Hydration kinetics and gel morphology of C-S-H

被引:0
|
作者
Ioannidou, K. [1 ,2 ]
Masoero, E. [3 ]
Levitz, P. [4 ,5 ]
Pellenq, R. J. -M. [1 ,2 ,6 ,7 ]
Del Gado, E. [8 ,9 ,10 ]
机构
[1] MIT, Dept Civil & Environm Engn, 77 Massachusetts Ave, Cambridge, MA 02139 USA
[2] MIT, MIT CNRS Joint Lab, Cambridge, MA 02139 USA
[3] Newcastle Univ, Sch Civil Engn & Geosci, Newcastle Upon Tyne NE1 7RU, Tyne & Wear, England
[4] CNRS, PHENIX Lab, Paris, France
[5] Univ Paris 06, Paris, France
[6] CNRS, CINaM, Marseille, France
[7] Aix Marseille Univ, Marseille, France
[8] Georgetown Univ, Dept Phys, Washington, DC 20057 USA
[9] Georgetown Univ, Inst Soft Matter Synth & Metrol, Washington, DC USA
[10] Swiss Fed Inst Technol, Dept Civil Environm & Geomat Engn, Zurich, Switzerland
关键词
CALCIUM-SILICATE-HYDRATE; GROWTH;
D O I
暂无
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Calcium-silicate hydrate (C-S-H) is the main binder in cement and concrete. It starts forming from the early stages of cement hydration and it progressively densifies as cement sets. C-S-H nanoscale building blocks form a cohesive gel, whose structure and mechanics are still poorly understood, in spite of its practical importance. Here we review a statistical physics approach recently developed, which allows us to investigate the C-S-H gel formation under the out-of-equilibrium conditions typical of cement hydration. Our approach is based on colloidal particles, precipitating in the pore solution and interacting with effective forces associated to the ionic environment. We present the evolution of the space filling of C-S-H with different particle interactions and compare them with experimental data at different lime concentrations. Moreover, we discuss the structural features of C-S-H in the mesoscale in terms of the scattering intensity. The comparison of our early stage C-S-H structures with small angle neutron scattering (SANS) experiments shows that long range spatial correlations and structural heterogeneties that develop in that early stages of hydration persist also in the hardened paste.
引用
收藏
页码:565 / 573
页数:9
相关论文
共 50 条
  • [1] STRUCTURE AND MORPHOLOGY OF C-S-H GEL
    DIAMOND, S
    AMERICAN CERAMIC SOCIETY BULLETIN, 1974, 53 (04): : 326 - 326
  • [2] Effect of hydration on the dielectric properties of C-S-H gel
    Cerveny, Silvina
    Arrese-Igor, Silvia
    Dolado, Jorge S.
    Gaitero, Juan J.
    Alegria, Angel
    Colmenero, Juan
    JOURNAL OF CHEMICAL PHYSICS, 2011, 134 (03):
  • [3] ON THE MORPHOLOGY OF TYPE-III C-S-H GEL
    DIAMOND, S
    LACHOWSKI, EE
    CEMENT AND CONCRETE RESEARCH, 1980, 10 (05) : 703 - 705
  • [4] Effect of the densification of C-S-H on hydration kinetics of tricalcium silicate
    Joseph, Shiju
    Bishnoi, Shashank
    Van Balen, Koen
    Cizer, Ozlem
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2018, 101 (06) : 2438 - 2449
  • [5] Impact of ZnO on C3S hydration and C-S-H morphology at early ages
    Li, Xuerun
    Scrivener, Karen L.
    CEMENT AND CONCRETE RESEARCH, 2022, 154
  • [6] Hydration Activity of Silica Fume and Its Effect on The Structure of C-S-H Gel
    Wang Lei
    He Zhen
    Yan Jianjun
    APPLIED MECHANICS AND MATERIALS I, PTS 1-3, 2013, 275-277 : 2084 - +
  • [7] CHEMICAL COMPOSITION OF C-S-H GEL FORMED IN THE HYDRATION OF CALCIUM SILICATE PASTES
    BENTUR, A
    BERGER, RL
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1979, 62 (3-4) : 117 - 120
  • [8] The influence of sulfate addition on hydration kinetics and C-S-H morphology of C3S and C3S/C3A systems
    Zunino, Franco
    Scrivener, Karen
    CEMENT AND CONCRETE RESEARCH, 2022, 160
  • [9] Dissolution kinetics of C-S-H gel: Flow-through experiments
    Trapote-Barreira, Ana
    Cama, Jordi
    Soler, Josep M.
    PHYSICS AND CHEMISTRY OF THE EARTH, 2014, 70-71 : 17 - 31
  • [10] REVIEW OF SYNTHESIS AND PROPERTIES OF TOBERMORITE, C-S-H(I), AND C-S-H GEL
    SNELL, DS
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1975, 58 (7-8) : 292 - 295