed on Fe-20Cr-15Ni in a pH 8.5 buffer solution
    HeeJin Jang
    ChanJin Park
    HyukSang Kwon
    Metals and Materials International, 2010, 16 : 247 - 252
  • [5] Photo-electrochemical analysis of passive film formed on Cr in pH 8.5 buffer solution
    Kim, JS
    Cho, EA
    Kwon, HS
    ELECTROCHIMICA ACTA, 2001, 47 (03) : 415 - 421
  • [6] Effects of solution temperature on electronic properties of passive film formed on Fe in pH 8.5 borate buffer solution
    Ahn, SJ
    Kwon, HS
    ELECTROCHIMICA ACTA, 2004, 49 (20) : 3347 - 3353
  • [7] Effects of Mo on the Passive Films Formed on Ni-(15, 30) Cr-5Mo Alloys in pH 8.5 Buffer Solution
    Jang, HeeJin
    Kwon, HyukSang
    JOURNAL OF THE KOREAN ELECTROCHEMICAL SOCIETY, 2009, 12 (03): : 258 - 262
  • [8] Effects of EDTA on the electronic properties of passive film on Fe-20Cr in pH 8.5 buffer solution
    Cho, E
    Ahn, S
    Kwon, H
    ELECTROCHIMICA ACTA, 2005, 50 (16-17) : 3383 - 3389
  • [9] Electronic Structures of Passive Film Formed on Ti and Cr in a Phosphate Buffer Solution of pH 7
    Kim, Seong-Cheol
    Tsuchiya, Hiroaki
    Manaka, Tomoyo
    Hanawa, Takao
    Fujimoto, Shinji
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2024, 171 (03)
  • [10] AN STM STUDY OF THE PASSIVE FILM FORMED ON IRON IN BORATE BUFFER SOLUTION
    RYAN, MP
    NEWMAN, RC
    THOMPSON, GE
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1995, 142 (10) : L177 - L179