Evaluation of stress corrosion resistance and corrosion fatigue fracture behavior of ultra-high-strength P/M Al-Zn-Mg alloy

被引:2
|
作者
Minoshima, K [1 ]
Okada, M
Komai, K
机构
[1] Kyoto Univ, Grad Sch Engn, Dept Mech Engn, Sakyo Ku, Kyoto 6068501, Japan
[2] Cent Japan Railway Co, Chuo Ku, Tokyo 1038288, Japan
关键词
corrosion fatigue; stress corrosion cracking; SSRT; fatigue strength; fatigue crack propagation; fractography; powder metallurgy; Al-Zn-Mg alloy;
D O I
10.1016/S0142-1123(98)00049-8
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Quasi-static tensile tests in air and slow strain rate tests (SSRTs) in a 3.5% NaCl solution were conducted in an ultra-high-strength P/M Al-Zn-Mg alloy fabricated through powder metallurgy. Attention is also paid to fatigue strength and fatigue crack growth behavior in laboratory air and in a 3.5% NaCl solution. The alloy has extremely high strength of about 800 MPa. However, elongation at break remains small, at about 1.3%. The final fracture occurs by a macroscopically flat crack normal to the tensile axis, with little reduction in area and little shear lip on the periphery of a smooth sample. However, it fails microscopically in a ductile manner, with dimples. Dimple size is less than 1 mu m, because the grain size of the alloy is extremely small. Strengthening mechanisms operating in the alloy are: small grains, sufficient metastable eta' phase in a matrix, and intermetallic compound acting as a fiber reinforcement. The SSRT strength in a 3.5% NaCl solution decreases slightly at a very low strain rate, that is smaller than those observed in aluminum alloys sensitive to stress corrosion. This means that the crack initiation resistance to stress corrosion is superior. However, under cyclic loading, the corrosion fatigue strength becomes lower than that conducted in air, because pitting corrosion on a sample surface acts as a stress concentrator. Crack initiation site of quasi-static and fatigue failure of the alloy is at inclusions, and hence, it is essential to decrease inclusions in the alloy for the improvement of the mechanical properties. Fatigue crack resistance of the alloy is inferior to conventional Al-Zn-Mg alloys fabricated by ingot metallurgy, because the fatigue fracture toughness, or ductility, of the alloy is inferior to other Al alloys, and intergranular cracking promotes crack growth. However, no influence of 3.5% NaCl solution on corrosion fatigue crack growth is observed, although an investigation is required into whether stress corrosion crack growth occurs or not, and at the same time, and of corrosion fatigue crack growth behavior at lower stress intensity. The fracture surface and crack initiation sites are closely examined using a high-resolution field emission type scanning electron microscope, and the fracture mechanisms of the alloy are discussed. (C) 1998. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:757 / 766
页数:10
相关论文
共 50 条
  • [1] Evaluation of stress corrosion resistance and corrosion fatigue fracture behavior of ultra-high-strength P/M Al-Zn-Mg alloy
    Minoshima, K
    Okada, M
    Komai, K
    LOW CYCLE FATIGUE AND ELASTO-PLASTIC BEHAVIOUR OF MATERIALS, 1998, : 393 - 398
  • [2] Evaluation of stress corrosion resistance and corrosion fatigue fracture behavior of ultra-high-strength P/M Al-Zn-Mg alloy
    Komai, K
    Minoshima, K
    Okada, M
    ALUMINUM ALLOYS 2002: THEIR PHYSICAL AND MECHANICAL PROPERTIES PTS 1-3, 2002, 396-4 : 1455 - 1460
  • [3] COMPARISON OF CORROSION AND STRESS CORROSION BEHAVIOR OF A TERNARY AL-ZN-MG ALLOY
    SEDRIKS, AJ
    GREEN, JAS
    MATERIALS PROTECTION, 1969, 8 (12): : 49 - &
  • [4] COMPARISON OF CORROSION AND STRESS CORROSION BEHAVIOR OF A TERNARY AL-ZN-MG ALLOY
    SEDRIKS, AJ
    GREEN, JAS
    CORROSION, 1969, 25 (12) : 6 - &
  • [5] CORROSION FATIGUE OF A HIGH-PURITY AL-ZN-MG ALLOY
    RICKER, RE
    DUQUETTE, DJ
    JOURNAL OF METALS, 1984, 36 (07): : 6 - 6
  • [6] COMPARISON OF CORROSION AND STRESS-CORROSION BEHAVIOR OF A TERNARY AL-ZN-MG ALLOY
    SEDRIKS, AJ
    GREEN, JAS
    NOVAK, DL
    METALLURGICAL TRANSACTIONS, 1970, 1 (07): : 1815 - &
  • [7] Effect of aging on the microstructure and stress corrosion resistance of Al-Zn-Mg alloy
    Ye L.-Y.
    Yang W.-Q.
    Tang J.-G.
    Liu S.-D.
    Deng Y.-L.
    Zhang X.-M.
    Gongcheng Kexue Xuebao/Chinese Journal of Engineering, 2019, 41 (12): : 1575 - 1582
  • [8] Effect of grain structure on stress corrosion resistance of Al-Zn-Mg alloy
    Ye L.
    Yao X.
    Tang J.
    Li H.
    Zhang X.
    Zhongnan Daxue Xuebao (Ziran Kexue Ban)/Journal of Central South University (Science and Technology), 2019, 50 (05): : 1049 - 1055
  • [9] FRACTURE BEHAVIOR OF A MEDIUM STRENGTH AL-ZN-MG ALLOY
    EMBURY, JD
    NES, E
    ZEITSCHRIFT FUR METALLKUNDE, 1973, 64 (11): : 805 - 812
  • [10] Coarse Grain Layer on Stress Corrosion Cracking Resistance of Al-Zn-Mg Alloy
    Ye, Lingying
    Yao, Xuebin
    Lin, Huaqiang
    Liu, Shengdan
    Deng, Yunlai
    Zhang, Xinming
    HIGH PERFORMANCE STRUCTURAL MATERIALS, 2018, : 337 - 347