Atomic diffusion and microstructure of SmCo5 multilayers with high coercivity

被引:9
|
作者
Qiu, Zhaoguo [1 ,2 ,3 ]
Liu, J. Ping [2 ]
Yu, Hongya [1 ,3 ]
Poudyal, Narayan [2 ]
Han, Guangbing [2 ,4 ,5 ]
Zeng, Dechang [1 ,3 ]
Hong, Yuan [1 ,3 ]
机构
[1] South China Univ Technol, Sch Mat Sci & Engn, Guangzhou 510640, Guangdong, Peoples R China
[2] Univ Texas Arlington, Dept Phys, Arlington, TX 76019 USA
[3] South China Univ Technol, Zhongshan R&D Ctr Mat Surface & Thin Films Techno, Gent Mat Surface Technol Guangdong Co Ltd, Zhongshan 528437, Peoples R China
[4] Shandong Univ, Sch Phys, Jinan 250100, Shandong, Peoples R China
[5] Shandong Univ, State Key Lab Crystal Mat, Jinan 250100, Shandong, Peoples R China
关键词
SmCo5 multilayer films; Atomic substitution; Diffusion; High coercivity; MAGNETIC-PROPERTIES; THIN-FILMS; UNDERLAYER; CR; TEMPERATURE; THICKNESS; OXIDATION;
D O I
10.1016/j.jallcom.2017.10.286
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Sm-Co multilayer films are deposited by plasma sputtering with a Cr underlayer and a Cu buffer layer, followed by annealing at different temperatures. The as-deposited films show low hard magnetic properties due to the existing amorphous Sm-Co phase. After annealing, for the films without Cu buffer layer, there is only Sm2Co17 phase in the films even at high annealing temperature and the coercivity is less than 12kOe. When inserting a Cu buffer layer, the well-crystalline SmCo5 single phase is obtained at relatively lower annealing temperature (500 degrees C and 550 degrees C) and extremely high in-plane coercivity (38kOe) is achieved. An analysis of Transmission electron microscopy (TEM) and Auger electron spectroscopy (AES) reveals that Cu atoms started to diffuse during the annealing process induced by thermal dynamics, concentration gradient and microstructure variations, and eventually uniformly distribute in SmCo layer and form Sm(Co,Cu)(5) phase. The exchange interaction energy calculation indicates that small fraction of Cu atoms preferentially substitute the Co(2c) site in SmCo5 lattice, which reduces the exchange coupling effects of Sm-Co and gives rise to the coercivity. The results provide a guidance to fabrication of single-phase Sm(Co,Cu)(5) multilayer films with superior performance that have applications in advanced electromagnetic and electronic devices. (c) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:45 / 52
页数:8
相关论文
共 50 条
  • [1] High Coercivity Through Texture Formation in SmCo5/Co Multilayers
    Sastry, P. U.
    Mishra, P. K.
    Krishnan, M.
    Chowdhury, P.
    Ravikumar, G.
    SOLID STATE PHYSICS, VOL 57, 2013, 1512 : 1098 - 1099
  • [2] Effect of Microstructure on the Coercivity of SmCo5 Intermetallic Compound
    Akhtar, Saleem
    Khan, Mushtaq
    Khan, A. Nusair
    Jaffery, Syed Husain Imran
    MATERIALS TRANSACTIONS, 2020, 61 (11) : 2195 - 2200
  • [3] Effect of several heat treatments on the microstructure and coercivity of SmCo5 magnets
    De Campos, M.F. (mcampos@metal.eeimvr.uff.br), 1600, Elsevier Ltd (368): : 1 - 2
  • [4] Effect of several heat treatments on the microstructure and coercivity of SMCo5 magnets
    de Campos, MF
    Okumura, H
    Hadjipanayis, GC
    Rodrigues, D
    Landgraf, FJG
    Neiva, AC
    Romero, SA
    Missell, FP
    JOURNAL OF ALLOYS AND COMPOUNDS, 2004, 368 (1-2) : 304 - 307
  • [5] High-coercivity SmCo5/α-Fe nanocomposite magnets
    Saito, Tetsuji (tetsuji.saito@it-chiba.ac.jp), 1600, Elsevier Ltd (735):
  • [6] High-coercivity SmCo5/α-Fe nanocomposite magnets
    Saito, Tetsuji
    Nishio-Hamane, Daisuke
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 735 : 218 - 223
  • [9] Chemical composition and coercivity of SmCo5 magnets
    de Campos, MF
    Landgraf, FJG
    Saito, NH
    Romero, SA
    Neiva, AC
    Missell, FP
    de Morais, E
    Gama, S
    Obrucheva, EV
    Jalnin, BV
    JOURNAL OF APPLIED PHYSICS, 1998, 84 (01) : 368 - 373
  • [10] Annealing effects on the coercivity of SmCo5 nanoparticles
    Chowdary, KM
    Giri, AK
    Pellerin, K
    Majetich, SA
    Scott, JHJ
    JOURNAL OF APPLIED PHYSICS, 1999, 85 (08) : 4331 - 4333