摘要
Limit load solutions for thin-walled cylinders with circumferential cracks under combined axial tension, bending and pressure are developed, considering the effect of pressure-induced hoop stress via the Mises yield criterion. The new solutions cover thin-walled cylinders with constant-depth or semi-elliptical surface cracks and through-wall cracks. The predictions of the new Mises-based limit load equation agree very well with elastic-perfectly plastic finite element results. However, net-section collapse equations, which ignore the hoop stress in the cylinder, tend to overestimate the limit load when internal pressure is dominant. The solution for constant-depth cracks without crack closure is proposed for inclusion in fitness-for-purpose assessment procedures for constant-depth or semi-elliptical surface cracks and through-wall cracks.
引用
收藏
页码:673 / 683
页数:11
相关论文
共 50 条
  • [1] Limit load solutions of thick-walled cylinders with fully circumferential cracks under combined internal pressure and axial tension
    Gao, Zengliang
    Cai, Gangsi
    Liang, Lihua
    Lei, Yuebao
    NUCLEAR ENGINEERING AND DESIGN, 2008, 238 (09) : 2155 - 2164
  • [2] Global limit load solutions for thick-walled cylinders with circumferential cracks under combined internal pressure, axial force and bending moment - Part I: Theoretical solutions
    Lei, Yuebao
    Li, Yuebing
    Gao, Zengliang
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2014, 114 : 23 - 40
  • [3] Limit load solutions of thick-walled cylinders with fully circumferential cracks under combined internal pressure and axial tension (vol 238, pg 2155, 2008)
    Gao, Zengliang
    Cai, Gangsi
    Liang, Lihua
    Lei, Yuebao
    NUCLEAR ENGINEERING AND DESIGN, 2015, 284 : 309 - 309
  • [4] Limit Load Solution for Thin-Walled Cylinder with Circumferential Crack under Combined Internal Pressure, Axial Force, Bending Moment and Torsion Moment
    Arun, Sutham
    Fakkaew, Wichaphon
    Fongsamootr, Thongchai
    CHIANG MAI JOURNAL OF SCIENCE, 2022, 49 (01): : 55 - 68
  • [5] Limit load for cylinders with axial internal surface cracks under combined internal pressure and global bending moment
    Yang, Zhancheng
    Li, Yuebing
    Lei, Yuebao
    Gao, Zengliang
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2021, 194
  • [6] Global limit load solutions for thick-walled cylinders with circumferential cracks under combined internal pressure, axial force and bending moment - Part II: Finite element validation
    Li, Yuebing
    Lei, Yuebao
    Gao, Zengliang
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2014, 114 : 41 - 60
  • [7] Limit Load Finite Element Analysis of Thick-walled Cylinders with Surface Cracks Under Combined Internal Pressure and Axial Tension
    Maarefdoust, Mahdi
    Akbarzade, Pooria
    MATERIAL AND MANUFACTURING TECHNOLOGY II, PTS 1 AND 2, 2012, 341-342 : 416 - +
  • [8] The plastic limit load of circumferentially cracked thin-walled pipes under axial force, internal pressure and asymmetrical bending
    Shu, HM
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2002, 79 (05) : 377 - 382
  • [9] Creep failure time of thin-walled pipes under combined internal pressure, bending, and tension
    A. El Megharbel
    Strength of Materials, 2010, 42 : 439 - 449
  • [10] CREEP FAILURE TIME OF THIN-WALLED PIPES UNDER COMBINED INTERNAL PRESSURE, BENDING, AND TENSION
    El Megharbel, A.
    STRENGTH OF MATERIALS, 2010, 42 (04) : 439 - 449