Helium implantation effects on mechanical properties of SiCf/SiC composites

被引:9
|
作者
Hasegawa, A [1 ]
Saito, M
Abe, K
Jones, RH
机构
[1] Tohoku Univ, Dept Quantum Sci & Energy Engn, Aoba Ku, Sendai, Miyagi 98077, Japan
[2] Pacific NW Natl Lab, Richland, WA 99352 USA
关键词
D O I
10.1016/S0022-3115(97)00342-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Helium effects on mechanical properties of SiC/SiC composites were studied to apply the composites on structural materials of a fusion reactor. Two types of 2D-SiC/SiC composites were examined in this work. Helium was implanted using 36 MeV alpha particles with an energy degrader system to obtain a uniform helium depth distribution in the specimen. The implantation temperature was 400-800 degrees C and the helium concentration after implantation was about 150-170 appm. Three-point bending test was carried out at room temperature. Results of bending test showed that a small decrease of bend strength was observed in the composite which had the higher bend strength before implantation. Helium implantation effect was not clearly observed in the lower bend strength composite. SEM observation results on the fracture surface gave no evidence for fiber coating failure. The decrease of bend strength after helium implantation may be attributed to a degradation of mechanical properties of the fibers by implanted helium. (C) 1998 Elsevier Science B.V.
引用
收藏
页码:31 / 35
页数:5
相关论文
共 50 条
  • [1] Helium implantation effects on mechanical properties of SiCf/SiC composites
    Tohoku Univ, Sendai, Japan
    Journal of Nuclear Materials, 1998, 253 : 31 - 35
  • [2] Comparison of the mechanical behaviour of SiCf/SiC composites following neutron irradiation and helium implantation
    Rebelo, AJF
    Scholz, HW
    Kolbe, H
    Tartaglia, GP
    Fenici, P
    JOURNAL OF NUCLEAR MATERIALS, 1998, 258 : 1582 - 1588
  • [3] Comparison of the mechanical behaviour of SiCf/SiC composites following neutron irradiation and helium implantation
    Rebelo, A.J.F.
    Scholz, H.W.
    Kolbe, H.
    Tartaglia, G.P.
    Fenici, P.
    Journal of Nuclear Materials, 1998, 258-263 (pt B): : 1582 - 1588
  • [4] Helium-bubble formation behavior of SiCf/SiC composites after helium implantation
    Hasegawa, A
    Saito, M
    Nogami, S
    Abe, K
    Jones, RH
    Takahashi, H
    JOURNAL OF NUCLEAR MATERIALS, 1999, 264 (03) : 355 - 358
  • [5] Preparation and mechanical properties of SiCf/SiC composites
    He, XB
    Qu, XH
    Ye, B
    JOURNAL OF INORGANIC MATERIALS, 2005, 20 (03) : 677 - 684
  • [6] Mechanical properties of SiC whiskers reinforced SiCf/SiC composites
    Jiang Zhuo-yu
    Shu Xiao-wen
    Lyu Xiao-xu
    Gao Ye
    Zhou Yi-ran
    Dong Yu-fei
    Jiao Jian
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2021, 49 (08): : 89 - 96
  • [7] Effects of interphases on mechanical properties of CVI-mini SiCf/SiC composites
    Zhao Wen-qing
    Qi Zhe
    Lyu Xiao-xu
    Jiao Jian
    Ma Zhuang
    Zhu Shi-zhen
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2021, 49 (07): : 71 - 77
  • [8] Mechanical properties of SiCf/SiC composites with PyC and the BN interface
    Yang, Bei
    Zhou, Xingui
    Chai, Yuxin
    CERAMICS INTERNATIONAL, 2015, 41 (05) : 7185 - 7190
  • [9] Effects of helium implantation on the mechanical properties of 4H-SiC
    Barbot, J. -F.
    Beaufort, M. -F.
    Audurier, V.
    SILICON CARBIDE AND RELATED MATERIALS 2009, PTS 1 AND 2, 2010, 645-648 : 721 - 724
  • [10] Effect of thermal cycling of SiCf/SiC composites on their mechanical properties
    Udayakumar, A.
    Stalin, M.
    Abhayalakshmi, M. B.
    Hariharan, Ramya
    Balasubramanian, M.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 442 (1-3) : S384 - S389